Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (6): 10-14    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF AUSTENITE DEFORMATION ON ISOTHERMAL NUCLEATION INCUBATION TIME OF PRO-EUTECTOID FERRITE
LI Jian;SUN Fuyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing
Cite this article: 

LI Jian;SUN Fuyu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. EFFECT OF AUSTENITE DEFORMATION ON ISOTHERMAL NUCLEATION INCUBATION TIME OF PRO-EUTECTOID FERRITE. Acta Metall Sin, 1990, 26(6): 10-14.

Download:  PDF(413KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A calculation method for the isothermal nucleation incubation timeof pre-eutectoid ferrite from deformed austenite has been developed by introducingFeder's incubation time expression into the decomposition of dsformed austenite.The effects of austenite deformation stored enerey and austenite grain boundary en-ergy change on the incubation time have been theoretically calculated. The calcula-ted result seems to be consistent with a rule of experimental data that the austenitedeformation stored energy and the change of austenite grain boundary energy arethe nature of austenite deformation affecting upon the ferrite nucleation.
Key words:  deformed austenite      ferrite      incubation time     
Received:  18 June 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I6/10

1 Cuddy L J. Metall Trans, 1981; 12A: 1313
2 Roberts W, Lidefelt H, Sandberg A. In: Sellars C M, Davies G J eds., Hot Working and Forming Processes, London: The Metals Society, 1980: 38
3 Sandberg A, Roberts W. In: DeArdo A J, Ratz G A, Wary P J eds., Thermomechanical Processing of Microalloyed Austenite, TMS-AIME, 1982: 405
4 Amin R K, Pickering F B. In: DeArdo A J, Ratz G A, Wary P J eds., Thermomechanical Processing of Microalloyed Austenite, TMS-AIME, 1982: 377
5 Ouchi C, Sampei T, Kozasu I.Trans Iron Steel Inst Jpn, 1982; 22: 214
6 Feder J, Russell K C, Lothe J, Pound G M. Adv Phys, 1966; 15: 111
7 Aaronson H I, Lee J K. In: Aaronson H I ed, Lectures on the theory of Phase Transformations, New York: TMS-AIME, 1975: 83
8 Gauties E, Simon A. In: Proc Int Conf on Phase Transformation, Abstract, Cambridge, 1987
9 徐祖耀.见:徐祖耀,李鹏兴主编,材料科学导论.上海科学技术出版社,1986:274
10 Kaufman L, Radcliffe S V, Cohen M. In: Zackay V F, Aaronson H I eds., Decomposition of Austenite by Diffusional Processes, London: Interscience, 1962; 313
11 Suzuki S, Weatherly G C, Houghton D C. Acta Metall, 1987; 35: 341
12 Wells C, Mehl R F. Trans AIME, 1941; 145: 315
13 Enomoto M, Aaronson H I. Metall Trans, 1986; 17A: 1385
14 Lange W F III, Enomoto M, Aaronson H I. Metall Trans, 1988; 19A: 427
15 李箭.冶金工业部钢铁研究总院博士学位论文,198
[1] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[2] CHENG Yuanyao, ZHAO Gang, XU Deming, MAO Xinping, LI Guangqiang. Effect of Austenitizing Temperature on Microstructures and Mechanical Properties of Si-Mn Hot-Rolled Plate After Quenching and Partitioning Treatment[J]. 金属学报, 2023, 59(3): 413-423.
[3] HOU Xuru, ZHAO Lin, REN Shubin, PENG Yun, MA Chengyong, TIAN Zhiling. Effect of Heat Input on Microstructure and Mechanical Properties of Marine High Strength Steel Fabricated by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(10): 1311-1323.
[4] SUN Yi, ZHENG Qinyuan, HU Baojia, WANG Ping, ZHENG Chengwu, LI Dianzhong. Mechanism of Dynamic Strain-Induced Ferrite Transformation in a 3Mn-0.2C Medium Mn Steel[J]. 金属学报, 2022, 58(5): 649-659.
[5] PENG Jun, JIN Xinyan, ZHONG Yong, WANG Li. Influence of Substrate Surface Structure on the Galvanizability of Fe-16Mn-0.7C-1.5Al TWIP Steel Sheet[J]. 金属学报, 2022, 58(12): 1600-1610.
[6] Xingpin CHEN,Wenjia LI,Ping REN,Wenquan CAO,Qing LIU. Effects of C Content on Microstructure and Properties ofFe-Mn-Al-C Low-Density Steels[J]. 金属学报, 2019, 55(8): 951-957.
[7] Hao CHEN, Congyu ZHANG, Jianing ZHU, Zenan YANG, Ran DING, Chi ZHANG, Zhigang YANG. Austenite/Ferrite Interface Migration and Alloying Elements Partitioning: An Overview[J]. 金属学报, 2018, 54(2): 217-227.
[8] Ke ZHANG, Zhaodong LI, Fengli SUI, Zhenghai ZHU, Xiaofeng ZHANG, Xinjun SUN, Zhenyi HUANG, Qilong YONG. Effect of Cooling Rate on Microstructure Evolution and Mechanical Properties of Ti-V-Mo Complex Microalloyed Steel[J]. 金属学报, 2018, 54(1): 31-38.
[9] Liming DONG,Li YANG,Jun DAI,Yu ZHANG,Xuelin WANG,Chengjia SHANG. Effect of Mn, Ni, Mo Contents on Microstructure Transition and Low Temperature Toughness of Weld Metal for K65 Hot Bending Pipe[J]. 金属学报, 2017, 53(6): 657-668.
[10] Jun ZHANG,Wenxiong CHEN,Chengwu ZHENG,Dianzhong LI. Phase-Field Modeling of Austenite-to-Ferrite Transformation in Fe-C-Mn Ternary Alloys[J]. 金属学报, 2017, 53(6): 760-768.
[11] Fengyu SONG,Yanmei LI,Ping WANG,Fuxian ZHU. EFFECTS OF HEAT INPUT ON THE MICROSTRUC-TURE AND IMPACT TOUGHNESS OF WELD METAL PROCESSED BY A NEW FLUXNOVEL FLUX CORED WIRE WELD[J]. 金属学报, 2016, 52(7): 890-896.
[12] Xuelin WANG,Liming DONG,Weiwei YANG,Yu ZHANG,Xuemin WANG,Chengjia SHANG. EFFECT OF Mn, Ni, Mo PROPORTION ON MICRO-STRUCTURE AND MECHANICAL PROPERTIESOF WELD METAL OF K65 PIPELINE STEEL[J]. 金属学报, 2016, 52(6): 649-660.
[13] Jun ZHANG,Chengwu ZHENG,Dianzhong LI. MODELING OF ISOTHERMAL AUSTENITE TO FERRITE TRANSFORMATION IN A Fe-CALLOY BY PHASE-FIELD METHOD[J]. 金属学报, 2016, 52(11): 1449-1458.
[14] Huidong WU,Chi ZHANG,Wenbo LIU,Zhigang YANG. SIMULATION OF GROWTH KINETICS OF PRO-EUTECTOID FERRITE USING MIXED CONTROL MODEL WITH CONSIDERATION OF DISLOCATION INTERACTION[J]. 金属学报, 2015, 51(9): 1136-1144.
[15] Lei WANG,Di TANG,Yong SONG. AUSTENITE TRANSFORMING IN CONTINUOUS COOLING PROCESS UNDER DIFFUSION CONTROL MODEL[J]. 金属学报, 2015, 51(11): 1341-1348.
No Suggested Reading articles found!