| INTERACTION OF Ce AGAINST Cu, P OR Ti IN Fe-BASE SOLUTION |
| WANG Yuekui;DU Ting Central Iron and Steel Rasearch Institute; Ministry of Metallurgical Industry; Beijing professor;Department No.16;Central Iron and Steel Research Institute; Ministry of Metallurgical Industry;Beijing 100081 |
|
Cite this article:
WANG Yuekui;DU Ting Central Iron and Steel Rasearch Institute; Ministry of Metallurgical Industry; Beijing professor;Department No.16;Central Iron and Steel Research Institute; Ministry of Metallurgical Industry;Beijing 100081. INTERACTION OF Ce AGAINST Cu, P OR Ti IN Fe-BASE SOLUTION. Acta Metall Sin, 1990, 26(3): 150-152.
|
|
|
Abstract The equilibrium products of Fe-Cu-Ce, Fe-P-Ce or Fe-Ti-Ce solution have beenidentified to be Ce_2O_2S, but not the intermetallic compounds of Ce against Cu, P or Ti.The equilibrium constant of Ce_2O_2S=2[Ce]+[O]+2[S] and the interaction coefficients betweensolutes in Fe-base solution have been determined as follows: K_(Ce_2O_2S)=2.57×10~(-15) e_(Ce)~(Cu)=-0.49; e_(Ce)~P=1.77; e_(Ce)~(Ti)=-3.62 e_(Cu)~(Ce)=-0.22; e_P~(Ce)=0.39; e_(Ti)~(Ce)=-1.23 ε_(Ce)~(Cu)=-128.0; ε_(Ce)~P=224.1; ε_(Ce)~(Ti)=-710.0The Ce decreases the activities of Cu and Ti in Fe-base solution and increases their solubilities,as well as increases the activity of P and decreases its solubility.
|
|
Received: 18 March 1990
|
1 周谦莉,杜挺.金属学报,1989;25:B11 2 Gschneidner K K Jr., Verkade M E. Selected Cerium Phase Diagrams, IS-RIC-7, Ames, Iowa: Iowa State University, 1974: 17 3 乐可襄,杜挺,李继宗,沈汝美.金属学报,1987;23:A99 4 Wu Yieming, Wang Longmei, Du Ting. J Less Common Met, 1985; 110: 187 5 Sigworth G K, Elliott J F. Met Sci, 1974: 8: 298 6 韩其勇.北京钢铁学院学报,1986;3:115 7 王常珍,王福珍,杜英敏,张小平.金属学报,1980;16:83 8 韩其勇,项长祥,董元篪,杨斯馥.钢铁,1984;19(7) :9 9 周谦莉,杜挺.钢铁研究总院学报,1988;8:55 10 唱鹤鸣,杜挺,余景生.钢铁研究总院学报,1988;8:93 11 唱鹤鸣,杜挺,余景生.金属学报,1989;25:B140K |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|