| INFLUENCE OF MnO ON REDUCTION OF TiO_2 IN Ti-CONTAINING SLAG OF BLAST FURNACE TYPE |
| DU Hegui;ZOU Anhua Northeast University of Technology; Shenyang |
|
Cite this article:
DU Hegui;ZOU Anhua Northeast University of Technology; Shenyang. INFLUENCE OF MnO ON REDUCTION OF TiO_2 IN Ti-CONTAINING SLAG OF BLAST FURNACE TYPE. Acta Metall Sin, 1991, 27(4): 73-79.
|
|
|
Abstract Studies were carried out of the formation of Ti(C,N) during smelting V-bearing titanomagnetite in blast furnace and the influence of MnO content on reductionof TiO_2 in the high titania containing slag. The reduction of TiO_2 is restricted byMnO predominantly at the slag/metal interface and no more at the slag/coke one.Both the MnO content about 4% and the basicity from 0.6 to 1.2 in slag may re-markably restrict the formation of Ti(C,N). MnO may also retard the reduction ofSiO_2 and accelerate the desulphidation under certain condition.
|
|
Received: 18 April 1991
|
1 田村庸,中村成子.铁钢,1985;71(12) :S934 2 Bell H B.Iron and Steel.1963;36:643 3 彭瑞伍,邹元爔.全国第一届冶金过程物理化学学术报告论文集,上海:上海科学技术出版社,1965:410-411 4 莫培根,陈钧珊.全国第一届冶金过程物理化学学术报告论文集,上海;上海科学技术出版社,1965:339 5 黄希祜.钢铁冶金原理.北京:冶金工业出版社,1981:159 6 Sommerville I D, Grieveson P, Taylor J. Ironmaking and Steelmaking, 1980; 7: 25 7 万谷志郎.熔渣热力学.东北工学院内部资料,1984 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|