|
|
|
| 低周疲劳寿命预测的能量模型探讨 |
| 陈凌;蒋家羚;范志超;陈学东;杨铁成 |
| 浙江大学化工机械研究所 |
|
| Discussion of energy model for low cycle fatigue life prediction |
| Chen Ling |
| 浙江大学化工机械研究所 |
引用本文:
陈凌; 蒋家羚; 范志超; 陈学东; 杨铁成 . 低周疲劳寿命预测的能量模型探讨[J]. 金属学报, 2006, 42(2): 195-200 .
,
,
,
,
.
Discussion of energy model for low cycle fatigue life prediction[J]. Acta Metall Sin, 2006, 42(2): 195-200 .
[1] Kwofie S. Int J Fatigue, 2001; 23: 829 [2] Smith K N, Watson P, Topper T H. J Mater, 1970; 5: 767 [3] Mrozinski S, Topolinski T. J Theor Appl Mech, 1999; 37: 223 [4] Lefebvre D, Neale K W, Ellyin F. J Eng Mater Technol, 1988; 103(1): 1 [5] Tchankov D S, Vesselinov K V. Int J Pressure Vessel Piping, 1998; 75: 955 [6] Feltner C E, Morrow J D. J Basic Eng, 1961; 83(3): 15 [7] Xiao L, Gu H C. J Eng Mater Technol, 1998; 120(2): 114 [8] Park J, Nelson D. Int J Fatigue, 2000; 22: 23 [9] Zhang W X, Chen F, Guo C B, Yu Q. Pressure Vessel Technol, 2002; 19(6): 4(张文孝,陈飞,郭成壁,于强.压力容器,2002;19(6):4) [10] Ellyin F. J Eng Mater Technol, 1985; 107(4): 119 [11] Sander B I. Fundemental of Cyclic Stress and Strain. Wisconsin: The University of Wisconsin Press, 1972: 52 [12] Xiao T, De W, Hao X. Int J Fatigue, 1989; 11: 353 [13] Xia Z, Kujawski D, Ellyin F. Int J Fatigue, 1996; 18: 335 [14] Ellyin F, Golos K, Xia Z. J Eng Mater Technol, 1991; 113(1): 112 [15] Ellyin F, Xia Z. J Eng Mater Technol, 1993; 115(4): 411 [16] Ellyin F. Mech Res Commun, 1974; 1(4): 219 [17] Tong X Y, Wang D J, Xu H. Acta Metall Sin, 1992; 28: A163(童小燕,王德俊,徐灏.金属学报,1992;28:A163) [18] Lemaitre J, Chobche J L. Mechanics of Solids Materials. Cambridge: Cambridge University Press, 1990: 65 [19] Yang G S. Damage Mechanics and Composite Material Damage. Beijing: National Defence Industry Press, 1995: 23(杨光松.损伤力学与复合材料损伤.北京:国防工业出版社,1995:23) [20] Tadeusz L. Int J Fatigue, 2001; 23: 467 [21] Wang R, Huang W B, Huang Z P. Introduction of Plasticity Mechanics. Beijing: Peking University Press, 1992: 1(王仁,黄文彬,黄筑平.塑性力学引论.北京:北京大学出版社,1992:11 [22] Wu D G, Zhang B. Calculus (I). Hangzhou: Zhejiang University Press, 1995: 183(吴迪光,张彬.微积分学(上).杭州:浙江大学出版社,1995:183) [23] Morrow J. ASTM STP 378, 1965: 45 [24] Golos K, Ellyin F. Theor Appl Fract Mech, 1987; 7: 169 [25] Zhao S B. Design for Fatigue Resistance. Beijing: China Machine Press, 1994: 100(赵少汴.抗疲劳设计.北京:机械工业出版社,1994:100) [26] Chen L, Jiang J L. J Mech Strength, 2005; 27(1): 121(陈凌,蒋家羚.机械强度,2005;27(1):121) [27] Chen L, Jiang J L. Pressure Vessel Technol, 2003; 20(10): 11 (陈凌,蒋家羚.压力容器,2003;20(10):11)T |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|