SUBSTRUCTURAL ALTERATION OF STAINLESS STEEL DURING CONSTANT STRAIN FATIGUE
WANG Jingyi;TAN Yuxu;MA Zenghai Xi'an Institute of Technology Xi'an Jiaotong University associate professor;Institute of Metallic Materials and Strength;Xi'an; Jiaotong University; Xi'an 710049
Cite this article:
WANG Jingyi;TAN Yuxu;MA Zenghai Xi'an Institute of Technology Xi'an Jiaotong University associate professor;Institute of Metallic Materials and Strength;Xi'an; Jiaotong University; Xi'an 710049. SUBSTRUCTURAL ALTERATION OF STAINLESS STEEL DURING CONSTANT STRAIN FATIGUE. Acta Metall Sin, 1990, 26(2): 52-56.
Abstract The alteration of substructure of an austenitic stainless steel hasbeen investigated during constant strain fatigue. No plateau stage on the cyclicstress-strain curve was observed for the stainless steel in contrast with a mono-crystalline pure copper specimen. This may be related to its low stacking fault en-ergy. During strain fatigue under various amplitudes the substructure of dislocationin austenite alterates correspondingly. It revealed to be associated with the appear-ance change of the cyclic stress-strain curve.
1 Buchinger L, Laird C. Mater Sci Eng, 1985; 76: 71 2 Buchinger L, Stanzl S. Philos Mag, A, 1984; 50: 275 3 Laird C. Mater Sci Eng, 1986; 80: 59 4 谈育煦,任利平,李刚.金属学报,1989;25:A62 5 Murr L E, Staudhammer K P, Hecker S S. Metall Trans, 1982; 13A: 627