| B、Sr联合处理Al-7Si合金及细化变质效果评估 |
| 陈 祥 耿慧远 李言祥 |
| 清华大学机械工程系; 先进成形制造教育部重点实验室; 北京100084 |
|
| Combined Treatment of Sr and B and Evaluation of Refinment--Modification |
| CHEN Xiang; GENG Huiyuan; LI Yanxiang |
| Key Laboratory for Advanced Materials Processing Technology; Ministry of Education; Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |
引用本文:
陈祥; 耿慧远; 李言祥 . B、Sr联合处理Al-7Si合金及细化变质效果评估[J]. 金属学报, 2006, 42(11): 1130-1136 .
,
,
.
Combined Treatment of Sr and B and Evaluation of Refinment--Modification[J]. Acta Metall Sin, 2006, 42(11): 1130-1136 .
[1] Croseley E, Mondolfo L F. AFS Trans, 1966; 74: 53 [2] Argyropoulos S, Closset B, Oger H. AFS Trans, 1983; 27: 351 [3] Paray F, Gruzleski J E. AFS Trans, 1994; 115: 833 [4] Apelian D, Sigworth G K, Wharler K R. AFS Trans, 1984; 92: 297 [5] Kori S A, Murty B S, Chakraborty M. Mater Sci Eng, 2000; A283: 94 [6] Kurfman V B. AFS Trans, 1961; 69: 234 [7] Charbonnier J. Hommes Foerie, 1975; 59: 29 [8] Ananthanarayanan L, Samuel F H, Gruzleski J E. AFS Trans, 1992; 113: 383 [9] Easton M, Stjohn D. Metall Mater Trans, 1999; 30A: 1613 [10] Charbonnier J. AFS Trans, 1984; 92: 907 [11] Bekaert F, Ghent E W. Aluminum, 1996; 72: 442 [12] Gong L Q. Spec Cast Nonferrous Alloys, 1996; 1: 16 (龚磊清.特种铸造及有色合金,1996;(1):16) [13] Tenekedjiev N and Gruzleski J E. AFS Trans, 1991; 35: 1 [14] Li Y X, Wang Q, Xu X R. Mater Rev, 2002; 16: 1 (李言祥,王强,徐雪蓉.材料导报, 2002;16:1) [15] Li Y X, Hu X, Xu X R. J Mater Sci Technol, 2001; 17: 73 [16] Li Y X, Xu X R, Wang Q, Liu B C. Int J Cast Met Res, 2003; 16: 41 [17] Wang Q, Li Y X, Li X C. Metall Mater Trans, 2003; 34A: 1175 [18] Li Y X, Geng H Y. Spec Cats Nonferrous Alloys, 2004; (6): 4 (李言祥,耿慧远.特种铸造及有色合金, 2004;(6):4) [19] Geng H Y, Li Y X, Chen X, Wang X. Scr Mater, 2005; 53: 69 [20] Chen X, Geng H Y, Li Y X. Acta Metall Sin, 2005; 41: 891 (陈祥,耿慧远,李言祥.金属学报, 2005;41:891) [21] Nogita K, McDonald S D, Dahle A K. Mater Trans, 2003; 44: 692 [22] Sigworth G K, Guzowski M M. AFS Trans, 1985; 93: 907 [23] Geng H Y. PhD Dissertation, Tsinghua University, Beijing, 2005 (耿慧远.清华大学博士学位论文,北京, 2005) [24] Liao H C, Sun G X. Scr Mater, 2003; 48: 1035 [25] Li J G, Zhang B Q, Wang L, Yang W Y, Ma H T. Mater Sci Eng, 2002; A328: 169 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|