Acta Metall Sin  1990, Vol. 26 Issue (4): 87-92    DOI:
Current Issue | Archive | Adv Search |
EXTRACTION OF Zn AND Cd FROM CHLORIDE SOLUTIONS BY TRI-n-BUTYL PHOSPHATE
JIANG Tao;SU Yuanfu East China University of Chemical Technology; Shanghai
Cite this article: 

JIANG Tao;SU Yuanfu East China University of Chemical Technology; Shanghai. EXTRACTION OF Zn AND Cd FROM CHLORIDE SOLUTIONS BY TRI-n-BUTYL PHOSPHATE. Acta Metall Sin, 1990, 26(4): 87-92.

Download:  PDF(533KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Studies have been made on the extraction of Zn and Cd by TBP (tri-n-butyl phosphate) from diluent HCl solutions of NaCl. The experiments show thatthe species extracted from dilueat HCl solutions of NaCl appear to be predominatelyZnCl_2·2TBP and CdCl_2·2TBP. For Cd, at lower acidities, anionic complexes of thetype HCdCl_3 are also extracted. As the acidity is increased, the type H_2CdCl_4 ap-pears to be predominate complexes in organic phase. For Zn, the acido-complexes ofthe type HZnCl_3 appear in organic phase after the acidity of solutions reachs a cer-tain value ([HCl]>0.1 mol/L). Furthermore, the ultraviolet absorption spectra ofboth aqueous and organic phases have been studied, and the infrared spectra of theorganic phases have been examined. The extraction mechanism and temperaturedependence are also discussed.
Key words:  extraction      solvent extraction      Zn      Cd      tri-n-butyl phosphate      zinc chloride     
Received:  18 April 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I4/87

1 Morris D F C, Short E J. J Chem Soc, 1962; (7) : 2662
2 Forrest V M P, Scargill D, Spickernell, D R. J Inorg Nucl Chem, 1969; 31: 187
3 Ishimori T, Watanabe K, Nakamura E. Bull Chem Soc Jpn, 1960; 33: 636
4 Sato T. J Appl Chem Biotechnol, 1972; 22: 123
5 株洲冶炼厂编.有色冶金中元素的分离与测定,北京:冶金工业出版社,1979:538
6 徐光宪,王文清,吴谨光,高宏成,施鼐,萃取化学原理,上海:上海科学技术出版社,1984:26
7 Кузницов.孙彦昕,邓佐卿,毕木天译.萃取过程的化学机理,北京:中国工业出版社,1965:193
[1] WANG Zongpu, WANG Weiguo, Rohrer Gregory S, CHEN Song, HONG Lihua, LIN Yan, FENG Xiaozheng, REN Shuai, ZHOU Bangxin. {111}/{111} Near Singular Boundaries in an Al-Zn-Mg-Cu Alloy Recrystallized After Rolling at Different Temperatures[J]. 金属学报, 2023, 59(7): 947-960.
[2] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[3] SHEN Gang, ZHANG Wentai, ZHOU Chao, JI Huanzhong, LUO En, ZHANG Haijun, WAN Guojiang. Mechanical Properties and Degradation Behavior of Hot-Extruded Zn-2Cu-0.5Zr Alloy[J]. 金属学报, 2022, 58(6): 781-791.
[4] YUAN Bo, GUO Mingxing, HAN Shaojie, ZHANG Jishan, ZHUANG Linzhong. Effect of 3%Zn Addition on the Non-Isothermal Precipitation Behaviors of Al-Mg-Si-Cu Alloys[J]. 金属学报, 2022, 58(3): 345-354.
[5] ZHU Liang, GUO Mingxing, YUAN Bo, ZHUANG Linzhong, ZHANG Jishan. Effect of Ageing Routes on Precipitation Behaviors of Al-0.7Mg-0.5Si-0.2Cu-0.5Zn Alloy[J]. 金属学报, 2020, 56(7): 997-1006.
[6] Yaohong LIU,Zhaohui WANG,Ke LIU,Shubo LI,Wenbo DU. Effects of Er on Hot Cracking Susceptibility of Mg-5Zn-xEr Magnesium Alloys[J]. 金属学报, 2019, 55(3): 389-398.
[7] Zhipeng WAN, Tao WANG, Yu SUN, Lianxi HU, Zhao LI, Peihuan LI, Yong ZHANG. Dynamic Softening Mechanisms of GH4720Li AlloyDuring Hot Deformation[J]. 金属学报, 2019, 55(2): 213-222.
[8] ZHU Shang,LI Zhihui,YAN Lizhen,LI Xiwu,ZHANG Yongan,XIONG Baiqing. Effects of Zn Addition on the Natural Ageing Behavior and Bake Hardening Response of a Pre-Aged Al-Mg-Si-Cu Alloy[J]. 金属学报, 2019, 55(11): 1395-1406.
[9] Yusheng ZHANG, Youbin WANG, Chunmin LI, Bingtao ZHOU, Keke CHENG, Yuezhou WEI. Preparation and Corrosion Resistance of the ZnAl-LDHs Film on 6061 Al Alloy Surface[J]. 金属学报, 2018, 54(10): 1417-1427.
[10] Di FENG, Xinming ZHANG, Hongmei CHEN, Yunxue JIN, Guoying WANG. Effect of Non-Isothermal Retrogression and Re-Ageing on Microstructure and Properties of Al-8Zn-2Mg-2Cu Alloy Thick Plate[J]. 金属学报, 2018, 54(1): 100-108.
[11] Ronghua CUI, Xinyu WANG, Zhengchao DONG, Chonggui ZHONG. First Principles Study on Elastic and Thermodynamic Properties of Mg1-xZnx Alloys[J]. 金属学报, 2017, 53(9): 1133-1139.
[12] Yi CHEN, Mingxing GUO, Long YI, Bo YUAN, Gaojie LI, Linzhong ZHUANG, Jishan ZHANG. Optimization and Controlling on the Microstructure, Texture and Properties of an Advanced Al-Mg-Si-Cu-Zn Alloy Sheet[J]. 金属学报, 2017, 53(8): 907-917.
[13] Ye ZHOU,Pingli MAO,Zhi WANG,Zheng LIU,Feng WANG. Investigations on Hot Tearing Behavior of Mg-7Zn-xCu-0.6Zr Alloys[J]. 金属学报, 2017, 53(7): 851-860.
[14] Xiuling SHANG,Bo ZHANG,Wei KE. Effect of Sb-Rich Intermetallic Phase on the CorrosionResistance of Zn Alloy in Near-Neutral and Acidic Solutions[J]. 金属学报, 2017, 53(3): 351-357.
[15] Tingfei XI, Lina WEI, Jing LIU, Xiaoli LIU, Zhen ZHEN, Yufeng ZHENG. Research Progress in Bioresorbable Magnesium Scaffolds[J]. 金属学报, 2017, 53(10): 1153-1167.
No Suggested Reading articles found!