| FRACTAL DIMENSION OF CAVITIES SHAPE CHANGES DURING SUPERPLASTIC DEFORMATION OF HIGH STRENGTH Al ALLOY 7475 |
| JIANG Xinggang;CUI Jianzhoug;MA Longxiang Northeast University of Technology; Shenyang Box 317; Northeast University of Technology; Shenyang 110006 |
|
Cite this article:
JIANG Xinggang;CUI Jianzhoug;MA Longxiang Northeast University of Technology; Shenyang Box 317; Northeast University of Technology; Shenyang 110006. FRACTAL DIMENSION OF CAVITIES SHAPE CHANGES DURING SUPERPLASTIC DEFORMATION OF HIGH STRENGTH Al ALLOY 7475. Acta Metall Sin, 1990, 26(4): 144-147.
|
|
|
Abstract The fractal dimension changes of cavities have been determined duringsuperplastic deformation of the high strength Al alloy 7475 with different strain,temperature, strain rate and grain size. The fractal dimension of cavities may in-crease with the increase of strain. It becomes higher as the alloy deformed underthe lower temperature, the greater strain rate and the coarser grain size. The alloywould be approaching to rupture if the fractal dimension of cavities raised to acertain extent.
|
|
Received: 18 April 1990
|
1 Pilling J, Ridley N. Res Mech, 1988; 23: 31 2 穆在勤,龙期威.金属学报,1988;24:A142 3 苏辉,张玉贵,阎振棨,金属学报,1989:25:A466 4 Pande C S, Richards L E, Louat N, Dempsey B D, Schwoeble A J. Acta Metall, 1987; 35: 1633 5 Mandelbrot B B, Passoja DE, Paullay A J. Nature, 1984; 308: 721 6 Lung C W, Mu Z Q. Phys Rev, 1988; 38B: 11781N |