| 低碳钢在海水中的阴极电化学行为 |
| 邹妍1); 郑莹莹1); 王燕华1); 王佳 1;2) |
1) 中国海洋大学化学化工学院; 青岛 266100
2) 中国科学院金属研究所金属腐蚀与防护国家重点实验室; 沈阳 110016 |
|
| CATHODIC ELECTROCHEMICAL BEHAVIORS OF MILD STEEL IN SEAWATER |
| ZOU Yan1); ZHENG Yingying1); WANG Yanhua1); WANG Jia1;2) |
1) College of Chemistry and Chemical Engineering; Ocean University of China; Qingdao 266100
2) State Key Laboratory for Corrosion and Protection; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016\par |
引用本文:
邹妍 郑莹莹 王燕华 王佳 . 低碳钢在海水中的阴极电化学行为[J]. 金属学报, 2010, 46(1): 123-128.
,
,
,
.
CATHODIC ELECTROCHEMICAL BEHAVIORS OF MILD STEEL IN SEAWATER[J]. Acta Metall Sin, 2010, 46(1): 123-128.
| [1] Oh S J, Cook D C, Townsend H E. Corros Sci, 1999; 41: 1687
[2] Garc´?a K E, Morales A L, Barrero C A, Greneche J M. Corros Sci, 2006; 48: 2813
[3] Deliyanni E A, Bakoyannakis D N, Zouboulis A I, Matis K A, Nalbandian L. Micropor Mesopor Mater, 2001; 42: 49
[4] Refait P, G´emin J–M R. Corros Sci, 1997; 39: 539
[5] R´emazeilles C, Refait P. Corros Sci, 2007; 49: 844
[6] Ma Y T, Li Y, Wang F H. Mater Chem Phys, 2008; 112: 844
[7] Kamimura T, Hara S, Miyuki H, Yamashita M, Uchid H. Corros Sci, 2006; 48: 2799
[8] Bousselmi L, Fiaud C, Tribollet B, Triki E. Electrochim Acta, 1999; 44: 4357
[9] Antony H, Perrin S, Dillmann P, Legrand L, Chauss´e A. Electrochim Acta, 2007; 52: 7754
[10] Stratmann M, M¨uller J. Corros Sci, 1994; 36: 327
[11] Stratmann M, Bohnenkamp K, Engell H–J. Corros Sci, 1983; 23: 969
[12] Stratmann M, Hovmann K. Corros Sci, 1989; 29: 1329
[13] Stratmann M, Streckel H. Corros Sci, 1990; 30: 697
[14] Misawa T, Asami K, Hashimoto K, Shimodaira S. Corros Sci, 1974; 14: 279
[15] Dillmann P, Mazaudier F, Hoerl´e S. Corros Sci, 2004; 46: 1401
[16] Refait P, Abdelmoula M, G´enin J–M R. Corros Sci, 1998; 40: 1547 |
|