| 低温变形低碳钢超细铁素体的形成 |
| 杨忠民 陈其安 |
| 钢铁研究总院结构材料研究所; 北京 100081 |
|
引用本文:
杨忠民; 陈其安 . 低温变形低碳钢超细铁素体的形成[J]. 金属学报, 2000, 36(10): 1061-1066 .
[1] Yada H, Matsumura Y. In: Tamura I ed., Proc nit CoofPhysical Metallurgy of Thermomechanical Processing ofSteel and Other Materials, Tokyo: Iron and Steel institute of Japan, 1988: 200 [2] Maki T. Tetsu Hagane, 1995; 81: 547(牧正志铁 钢,1995;81:547) [3] Mintz B, Abu-Shosha R, Shaker M. Mater Sci Technol,1993; 9: 907 [4] Choo Wung Yong, Seo Dong-Han, Lee Sang Woo.CAMP-ISIJ, 1999; 12: 369(Choo Wung Yong, Seo Dong-Hua, Lee Sang Woo. 材料日本铁钢协会讲演论文集,1999; 12:369) [5] Miotz B, Lewis J, Jonas J J. Mater Sci Technol, 1997; 13:379 [6] Yada H, Li C M, Yamagata H. ISIJ Int, 2000; 40: 200^ |
|