| MAGNETIC ANISOTROPY OF AS-QUENCHED AMORPHOUS ALLOY RIBBONS |
| XIONG Xiangyuan;HE Kaiyuan Northeast University of Technology; Shenyang |
|
Cite this article:
XIONG Xiangyuan;HE Kaiyuan Northeast University of Technology; Shenyang. MAGNETIC ANISOTROPY OF AS-QUENCHED AMORPHOUS ALLOY RIBBONS. Acta Metall Sin, 1991, 27(3): 121-125.
|
|
|
Abstract The in-plane magnetic anisotropy of as-quenched Fe-base, FeNi-baseand Co-base amorphous alloy ribbons has been studied. The variation of anisotropywith stress relief annealing and the magnetization square dependence on anisotropyconstant were determined. It was found that the in-plane magnetic anisotropy con-sists of two components, i. e., one related to the coupling between magnetostrictionand stress, and the other originated from surface shape effect.
|
|
Received: 18 March 1991
|
1 Fujimori H. In: Luborsky F E ed, Amorphous Metallic Alloys, Vol. Ⅰ, London: Butterworths, 1983: 300--316 2 Morita H, Fujimori H, Obi Y. Appl Phys, 1979; 20: 125--127 3 Takahashi M. Kim C O. Jpn J Appl Phys, 1977; 16: 2061--2062 4 Takahashi M, Ishio S. Jpn J Appl Phys, 1977; 16: 2273--2274 5 Takahashi M, Miyazaki T. Jpn J Appl Phys, 1979; 18: 743--752 6 Miyazaki T, Takahashi M. Jpn J Appl Phys, 1978; 17: 1755--1763 7 Morita H, Obi Y, Fujimori H. In: Steeb S, Warlimont H eds., Rapidly Quenched Metals. Vol. Ⅱ. Amsterdam: North-Holland, 1985: 1283 8 Luborsky F E. Becker J J. McCary R O. IEEE Trans Magn. 1975; MAG-11: 1644 9 Becker J J. AIP Conf Proc, 1975; 29: 204 10 林肇华,戴道生.物理学报,1982;31:871--881 11 Osborn J A. Phys Rev, 1945; 67: 351--357 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|