Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (6): 57-62    DOI:
Current Issue | Archive | Adv Search |
ON THE ORDERING TRANSFORMATIONS IN Ti_3 Al-Nb ALLOY
LI Dong;ZHOU Jing;CHANG Xin;GUAN Shaoxuan Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

LI Dong;ZHOU Jing;CHANG Xin;GUAN Shaoxuan Institute of Metal Research; Academia Sinica; Shenyang. ON THE ORDERING TRANSFORMATIONS IN Ti_3 Al-Nb ALLOY. Acta Metall Sin, 1990, 26(6): 57-62.

Download:  PDF(2129KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Study was made of the behaviour of ordering transformation in Ti_3Al-Nb alloy, including the ordering at high temperature, the transformation of hightemperature β phase during cooling, and the decomposition of metastable β phaseduring aging. Results show that the ordered primary a_2 and high temperature β inalloy occurred at 1060℃. The transformation of high temperature β phase proceedby β→a_2+ω type during cooling, and the decomposition of metastable β and ωtype proceeded by (β+ω type)_(metastable)→(a_2+β)_(stable) during aging at 700℃.
Key words:  Ti_3Al-Nb alloy      ordering transformation      α_2      β      ω     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/57

1 Sastry S M L, Lipsitt H A. Metall Trans, 1977; 8A: 1543
2 Strychor R, Williams J C, Soffa W A. Metall Trans, 1988; 19A: 225
3 Prasetyo A, Reynaud F, Warlimont H. Acta Metall, 1976; 24: 1009
4 Prasetyo A, Reynaud F, Warlimont H. Acta Metall, 1976; 24: 651
5 Baneriee R, Cahn R W. Acta Metall, 1983; 31: 1721
6 Reynaud P F. J Appl Crystallogr, 1976; 9: 263.
[1] HU Min, ZHOU Shengyu, GUO Jingyuan, HU Minghao, LI Chong, LI Huijun, WANG Zumin, LIU Yongchang. Oxidation Behavior of Micro-Regions in Multiphase Ni3Al-Based Superalloys[J]. 金属学报, 2023, 59(10): 1346-1354.
[2] YAN Mengqi, CHEN Liquan, YANG Ping, HUANG Lijun, TONG Jianbo, LI Huanfeng, GUO Pengda. Effect of Hot Deformation Parameters on the Evolution of Microstructure and Texture of β Phase in TC18 Titanium Alloy[J]. 金属学报, 2021, 57(7): 880-890.
[3] DAI Jincai, MIN Xiaohua, ZHOU Kesong, YAO Kai, WANG Weiqiang. Coupling Effect of Pre-Strain Combined with Isothermal Ageing on Mechanical Properties in a Multilayered Ti-10Mo-1Fe/3Fe Alloy[J]. 金属学报, 2021, 57(6): 767-779.
[4] LI Jinshan, TANG Bin, FAN Jiangkun, WANG Chuanyun, HUA Ke, ZHANG Mengqi, DAI Jinhua, KOU Hongchao. Deformation Mechanism and Microstructure Control of High Strength Metastable β Titanium Alloy[J]. 金属学报, 2021, 57(11): 1438-1454.
[5] LIU Xianfeng, LIU Dong, LIU Renci, CUI Yuyou, YANG Rui. Microstructure and Tensile Properties of Ti-43.5Al-4Nb-1Mo-0.1B Alloy Processed by Hot Canned Extrusion[J]. 金属学报, 2020, 56(7): 979-987.
[6] WANG Xi,LIU Renci,CAO Ruxin,JIA Qing,CUI Yuyou,YANG Rui. Effect of Cooling Rate on Boride and Room Temperature Tensile Properties of β-Solidifying γ-TiAl Alloys[J]. 金属学报, 2020, 56(2): 203-211.
[7] Sensen HUANG,Yingjie MA,Shilin ZHANG,Min QI,Jiafeng LEI,Yaping ZONG,Rui YANG. Influence of Alloying Elements Partitioning Behaviors on the Microstructure and Mechanical Propertiesin α+β Titanium Alloy[J]. 金属学报, 2019, 55(6): 741-750.
[8] Xiaohua MIN, Li XIANG, Mingjia LI, Kai YAO, Satoshi EMURA, Congqian CHENG, Koichi TSUCHIYA. Effect of {332}<113> Twins Combined with Isothermal ω-Phase on Mechanical Properties in Ti-15Mo Alloy with Different Oxygen Contents[J]. 金属学报, 2018, 54(9): 1262-1272.
[9] Mingliang HUANG, Hongyu SUN. Interaction Between β-Sn Grain Orientation and Electromigration Behavior in Flip-Chip Lead-Free Solder Bumps[J]. 金属学报, 2018, 54(7): 1077-1086.
[10] Yizhe MAO, Jianguo LI, Lei FENG. Effect of Coarse β(Al3Mg2) Phase on Microstructure Evolution in 573 K Annealed Al-10Mg Alloy by Uniaxial Compression[J]. 金属学报, 2018, 54(10): 1451-1460.
[11] Likui NING,Jian TONG,Enze LIU,Zheng TAN,Huisi JI,Zhi ZHENG. Effect of Ru on the Solidification Microstructure of a Ni-Based Single Crystal Superalloy with High Cr Content[J]. 金属学报, 2017, 53(4): 423-432.
[12] Bing CHEN,Changyuan GAO,Jiao HUANG,Yajing MAO,Meiyi YAO,Jinlong ZHANG,Bangxin ZHOU,Qiang LI. Corrosion Behavior of Second Phase Alloys of β-(Nb, Zr) in Deionized Water at 360 ℃[J]. 金属学报, 2017, 53(4): 447-454.
[13] Yong LI,Mingxing GUO,Ning JIANG,Xukai ZHANG,Yan ZHANG,Linzhong ZHUANG,Jishan ZHANG. PRECIPITATION BEHAVIORS AND PREPARATION OF AN ADVANCED Al-0.93Mg-0.78Si-0.20Cu-3.00Zn ALLOY FOR AUTOMOTIVE APPLICATION[J]. 金属学报, 2016, 52(2): 191-201.
[14] DING Jinjun;ZHAO Gang;HAO Shiming (Department of Materials Science and Engineering; School of Materials and Metallurgy; Northeastern University;Shenyang 110006). PHASE EQUILIBRIUM RELATIONSHIPS OF α_2(α)/γ IN THE Ti-Al-Cr TERNARY SYSTEM[J]. 金属学报, 1998, 34(2): 171-175.
[15] LIN Qin; LI Rong; YE Wen; CHEN Hing (University of Science and Technology Beijing Beijing;Beijing 100083)LIU Renmin (General Research Institute of Non-Ferrous Metals Beijing; Beijing 100088). KINETICS OF HYDROGEN ABSORPTION IN ML-Ni-Co-Mn-Al ALLOYS[J]. 金属学报, 1996, 32(6): 624-628.
No Suggested Reading articles found!