INTERACTION BETWEEN PRECIPITATED V_4C_3 PARTICLES AND DEFORMATION TWIN
XIE Changsheng Huazhong University of Science and Technology; Wuhan
Cite this article: 

XIE Changsheng Huazhong University of Science and Technology; Wuhan. INTERACTION BETWEEN PRECIPITATED V_4C_3 PARTICLES AND DEFORMATION TWIN. Acta Metall Sin, 1990, 26(6): 75-77.

Download:  PDF(911KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The interfacial cornelation between the precipitated V_4C_3 particles and matrix γ-phase as well as the retarding effect of V_4C_3 particles on the development of deformationtwin have been investigated by using Moire pattern of double diffraction of V_4C_3 and γ-phase.The twinning dislocation may be transformed into interfacial dislocation under external stress,and may be continuously moved through bypass or cross--slip.
Key words:  V_4C_3      deformation twin      Moire pattern     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/75

1 谢长生,曹念荪,崔崑.兵器材料科学与工程,1987;(5) :15
2 谢长生,何向山,崔崑.金属科学与工艺,1987;6(2) :48
3 武钢钢研所.钢铁研究情报,1977;(1) :186
4 Bassett G A, Menter J W, Pashley D W. Proc R Soc London, Ser. A, 1958; 246: 345
5 Mahajan S, Chn G Y. Acta Metall, 1973; 21: 1353B
[1] YU Chenfan, ZHAO Congcong, ZHANG Zhefeng, LIU Wei. Tensile Properties of Selective Laser Melted 316L Stainless Steel[J]. 金属学报, 2020, 56(5): 683-692.
[2] Futao DONG,Fei XUE,Yaqiang TIAN,Liansheng CHEN,Linxiu DU,Xianghua LIU. Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. 金属学报, 2019, 55(6): 792-800.
[3] Yubi GAO, Yutian DING, Jianjun CHEN, Jiayu XU, Yuanjun MA, Dong ZHANG. Evolution of Microstructure and Texture During Cold Deformation of Hot-Extruded GH3625 Alloy[J]. 金属学报, 2019, 55(4): 547-554.
[4] ZHOU Bo, SUI Manling. Generation and Interaction Mechanism of Tension Kink Band in AZ31 Magnesium Alloy[J]. 金属学报, 2019, 55(12): 1512-1518.
[5] Dongdong LI, Lihe QIAN, Shuai LIU, Jiangying MENG, Fucheng ZHANG. Effect of Manganese Content on Tensile Deformation Behavior of Fe-Mn-C TWIP Steels[J]. 金属学报, 2018, 54(12): 1777-1784.
[6] Zhiwei SHAN, Boyu LIU. THE MECHANISM OF {101̅2} DEFORMATION TWINNING IN MAGNESIUM[J]. 金属学报, 2016, 52(10): 1267-1278.
[7] Xinning ZHANG,Yingdong QU,Rongde LI,Junhua YOU. MECHANISM OF CRACK NUCLEATION AND PROPA- GATION OF FERRITE DUCTILE IRON DURING IMPACT FRACTURE UNDER LOW TEMPERATURES[J]. 金属学报, 2015, 51(11): 1333-1340.
[8] GUO Pengcheng, QIAN Lihe, MENG Jiangying, ZHANG Fucheng. MONOTONIC TENSION AND TENSION-COMPRES- SION CYCLIC DEFORMATION BEHAVIORS OF HIGH MANGANESE AUSTENITIC TWIP STEEL[J]. 金属学报, 2014, 50(4): 415-422.
[9] ZHANG Zhibo LIU Zhenyu ZHANG Weina. EFFECT OF VC PARTICLES ON THE STRAIN HARDENING BEHAVIOR OF TWIP STEEL[J]. 金属学报, 2012, 48(9): 1067-1073.
[10] WU Zhiqiang, TANG Zhengyou, LI Huaying,ZHANG Haidong. EFFECT OF STRAIN RATE ON MICROSTRUCTURE EVOLUTION AND MECHANICAL BEHAVIOR OF A LOW C HIGH Mn TRIP/TWIP STEELS[J]. 金属学报, 2012, 48(5): 593-600.
[11] WEN Yuhua ZHANG Wanhu SI Haitao XIONG Renlong PENG Huabei. STUDY ON WORK HARDENING BEHAVIOUR AND MECHANISM OF HIGH SILICON AUSTENITIC HIGH MANGANESE STEEL[J]. 金属学报, 2012, 48(10): 1153-1159.
[12] QIN Xiaomei CHEN Liqing DI Hongshuang DENG Wei. EFFECT OF DEFORMATION TEMPERATURE ON TENSILE DEFORMATION MECHANISM OF Fe-23Mn-2Al-0.2C TWIP STEEL[J]. 金属学报, 2011, 47(9): 1117-1122.
[13] WANG Shuhan LIU Zhenyu ZHANG Weina WANG Guodong. INVESTIGATIONS ON TEMPERATURE DEPENDENCE OF MECHANICAL PROPERTIES AND THE DEFORMATION MECHANISM OF A TWIP STEEL[J]. 金属学报, 2009, 45(5): 573-578.
[14] HUANG Wenke KONG Fanya. MICROSTRUCTURE AND MECHANICAL PROPERTY OF COLD DRAWN HIGH STRENGTH 00Cr18Ni10N STAINLESS STEEL WIRE[J]. 金属学报, 2009, 45(3): 275-279.
[15] RONG Lijian; (Institute of Meial Research; Chinese Academy of Sciences; Shenyang 110015) PING Dehai; LI Yiyi; SHI Changxu (Lab of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). TEM STUDY ON DEFORMATION MICROSTRUCTURE IN A Fe-Mn-Si-Cr-Ni SHAPE MEMORY ALLOY[J]. 金属学报, 1995, 31(9): 399-404.
No Suggested Reading articles found!