| 单晶Cu表面黏-滑效应的分子动力学模拟 |
| 程东;严志军;严立 |
| 大连海事大学轮机工程学院; 大连 116026 |
|
| Molecular Dynamic Simulations of the Stick--Slip Phenomenon on the Surface of Cu Single CrystaL |
| CHENG Dong; YAN Zhijun;YAN Li |
| Marine Engineering College; Dalian Maritime University; Dalian 116026 |
引用本文:
程东; 严志军; 严立 . 单晶Cu表面黏-滑效应的分子动力学模拟[J]. 金属学报, 2006, 42(11): 1149-1152 .
,
,
.
Molecular Dynamic Simulations of the Stick--Slip Phenomenon on the Surface of Cu Single CrystaL[J]. Acta Metall Sin, 2006, 42(11): 1149-1152 .
[1] Fujisawa S, Kishi E, Sugawara Y, Morita S. Phys Rev, 1995; 51B: 7849 [2] Gnecco E, Bennewitz R, Socoliuc A, Meyer E. Wear, 2003; 254: 859 [3] Bennewitz R, Gyalog T, Guggisberg M, Bammerlin M, Meyer E, Guntherodt H J. Phys Rev, 1999; 60B: R11301 [4] Tomlinson G A. Philos Mag S, 1929; 77: 905 [5] Gnecco E, Bennewitz R, Gyalog T, Loppacher C, Bammerlin M, Meyer E, Guntherodt H J. Phys Rev Lett, 2000; 84: 1172 [6] Hurtado J A, Kim K S. Proc R Soc London, 1999; 455A: 3363 [7] Rekhviashvili S Sh. Technol Phys, 2002; 47: 140 [8] Sorensen M R, Jacobsen K W, Stoltze P. Phys Rev, 1996; 53B: 2101 [9] Buldum A, Ciraci S. Phys Rev, 1997; 55B: 2606 [10] Buldum A, Ciraci S, Batra I P. Phys Rev, 1998; 57B: 2468 [11] Zhang L C, Tanaka H. Wear, 1997; 211: 44 [12] Krim L. Am J Phys, 2002; 70: 890 [13] Ringlein J, Robbins M O. Am J Phys, 2004; 72: 884 [14] Zhang L C, Johnson K L, Cheong W C D. Tribol Lett, 2001; 10: 23 [15] Rozman M G, Urbakh M, Klafter J. Physica, 1999; 266A: 272 [16] Wadley H N G, Zhou A X, Johnson R A, Neurock M. Prog Mater Sci, 2001; 46: 329 [17] Zhou X W, Wadley H N G, Johnson R A. Acta Mater, 2001; 49: 4005 [18] Haile J M. Molecular Dynamics Simulation: Elementary Methods, New York: John Wiley, 1992 [19] Parrinello M, Rahman A, J Appl Phys, 1981; 52: 7180 [20] Parrinello M, Rahman A. J Chem Phys, 1982; 76: 2662 [21] Cheng D, Yan L, Yan Z J . 3rd Int Conf on Material Processing for Properties and Performance, Singapore: Institute of Materials (East Asia), 2004: 611 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|