| 快速凝固Al-In偏晶合金的显微结构 |
| 刘源 郭景杰 |
| 哈尔滨工业大学材料科学与工程学院;哈尔滨 150001 |
|
引用本文:
刘源; 郭景杰 . 快速凝固Al-In偏晶合金的显微结构[J]. 金属学报, 2000, 36(12): 1233-1236 .
[1] Liu H L, Xie X N, Cat J L, Jiang L S, Wang G G. PowderMetall Technol, 1990; 8: 39(刘红琳,解晓宁,蔡筠林,江留主,王良国.粉末冶金技术,1990; 8:39) [2] Mohan S, Agarwala V, Ray R. Mater Sci Eng, 1991; 144A:215 [3] Carlberg T, nedriksson H. Metall Trans, 1980; 11A: 1665 [4] Chattopadhyay K, Ramachandrarao P. J Mater Sci, 1980;15: 685 [5] Grugel R N, Lograsso T A, Hellawell A. Metall Trans,1984; 15A: 1003 [6] Xian A P, Zhang X M, Li Z Y, Liu Q Q, Chen J Z, Li YY. Acta Metall Sin, 1996; 32: 113(冼爱平,张修睦,李忠玉,刘清泉,陈继志,李依依.金属学报,1996;32:113 [7] Walter H U. In: Feuerbacher B, Hamacher H, NaumannR J eds., Materials Science in Space. Berlin: Springer-Verlag, 1986: 343 [8] Inoue A, Yano N, Matsuzaki K, Masumoto T. i MaterSci, 1987; 22: 123 [9] Zhang D L, Cantor B. Philos Mag, 1990; 62A: 557 [10] Ratke L. Adv Space Res, 1988; 8: 7 [11] Zhao J Z. Ph D Dissertation, Harbin Institute of Technology, 1994(赵九州.哈尔滨工业大学博士学位论文,1994) [12] Gillen A G, Cantor B. Acta Metall, 1985; 33: 1813 [13] Han Q Y, Hunt J D. Acta Metall Sin, 1996; 32: 363(韩青友,Hunt J D.金属学报,1996;32:363) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|