| 电磁搅拌对管线钢埋弧焊熔敷金属低温韧性的影响 |
| 国旭明 钱百年 |
| 中国科学院金属研究所; 沈阳 110015 |
|
引用本文:
国旭明; 钱百年 . 电磁搅拌对管线钢埋弧焊熔敷金属低温韧性的影响[J]. 金属学报, 2000, 36(2): 177-180 .
[1] Pear B P, Kerr K W. Metall Trans, 1981; B12: 479 [2] Villafuerte J C, Kerr H W. Weld J, 1990; 69(2): 1s [3] Bhadeshia H K D H. J Mater Sci Lets, 1985; (4): 305 [4] AB M A,AB P Y. C KTpoMa Ar M BM. K:1984: 8 [5] Zhang W Y. Heat Transport in Welding. Beijing: MechnicalIndustry Press, 1989: 64(张文铖.焊接传热学.北京:机械工业出版社,1989:64) [6] Ricks R A, Howed P R, Barritte G S. J Mater Sci, 1982; 17:732 [7] Babu S S, David S A. Mater Sci Technol, 1995; 11: 186 [8] Kluken A O, Grong O. Metall Trans, 1989; A20: 1335h |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|