镍基单晶高温合金CMSX-2持久拉伸的显微组织形态及力学行为 |
彭志方 燕平 |
武汉水利电力大学材料工程系; 武汉 430072 |
|
引用本文:
彭志方; 燕平 . 镍基单晶高温合金CMSX-2持久拉伸的显微组织形态及力学行为[J]. 金属学报, 1999, 35(3): 265-270 .
[1] Tien J K, Copley S M. Metall Trans, 1971; 2: 543 [2] Nathal M V, Ebcrt L J. Scr Metall, 1983; 17: 1151 [3] Gayda J, Mackay R A. Scr Metall, 1989; 23: 1835 [4] Socrate S, Parks D M. Acta Metall Mater, 1993; 41: 2185 [5] Caron P, Khan T. Mater Sci Eng, 1983; 61: 173 [6] Nathal R A. Metall Trans, 1987; 18A: 1961 [7] Nathal M V, Ebert J. Metall Tabs, 1985; 16A: 427 [8] Mackay R A, Ebert L J. Metall Trans, 1985; 16A: 1969 [9] Nathal M V, Mackay R A, Miner R V. Metall Trans, 1989;20A: 133 [10] Draper S, Hull D, Dreshfield R. Metall Trans, 1989; 20A: 683 [11] Feller-Kniepmeier M, Link T. Metall Trans, 1989; 20A: 1237 [12] Ai S H, Lupinc V, Maldini M. Acta Metall Sin, 1992; 28:A126(艾素华, Lupine V, Maldini M.金属学报, 1992; 28: A126) [13] Pollock T M, Argon A S. Acta Metall Mated 1994; 42: 1859 [14] Guo X P, Fu H Z, Xun J H. Acta Metall Sin, 1994; 30: A321(郭喜平,傅恒志,孙家华.金属学报,1994;30:A321) [15] Peng Z F, Glatzel U, Feller-Kniepmeier M. Acta Metall Sin,1995; 31: A531(彭志方,Glatzel U Feller-Kniepmeier M. 金属学报,1995; 31:A531) [16] Peng Z F, Glatzel U, Link T, Feller-Kniepmeier M. ScrMater, 1996; 34: 221 [17] Nabarro F R N. Metall Mater Trans, 1996; 27A: 513 [18] Peng Z F, Yan Y H. Acta Metall Sin, 1997, 33: 1147(彭志方,严演辉.金属学报,1997;33:1147) [19] Peng Z F, Ren Y Y, Fan B Z, Yan P, Zhao J C, Sun J H.Acta Metall Sin, 1999; 35: 9(彭志方,任遥遥,樊宝珍,燕平,赵京展,孙家华.金属学报,1999; 35:9) [20] Hendersor P J, Lindblom J. Scr Mater, 1997; 37: 491 [21] Evans H E. Mechanisms of Creep Fracture, England:Elscvicr Applied Science Publishers, 1984: 283 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|