| 四种铁基合金的M■ssbauer谱研究 |
| 王魁香;郝兆印;邓京川;刘密兰;陆国会 |
| 吉林大学 |
|
| M SSBAUER SPECTRA OF FOUR Fe-BASED ALLOYS |
| WANG Kuixiang; HAO Zhaoyin; DENG Jingchuan; LIU Milan; LU Guohui(Jilin University; Changchun 130073)(Manuscript received 1995-06-19; in revised form 1995-09-16) |
引用本文:
王魁香;郝兆印;邓京川;刘密兰;陆国会. 四种铁基合金的M■ssbauer谱研究[J]. 金属学报, 1996, 32(5): 469-473.
,
,
,
,
.
M SSBAUER SPECTRA OF FOUR Fe-BASED ALLOYS[J]. Acta Metall Sin, 1996, 32(5): 469-473.
| 1GonserU著,徐英庭,李哲,李国栋,应育浦译.穆斯堡尔谱学.北京:科学出版社,1979:1082HaoZhaoyin,HeYixing,ChenYufei,WanDerong.JCrystGrowth.,1994;140:4413HuckB,SaurenbachF,HesseJ.HyperfineInteract,1986;28:4794郝兆印,王魁香.高压物理学报,1991;5:1775LomerWM,MarshallW.PhilosMag.1958;3:1856SonmuraT,FujitaFE.JMagnMagnMater,1979;10:2557AdachiH,ImotoS.JPhysSocJpn,1979;46:1194T |
|