| Q235碳素钢应变强化相变的基本特点及影响因素 |
| 杨平 傅云义 崔凤娥 孙祖庆 |
| 北京科技大学材料科学与工程学院;北京100083 |
|
引用本文:
杨平; 傅云义; 崔凤娥; 孙祖庆 . Q235碳素钢应变强化相变的基本特点及影响因素[J]. 金属学报, 2001, 37(6): 592-600 .
[1] Yada H, Matsumura Y, Nakajima K. United StatesPatent, No.4466842 1984 [2] Matsumura Y, Yada H. Trans ISIJ, 1987; 27: 492 [3] Yang P, Fu Y Y, Cul F E, Sun Z Q. Acta Metall Sin. 2001;37: 617(杨平,傅云义,崔凤娥,孙祖庆.金属学报,2001;37:617) [4] Hickson M R, Hodgson P D. Mat Sci Tech, 1999; 15: 85 [5] Hodgson P D, Hickson M R, Gibbs R K. Mat Sci Forum,1998; 284-286: 63 [6] Torizuka S, Umezawa O, Tsuzaki K, Nagal K. Mat SciForum, 1998; 284-286: 225 [7] Ishikawa T, Nomiyama Y, Yoshikawa H, Imal S, Inoue T.Nippon Steel Technical Report, 1997, 75: 31 [8] Yang P, Cui F, Ma S, Wang F. The 4th Inter Confer-ence on HSLA Steels, Liu G Q, wing F M, Wang Z B,Zhang H T, Metallurgical Industry Press. Eds, et al., Oct.31-Nov.2, China Xi'an; 2000: 215 [9] Yang P, Fu Y Y, Cul F E, Sun Z Q. Acta Metall Sin, 2001;37: 601(杨平,傅云义,崔凤娥,孙祖庆.金属学报,2001;37:601) [10] Yang W, Hu A, Sun Z. Acta Metall Sin, 2000; 36: 1055(杨王玥,胡安民,孙祖庆,金属学报,2000;36:1055)? |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|