| 液态Ni-Fe合金的超过冷与热力学性质 |
| 魏炳波;董长星 |
| 西北工业大学 |
|
| HYPERCOOLING AND THERMODYNAMIC PROPERTIES OF LIQUID Ni-Fe ALLOYS |
| WEI Bingbo; DONG Changxing(Northwestern Polytechnical University; Xi'an 710072)(Manuscript received 1995-09-25) |
引用本文:
魏炳波;董长星. 液态Ni-Fe合金的超过冷与热力学性质[J]. 金属学报, 1996, 32(4): 357-362.
,
.
HYPERCOOLING AND THERMODYNAMIC PROPERTIES OF LIQUID Ni-Fe ALLOYS[J]. Acta Metall Sin, 1996, 32(4): 357-362.
| 1SahmPR,KellerMH,SchieweB.ResearchProgramof theGermanSpacelabMissionD-2.2nded,Kln,Germany:WissenschaftlicheProjecktfhrung//DLR,1993:3632EvansND,HofmeisterWH,BayuzickRJ,RobinsonMB.MetallTrans,1986;17A:9733WeiB,HerlachDM,FeuerbacherB,SommerF.ActaMetallMater,1993;41:18014GomersallDW,ShiraishiSY,WardRG.JAustInstMet,1965;10:2205WillneckerR,HerlachDM,FeuerbacherB.ApplPhysLett,1986;49:13396HofmeisterWH,RobinsonMB,BayuzickRJ.MaterResSocSympProc,1987;87:1497魏炳波,杨根仓,周尧和.金属学报,1990;26:B3438TurnbullD,JChemPhys,1952;20:4119魏炳波,王彬,BarthM,HerlachDM.金属学报,1994;30:B289 |
|