Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (4): 145-147    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMIC STUDY ON SOLUBILITY OF NITROGEN IN GRAY CAST IRON MELTS
ZHAI Qijie;HU Hanqi University of Science and Technology Beijing
Cite this article: 

ZHAI Qijie;HU Hanqi University of Science and Technology Beijing. THERMODYNAMIC STUDY ON SOLUBILITY OF NITROGEN IN GRAY CAST IRON MELTS. Acta Metall Sin, 1991, 27(4): 145-147.

Download:  PDF(267KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The expressions of the dependence of the solubility of nitrogen in the moltengray cast iron on the temperature and composition of melts were advanced under the conditionsof foundry practice. Three gray cast iron specimens with different compositions were examinedin good agreement with derived expression.
Key words:  gray cast iron      nitrogen      solubility     
Received:  18 April 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I4/145

1 翟启杰,马蕊,胡汉起.钢铁研究学报,1990;2(3) :89-94
2 丁培墉.物理化学.北京:冶金工业出版社,1979:105,114-115
3 Hughes I C H. Trans Am Foundrymen's Soc, 1969; 77: 121--133
4 Dawson J V. Foundry Trade J, 1985; 158(3304) : 315--322
5 徐祖耀.金属材料热力学.北京:科学出版社,1981:138
6 马理.北京科技大学学报(物质结构分析和化学分析专辑),1989:(3) :96-100M
[1] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[2] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[3] LI Yuxing, LIU Xinghao, WANG Cailin, HU Qihui, WANG Jinghan, MA Hongtao, ZHANG Nan. Research Progress on Corrosion Behavior of Gaseous CO2 Transportation Pipelines Containing Impurities[J]. 金属学报, 2021, 57(3): 283-294.
[4] PENG Yun,SONG Liang,ZHAO Lin,MA Chengyong,ZHAO Haiyan,TIAN Zhiling. Research Status of Weldability of Advanced Steel[J]. 金属学报, 2020, 56(4): 601-618.
[5] Shasha YANG,Feng YANG,Minghui CHEN,Yunsong NIU,Shenglong ZHU,Fuhui WANG. Effect of Nitrogen Doping on Microstructure and Wear Resistance of Tantalum Coatings Deposited by Direct Current Magnetron Sputtering[J]. 金属学报, 2019, 55(3): 308-316.
[6] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[7] Qingchuan WANG, Bingchun ZHANG, Yibin REN, Ke YANG. Research and Application of Biomedical Nickel-Free Stainless Steels[J]. 金属学报, 2017, 53(10): 1311-1316.
[8] Yibin REN, Haochuan ZHAO, Ke YANG. Study on Lightweight Design and Biomechanical Property of High Nitrogen Nickel Free Stainless Steel Plate: Effect of Thickness Thinning[J]. 金属学报, 2017, 53(10): 1331-1336.
[9] Yanxin QIAO,Shuo WANG,Bin Liu,Yugui ZHENG,Huabing LI,Zhouhua JIANG. SYNERGISTIC EFFECT OF CORROSION AND CAVITATION EROSION OF HIGH NITROGEN STAINLESS STEEL[J]. 金属学报, 2016, 52(2): 233-240.
[10] Zhibin FAN, Xiaoping LIN, Yun DONG, Jie YE, Chan LI, Bo LI. AGE-HARDENING RESPONSE FOR Mg96.17Zn3.15Y0.5Zr0.18 SOLID SOLUTION ALLOY UNDER HIGH PRESSURE[J]. 金属学报, 2016, 52(12): 1491-1496.
[11] LI Dongjie, LU Shanping, LI Dianzhong, LI Yiyi. INVESTIGATION OF THE MICROSTRUCTURE AND IMPACT PROPERTIES OF THE HIGH NITROGEN STAINLESS STEEL WELD[J]. 金属学报, 2013, 49(2): 129-136.
[12] LEI Mingkai WANG Kesheng OU Yi Xiang ZHANG Lei. PLASMA–BASED LOW–ENERGY NITROGEN ION IMPLANTATION OF 2Cr13 MARTENSITIC STAINLESS STEEL USED IN PUMPS AND VALVES[J]. 金属学报, 2011, 47(12): 1490-1494.
[13] XU Mingzhou WANG Jianjun LIU Chunming. LOW TEMPERATURE DEFORMATION BEHAVIOR OF HIGH–NITROGEN NICKEL–FREE AUSTENITIC STAINLESS STEELS[J]. 金属学报, 2011, 47(10): 1335-1341.
[14] . A Model for Calculating Solubility of Hydrogen in Molten Alloys[J]. 金属学报, 2008, 44(2): 129-133 .
[15] WANG Songtao; YANG Ke; SHAN Yiyin; LI Laifeng. Effects of Cold Deformation on Microstructure And Mechanical Behavior of a High Nitrogen Austenitic Stainless Steel[J]. 金属学报, 2007, 43(7): 713-718 .
No Suggested Reading articles found!