| 过冷DD3单晶高温合金凝固组织细化的再结晶机制 |
| 刘峰 杨根仓 郭学峰 |
| 西北工业大学凝固技术国家重点实验室;西安 710072 |
|
引用本文:
刘峰; 杨根仓; 郭学峰 . 过冷DD3单晶高温合金凝固组织细化的再结晶机制[J]. 金属学报, 2001, 37(1): 13-18 .
[1] Kattamis T Z, Flemings M C. TMS-AIME, 1966; 236:1523 [2] Powell G L F, Hogan L M. TMS-AIME, 1969; 245: 407 [3] Walker J L. In: Pierre G R St ed., The Physical Chemistryof Process Metallurgy, Part 2, New York: Interscience,1959: 845 [4] Herlach D M. Mater Sci Eng, 1994; 12R: 177 [5] Schwarz M, Karma A, Eckler K, Herlach D M. Phys RevLett, 1994; 73: 380 [6] Horvay G. J Heat Mass Transfer, 1965; 8: 195 [7] Glicksman M E. Acta Metall, 1965; 13: 1231 [8] Jackson K A, Hunt J D, Uhlmann D R, Seward T P III.TMS-AIDE, 1966; 236: 149 [9] Gartner R F, Norman A F, Greer A L, Zambon A, Ramous E. Acta Mater 1997; 45: 51 [10] Cochrane R F, Herlach D M, Feuerbacher B. Mater SciEng, 1991; 133A: 706 [11] Du W. Ph.D Thesis, Northwestern Polytechnical Universityl Xi'an, 1998(杜 伟。西北工业大学博士学位论文,西安,1998) [12] Liu F, Cai Y, Guo X F, Yang G C. Casting, 2000; 6: 344 [13] Chakravorty S, West D R F. J Mater Sci, 1984; 19: 3574 [14] Machlin E S, Shao J. Metall Trans, 1978; 9A: 561 [15] Liu F, Guo X F, Cai Y, Yang G C. Acta Metall Sin, 2000;36:567(刘峰,郭学峰,蔡瑜,杨根仓.金属学报,2000;36:567) [16] Li J F, Yang G C, Zhou Y H. J Cryst Growth,1998; 192:462 [17] Piccone T J, Wu Y, Shiohara Y, Flemings M C. MetallTrans, 1987; 18A: 915 [18] Boettinger W J, Coriell S R, Trivedi R. In: Mehrabian R,Parrish P A eds., Rapid Solidification Processing: Principles and Technologies IV, Baton Rouge, LA, Claitor's,1988: 13 [19] Guo X F. Ph D Thesis, Northwestern Polytechnical Universityl Xi'an, 1999(郭学峰.西北工业大学博士学位论文,西安,1999) [20] Dahle A K, Thevik H J, Arnberg L, John D H St. MetallMater Trans, 1999; 30B: 287 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|