Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (4): 142-144    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMIC PROPERTIES OF Cu-Ce-S AND Cu-Y-S LIQUID SOLUTIONS
LI Guodong;DU Ting Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

LI Guodong;DU Ting Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. THERMODYNAMIC PROPERTIES OF Cu-Ce-S AND Cu-Y-S LIQUID SOLUTIONS. Acta Metall Sin, 1991, 27(4): 142-144.

Download:  PDF(251KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The thermodynamic properties of Cu-Ce-S and Cu-Y-S liquid solutions werestudied by the chemical equilibrium technique at 1200℃. The equilibrium constants and thestandard free energies of CeS or YS formation were determined for the reactions CeS=[Ce]+[S]and YS=[Y]+[S]. For the solutions of Ce_((1)) and Y_((1)), in pure Cu according to the reactions:Ce_((1))=[Ce], and Y_((1))=[Y], the standard free energies of solutions were found. The first orderand second order interaction coefficients between solute elements as well as the activity coeffi-ciants γ_C~0 and γ_Y~0 in liquid Cu were also determined.
Key words:  Cu-Ce-S systcm      Cu-Y-S system      thermodynamic property     
Received:  18 April 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I4/142

1 Sigworth G K, Elliott J F. Can Metall Q, 1974; 13: 455
2 大石敏雄,小野胜敏.日本金属学会会报,1986;25:291
3 Niemelae J, Taskinen P. Scand J Metall, 1984; 15: 382
4 Turkdogan E T. Physical Chemistry of High Temperature Technology, New York: Academic Press. 1980: 9
5 Wilson W G, Kay D A R, Vahed A. J Met, 1974; 26(5) : 1
[1] HUANGFU Hao, WANG Zilong, LIU Yongli, MENG Fanshun, SONG Jiupeng, QI Yang. A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties[J]. 金属学报, 2022, 58(2): 231-240.
[2] Ronghua CUI, Xinyu WANG, Zhengchao DONG, Chonggui ZHONG. First Principles Study on Elastic and Thermodynamic Properties of Mg1-xZnx Alloys[J]. 金属学报, 2017, 53(9): 1133-1139.
[3] ZHANG Xudong, WANG Shaoqing. FIRST-PRINCIPLES INVESTIGATION OF THE THERMODYNAMICS PROPERTIES OF Al3Sc AND Al3Zr INTERMETALLICS[J]. 金属学报, 2013, 29(4): 501-505.
[4] WEI Bingbo; DONG Changxing(Northwestern Polytechnical University; Xi'an 710072)(Manuscript received 1995-09-25). HYPERCOOLING AND THERMODYNAMIC PROPERTIES OF LIQUID Ni-Fe ALLOYS[J]. 金属学报, 1996, 32(4): 357-362.
[5] ZENG Wenming;CHEN Nianyi(Shanghai Institute of Metallurgy;Chinese Academy of Sciences;Shanghai 200050);YE Dalun(Kunming University of Science and Technology; Kunming 650093)(Manuscript received 1995-10-24;in revised form 1996-08-13). THERMODYNAMIC PROPERTIES OF Sn-Sb ALLOYS[J]. 金属学报, 1996, 32(12): 1233-1237.
[6] CHEN Qiyuan; ZENG Wenming; ZHANG Pingmin (Central-South University of Technology; Changsha 410083)GU Songqing; YANG Guanqun; ZHOU Huifang; YIN Zhonglin (Zhengzhou Research institute of Light Metals; Zhengzhou 450041) (Manuscript received 1995-02-23; in revised form 1995-06-29). THERMODYNAMIC PROPERTIES OF SOME ALUMINUM COMPOUNDS[J]. 金属学报, 1996, 32(1): 6-14.
[7] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
[8] XU Qian;QIU Zhuxian Northeast University of Technology; Shenyang. CALCULATION OF THERMODYNAMIC PROPERTIES OF LiF-AlF_3 MELTS[J]. 金属学报, 1993, 29(9): 60-64.
[9] FU Zhiping;LU Dongliang;ZHAN Qianbao;ZHOU Jicheng Shanghai Institute of Metallurgy; Academia Sinica; Correspondent professor; Shanghai Institute of MetaHurgy; Academia Sinica; Shanghai 20050. THERMODYNAMIC PROPERTIES OF HOLE TRAPS A AND B IN GaAs[J]. 金属学报, 1992, 28(5): 59-63.
[10] TAO Dongping Kunming Institute of Technology. PREDICTION ABOUT THERMODYNAMIC PROPERTIES OF TERNARY LIQUID ALLOYS FROM WILSON EQUATION[J]. 金属学报, 1991, 27(6): 92-98.
[11] XU Chi;JIANG Naixiong;CHEN Nianyi Shanghai Institute of Metallurgy; Academia sinica. THERMODYNAMICS OF COMPUTERIZED SIMULATION OF MOLTEN LIF-KF SOLUTION BY MONTE CARLO METHOD[J]. 金属学报, 1991, 27(5): 144-147.
No Suggested Reading articles found!