| 动态应变时效对316L不锈钢疲劳蠕变行为的影响 |
| 江慧丰1;2;陈学东1;范志超1;董杰1;2;姜恒1;陆守香2 |
1 合肥通用机械研究院国家压力容器与管道安全工程技术研究中心; 合肥 230031
2 中国科技大学安全科学与工程系; 合肥 230027 |
|
| EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL |
| JIANG Huifeng1;2; CHEN Xuedong1;FAN Zhichao1;DONG Jie1;2;JIANG Heng1;LU Shouxiang2 |
1 National Technology Research Center on Pressure Vessel and Pipeline Safety Engineering; Hefei General Machinery Research Institute; Hefei 230031
2 Department of Safety Science and Engineering; University of Science and Technology of China; Hefei 230027 |
引用本文:
江慧丰 陈学东 范志超 董杰 姜恒 陆守香. 动态应变时效对316L不锈钢疲劳蠕变行为的影响[J]. 金属学报, 2009, 45(3): 326-330.
,
.
EFFECT OF DYNAMIC STRAIN AGING ON FATIGUE--CREEP BEHAVIOR OF 316L AUSTENITIC STAINLESS STEEL[J]. Acta Metall Sin, 2009, 45(3): 326-330.
| [1] Plumbridge W J. J Mater Proc Technol, 1996; 56: 502
[2] Qian K W, Li X Q, Xiao L G. J Fuzhou Univ (Nat Sci), 2001; 29: 8
(钱匡武, 李孝琦, 萧林钢. 福州大学学报(自然科学版), 2001; 29: 8)
[3] Chen W Z, Qian K W. Acta Metall Sin, 1989; 25: 132
(陈文哲, 钱匡武. 金属学报, 1989; 25: 132)
[4] Peng K P, Chen W Z, Qian K W. Acta Metall Sin, 1993; 29: 283
(彭开萍, 陈文哲, 钱匡武. 金属学报, 1993; 29: 283)
[5] Jiang H F, Zhang Q C, Chen X D. Acta Mater, 2007; 55: 2219
[6] Jiang H F, Zhang Q C, Jiang Z Y, Wu X P. Acta Metall Sin, 2005; 41: 727
(江慧丰, 张青川, 蒋震宇, 伍小平. 金属学报, 2005; 41: 727)
[7] Jiang H F, Zhang Q C, Xu Y H, Wu X P. Acta Metall Sin, 2006; 42: 139
(江慧丰, 张青川, 徐毅豪, 伍小平. 金属学报, 2006; 42: 139)
[8] Hong S G, Lee S B, Byun T S. Mater Sci Eng, 2007; A457: 139
[9] Mannan S L. Bull Mater Sci, 1993; 16: 561
[10] Hong S G, Lee S B. J Nucl Mater, 2004; 328: 232
[11] Zhang L, Jiang H F, Jiang H. Pressure Vessel Technology, 2008; 25(7): 6
(张莉, 江慧丰, 姜恒. 压力容器, 2008; 25(7): 6)
[12] Miguel M C, Vespignani A, Zapperi S. Nature, 2001; 410: 667 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|