| Al-Zn-Li-Mg-Cu合金在433 K的时效行为 |
| 谷亦杰 魏炳忱 张永刚 陈昌麒 |
| 北京航空航天大学材料科学与工程系;北京 100083 |
|
引用本文:
谷亦杰; 魏炳忱; 张永刚; 陈昌麒 . Al-Zn-Li-Mg-Cu合金在433 K的时效行为[J]. 金属学报, 2001, 37(1): 19-22 .
[1] Huang Z W, Loretto M H, White J. Mater Sci Technol,1993; 9: 967 [2] Sodergren A, Lioyd D J. Acta Metall, 1988; 36: 2107 [3] Dinsdale K, Noble B, Harris S J. Mater Sci Eng, 1988;104A: 75 [4] Singh V, Mukhopadhyay A K, Prasad K S. Scr Mater,1997; 37: 1519 [5] Williams D B, Edington J W. Met Sci, 1975; 9: 529 [6] Baumann S F, Williams D D. Scr Metall, 1984; 18: 611 [7] Raman K S. Scr Metall, 1971; 5: 79 [8] Kar R J, Bohlen J W, Chanani G R. In: Sander T H Jr,Starker E A Jr eds., Aluminum -Lithium Alloy II,Pennesylvania, USA, TMS-AIME, 1984:255 [9] Gregson P J, Flower H M, Tite C N J, Mukhopadhyay AK. Mater Sci Technol, 1986; 2: 349 [10] Baumann S P, Williams D B. Metall Trans,1985; 16A:1203 [11] Kumar K S, Brown S A, Pickens J R. Acta Mater 1996;44: 1899 [12] Sekhar J A. Curr Sci, 1985; 54: 904 [13] Follstaedt D M, Knapp A. Mater Sci Eng, 1987; 90: 1v |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|