Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (5): 39-43    DOI:
Current Issue | Archive | Adv Search |
IMPROVEMENT ON FATIGUE LIFE OF Ti-6Al-4V ALLOY BY CARBON ION IMPLANTATION
ZHANG Dawei;YU Weicheng;WANG Zhongguang Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

ZHANG Dawei;YU Weicheng;WANG Zhongguang Institute of Metal Research; Academia Sinica; Shenyang. IMPROVEMENT ON FATIGUE LIFE OF Ti-6Al-4V ALLOY BY CARBON ION IMPLANTATION. Acta Metall Sin, 1990, 26(5): 39-43.

Download:  PDF(1547KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The fatigue limit of Ti-6Al-4V alloy could be improved over 28% byimplantation of a dose of 3×10~(17) ion/cm~2 of C at 80 keV under stress-controlledtension-zero condition. The microstructure of surface layer, whether implanted ornot, and before or after fatiguing, as well as the concentration distribution of imp-lanted ion along the depth of surface layer were examined by SEM, TEM andSIMS. A great deal of radiation damages and a good many fine TiC particles arefound in the implanted layer. The fatigue cracking origins, implanted or not, occurin subsrface under lower stress and longer fatigue life. And the implanting speciesdiffuse into substrate under cyclic loading.
Key words:  surface modification      ion implantation      fatigue     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/39

1 McCafferty E, Hubler G K, Natishan P M, Moore P G. Kant R A, Sartwell B D. Mater Sci Eng, 1987; 86: 1
2 Mchargue C J. Int Met Rev, 1986; 31(2) : 58
3 张大伟,于维成,王中光.腐蚀科学与防护技术.1990;2(1)
4 Vardiman R G, Kant R A. J Appl Phys, 1982; 53: 690
5 Hutchings R. Mater Sci Eng, 1985; 69: 135
6 Eylon D, Pierce C M. Metall Trans, 1976; 7A: 111
7 Neal D F, Blenkinsop P A. Acta Metall, 1976; 24: 59
8 Friedel,J,王煜译.位错,北京:科学出版社,1980:67
[1] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[2] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[3] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[6] ZHANG Bin, TIAN Da, SONG Zhuman, ZHANG Guangping. Research Progress in Dwell Fatigue Service Reliability of Titanium Alloys for Pressure Shell of Deep-Sea Submersible[J]. 金属学报, 2023, 59(6): 713-726.
[7] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[8] GAO Han, LIU Li, ZHOU Xiaoyu, ZHOU Xinyi, CAI Wenjun, ZHOU Hongling. Preparation and Bioactivity of Micro-Nano Structure on Ti6Al4V Surface[J]. 金属学报, 2023, 59(11): 1466-1474.
[9] QI Zhao, WANG Bin, ZHANG Peng, LIU Rui, ZHANG Zhenjun, ZHANG Zhefeng. Effects of Stress Ratio on the Fatigue Crack Growth Rate Under Steady State of Selective Laser Melted TC4 Alloy with Defects[J]. 金属学报, 2023, 59(10): 1411-1418.
[10] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[11] ZHOU Hongwei, GAO Jianbing, SHEN Jiaming, ZHAO Wei, BAI Fengmei, HE Yizhu. Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature[J]. 金属学报, 2022, 58(8): 1013-1023.
[12] SONG Wenshuo, SONG Zhuman, LUO Xuemei, ZHANG Guangping, ZHANG Bin. Fatigue Life Prediction of High Strength Aluminum Alloy Conductor Wires with Rough Surface[J]. 金属学报, 2022, 58(8): 1035-1043.
[13] CUI Zhenduo, ZHU Jiamin, JIANG Hui, WU Shuilin, ZHU Shengli. Research Progress of the Surface Modification of Titanium and Titanium Alloys for Biomedical Application[J]. 金属学报, 2022, 58(7): 837-856.
[14] TIAN Ni, SHI Xu, LIU Wei, LIU Chuncheng, ZHAO Gang, ZUO Liang. Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate[J]. 金属学报, 2022, 58(6): 760-770.
[15] YANG Qinzheng, YANG Xiaoguang, HUANG Weiqing, SHI Duoqi. Propagation Behaviors of Small Cracks in Powder Metallurgy Nickel-Based Superalloy FGH4096[J]. 金属学报, 2022, 58(5): 683-694.
No Suggested Reading articles found!