| THERMAL STABILITY AND PERPENDICULAR ANISOTROPY OF AMORPHOUS TbFeCo FILMS |
| LU Jian;WANG Yinjun;MA Ruzhang Institute of Physics; Academia Sinica; Beijing University of Science and Technology Beijing LU Jian; Department No.2; Institute of Metallurgy; Shoudu Iron and Steel Company;Beijing 100085 |
|
Cite this article:
LU Jian;WANG Yinjun;MA Ruzhang Institute of Physics; Academia Sinica; Beijing University of Science and Technology Beijing LU Jian; Department No.2; Institute of Metallurgy; Shoudu Iron and Steel Company;Beijing 100085. THERMAL STABILITY AND PERPENDICULAR ANISOTROPY OF AMORPHOUS TbFeCo FILMS. Acta Metall Sin, 1989, 25(6): 108-111.
|
|
|
Abstract The perpendicular anisotropy, coercivity and Kerr rotation angle ofthe amorphous Tb_(32)Fe_(54)Co_(14) films were studied. The X-ray, electron diffraction,XPS and AES profile confirmed that no obvious change in their amorphous struc-ture and oxygen concentration is observed after annealing at 100℃, while theirproperties alter evidently under bending stress. It is believed that the perpendicularanisotropy in the Tb_(32)Fe_(54)Co_(14) film mainly arises from the induced stress duringpreparation and the magnetostriction coupling stress, as well as, the thermalinstability of the film is related closely to the stress relaxation during annealing.
|
|
Received: 18 June 1989
|
1 Hartmann M, Jacobs B A J, Broat J J M. Philips Tech Rev, 1985; 42: 37 2 Katayama T, Hasegawa K, Kawanishi K, Tsushima T. J Appl Phys, 1978; 49: 1759 3 Grundy P J, Lacey E T E, Wright C D. IEEE Trans Magn, 1987; MAG-23: 2632 4 Luborsky F E. IEEE Trans Magn, 1984; MAG-20: 1305 5 Takayama S, Niihara T, Kaneko K, Sugita Y, Ojima M. J Appl Phys, 1987; 61: 2610 6 Yumoto S, Taki K, Tsukamoto Y, Habara T, Okada M, Yokota H, Gokan H. IEEE Trans Magn, 1987; MAG-23: 2605 7 王荫君,唐谦,杨克敏,蔡衡,沈建祥,张绪信.物理学报,1987;36:705 8 Orehard A, Thornton T. J Electron Spectrosc Relat Phenom, 1978; 13: 27 9 Hashimoto S. Ochiai Y, Kaneko M, Watanabe K, Aso K. IEEE Trans Magn, 1987; MAG 23: 2278 10 郭贻诚,王震西.非晶态物理学,北京:科学出版社,1984:426 11 Rour R j,Young W C.汪一麒,汪一骏译.应力应变公式,北京:中国建筑出版社,1985:16 12 Wang Y J, Cai H, Tang Q, Yang K M, Li J Y, Wang J L. J Magn Magn Mater, 1987; 66: 84 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|