| INFLUENCE OF GRAIN SIZE AND ORDERING DEGREE OF PARENT PHASE ON SHAPE MEMORY EFFECT IN A CuZnAl ALLOY CONTAINING BORON |
| WU Jianxin;JIANG Bohong;Hsu T. Y. XU Zuyao Shanghai Jiao Tong University |
|
Cite this article:
WU Jianxin;JIANG Bohong;Hsu T. Y. XU Zuyao Shanghai Jiao Tong University. INFLUENCE OF GRAIN SIZE AND ORDERING DEGREE OF PARENT PHASE ON SHAPE MEMORY EFFECT IN A CuZnAl ALLOY CONTAINING BORON. Acta Metall Sin, 1989, 25(3): 17-22.
|
|
|
Abstract Influence of the grain size and ordering degree of the parent phase onthe shape memory recovery in a Cu-25.62 Zn-3.97 Al-0.0018B (wt-%) memory alloyis investigated. A mathematical relationship is set up between the recovery ratio andordering degree, probability of atoms at their ordered sites, grain size, the widthof the grain boundary affected regions, the stress during deformation, as well as thecritical shear stress. Shape memory effect reaches a maximum with varying grainsize and increases linearly with increasing ordering parameter, that agrees well withexperimental results.
|
|
Received: 18 March 1989
|
1 Perkins J. Mater Sci Eng, 1981; 51: 181 2 Qi X (漆璿), Jiang B H (江伯鸿), Hsu T Y (Xu Zuyao) (徐祖耀). Mater Sci Eng, 1987; 93: 205 3 Miyazaki S, Otsuka K, Sakamoto H, Shimizu K. Trans Jpn Inst Met, 1981; 4: 244 4 Lee J S. Wayman C M. Metallography, 1986; 19: 401 5 Adnyana D N. Metallography, 1985; 18: 187 6 Melton K N, Mercier O. In: Haason P, Gerold V, Kostorz G eds., Strength of Metals and Alloys, Vol. Ⅱ, Proc 5th Int Conf, Aachen, FRG. Aug. 27--31, 1979, Pergamon Press, 1980: 1243 7 Sugimoto K. J Phys, (Paris), Colloque C4, Supplement au №12, 1982; 43: C4--761 8 Wu J K (吴建新), Jiang B H (江伯鸿), Hsu T Y (Xu Zuyao) (徐祖耀). Acta Metall., 1988; 6: 1521 9 Weibel E R. Morphometry of the Humanlung Berlin: Springer-Verlag, 1963 10 Iain L M. Principle of Mechanical Metallurgy, London: Arnold, 1981: 185 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|