| 钢包内喷嘴与透气砖吹氩去夹杂水模型研究 |
| 郑淑国 朱苗勇 |
| 东北大学材料与冶金学院; 沈阳 110004 |
|
| Water Model Study on Removing Inclusions in a Ladle With Argon Injected Through |
| ZHENG Shuguo; ZHU Miaoyong |
| School of Materials and Metallurgy; Northeastern University; Shenyang 110004 |
引用本文:
郑淑国; 朱苗勇 . 钢包内喷嘴与透气砖吹氩去夹杂水模型研究[J]. 金属学报, 2006, 42(11): 1143-1148 .
,
.
Water Model Study on Removing Inclusions in a Ladle With Argon Injected Through[J]. Acta Metall Sin, 2006, 42(11): 1143-1148 .
[1] Murthy G G K, Mehrotra S P. Ironmaking Steelmaking, 1992; 19: 377 [2] Yin H B, Jin S T. Eng Chem Metall, 1994; 15: 202 (尹弘斌,金山同.化工冶金,1994;15:202) [3] Zhou Y, Wang H C, Wang S J, Yue K X, Dong Y C. Steelmaking, 2002; 18(1): 38 (周云,王海川,王世俊,乐可襄,董元篪.炼钢,2002;18(1): 38) [4] Mazumdar D, Guthrie R I L. ISIJ Int, 1995; 35: 1 [5] Chen Y S, He Y D, Huang Z Z. J Baotou Univ Iron Steel Technol, 2003; 22: 297 (陈义胜,贺友多,黄宗泽.包头钢铁学院学报,2003;22:297) [6] Mazumdar D, Evans J W. ISIJ Int, 2004; 44: 447 [7] Ren S B, Chen Y S, Huang Z Z, He Y D. J Baotou Univ Iron Steel Technol, 2002; 21: 313 (任三兵,陈义胜,黄宗泽,贺友多.包头钢铁学院学报,2002; 21:313) [8] Fan C M, Hwang W S. Ironmaking Steelmaking, 2002; 29: 415 [9] Fan C, Liu Z Z, Cai K K, Liu S H, Liang M, Gong F, Liu R N. Iron Steel, 2003; 38(3): 18 (樊晨,刘中柱,蔡开科,刘石虹,梁玫,巩飞,刘瑞宁.钢铁,2003;38(3):18) [10] Lindskog N, Sandberg H. Scandinavian J Metall, 1973; 2: 71 [11] Okumura K, Ban M, Hirasawa M, Sano M, Mori K. ISIJ Int, 1995; 35: 832 [12] Liu X H, Mao Y, Song C, Sun W, Zhang J P, Yang A N, Cai K K. Iron Steel, 2005; 40(2): 27 (刘学华,茆勇,宋超,孙维,张建平,杨阿娜,蔡开科.钢铁,2005;40(2):27) [13] Xue Z L, Wang Y F, Wang L T, Li Z B, Zhang J W. Acta Metall Sin, 2003; 39: 431 (薛正良,王义芳,王立涛,李正邦,张家雯.金属学报,2003; 39:431) [14] Engh T A, Lindskog N. Scand J Metall, 1975; 4: 49 [15] Zhu M Y, Liu J H, Zheng S G. The 3rd China-Korea Joint Symposium on Advanced Steel Technology, Shang hai, 2003: 46 [16] Soder M, Jonsson P, Jonsson L. Steel Res, 2004; 75: 128 [17] Wang L T, Zhang Q Y, Peng S H, Li Z B. ISIJ Int, 2005; 45: 331 [18] Jin Y, Bi X G, Fu L C. Steelmaking, 2005; 21(4): 31 (金炎,毕学工,傅连春.炼钢, 2005;21(4):31) [19] Soder M, Jonsson P, Alexis J. Scand J Metall, 2002; 31: 210 [20] Liu Y B, Wang S J, Zhou Y, Wang H C, Yue K X. J Baotou Univ Iron Steel Technol, 2001; 20: 272 (刘水兵,王世俊,周云,王海川,乐可襄.包头钢铁学院学报,2001;20:272) [21] Iguchi M, Nozawa K, Morita Z I. ISIJ Int, 1991; 31: 952 [22] Zhu M Y. PhD Thesis, Northeastern University, Shenyang, 1994 (朱苗勇.东北大学博士学位论文,沈阳,1994) [23] Zhu M Y, Swada I, Xiao Z Q. Acta Metall Sin, 1995; 31: B346 (朱苗勇,沢田郁夫,肖泽强.金属学报, 1995;31:B346) [24] Ren S B, Chen Y S, Huang Z Z, He Y D. J Baotou Univ Iron Steel Technol, 2003; 22: 193 (任三兵,陈义胜,黄宗泽,贺友多.包头钢铁学院学报,2003; 22:193) [25] Zhu M Y, Xiao Z Q. Maths-physical Modeling of Steel Refining Process. Beijing: Metallurgical Industry Press, 1998: 124 (朱苗勇,萧泽强.钢的精炼过程数学物理模拟.北京:冶金工业出版社, 1998:124) [26] Sahai Y, Emi T. ISIJ Int, 1996; 36: 1166 [27] Zhu M Y, Zheng S G, Huang Z Z, Gu W P. Steel Res, 2005, 76: 718 [28] Wang L H, Lee H G, Hayes P. ISIJ Int, 1996; 36: 7 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|