X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST
TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun
Cite this article:
TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST. Acta Metall Sin, 1989, 25(2): 82-84.
Abstract X-ray diffraction Fourier profile analysis has been performed for polycrystallineα-brass plate with 31.55 wt-% Zn after a series of uniaxial tensile tests with differentstrain rates.Dislocation density ρ and configuration parameter M may be presented as a function of appliedstress σ_a. A mechanism of alternative long-range and short-range strain hardening has been pro-posed.
1 Haase P著,肖纪美等译.物理金属学,科学出版社,1984;243 2 Nabarro F R N, Basinski Z S, Holt D B. Adv Phys, 1964; 13: 139 3 Rowe G W. Principles of Industrial Metalworking Processes. London: Arnold, 1977: 308 4 冯端,王业宁,丘第荣.金属物理,(下册),科学出版社,1975:676,697 5 Wang Yuming, Lee Shansan, Lee Yenchin. J Appl Cryst. 1982: 15; 35 6 滕凤恩,李庚新,王永申.吉林大学自然科学学报,待发表 7 Bailey J E, Hirsch P B. Philos Max, 1960; 5: 485 8 Worosin B, Graham R A. Mater Sci Eng, 1984; 66: 73 9 Suh N P, Turner A P L. Elements of the Mechanical Behavior of Solids, New York: McGraw-Hill, 1975[
WANG Huabin; HAN Jiecai; ZHANG Xinhong; DU Shanyi (Center for Composite Materials; Harbin Institute of Technology; Harbin 150001)Correspondent: WANG Huabin; lecturer;Tel: (0451)6414167; Fax: (0451)6415605. REACTION MECHANISM OF CONTINUALLY HEATING Ni AND A1 PARTICLES[J]. 金属学报, 1998, 34(9): 992-998.