| 微量元素磷、硼对直接时效IN718合金持久蠕变性能的影响 |
| 李娜; 郭守仁; 卢德忠; 孙文儒; 孟晓娜; 胡壮麒 |
| 中国科学院金属研究所; 沈阳 110016 |
|
引用本文:
李娜; 郭守仁; 卢德忠; 孙文儒; 孟晓娜; 胡壮麒 . 微量元素磷、硼对直接时效IN718合金持久蠕变性能的影响[J]. 金属学报, 2003, 39(12): 1255-1258 .
[1] Cao W D, Kennedy R L. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, TMS, 1994:463 [2] Kennedy R L, Cao W D, Thomas W M. Adv Mater Process, 1996; 150(3) : 33 [3] Xie X S, Liu X B, Hu Y H, Tang B, Xu Z C, Dong J X, Ni K Q, Zhu Y X, Tien S S, Zhang L P, Xie W. In: Kissinger R D, Deye D 3, Anton D L, Cetel A D, Nathal M V, Pollock T M, Woodford D A eds, Superalloys 1996, TMS, 1996:599 [4] Guo S R, Sun W R, Lu D Z, Hu Z Q. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, TMS,1997:521 [5] Sun W R, Guo S R, Lu D Z, Hu Z Q. Metall Mater Trans,1997; 28A: 649 [6] Liu X, Dong J X, Tang B, Hu Y, Xie X S. Mater Sci Eng A, 1999; 270:190 [7] Horton J A, McKamey C G, Miller M K, Cao W D, Kennedy R L. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, TMS, 1997:401 [8] McKamey C G, Carmichael C A, Cao W D, Kennedy R L. Scr Mater, 1998; 38:485 [9] Cao W D, Kennedy R L. In: Loria E A ed, Superalloys 718, 625, 706 and Various Derivatives, TMS, 2001:45510 [10] Funkenbusch A W, Heldt L A, Stein D F. Metall Trans,1982; 13A: 611 [11] Yonezawa T, Onimura K, Sakamoto O, Sasaguri N,Nakata H, Susukida H. Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors,NACE, Houston, TX, 1984:345 [12] Was G S, Martin G R. Metall Trans, 1985; 16A: 349 [13] Hall E L, Briant C L. Metall Trans A, 1985; 16A: 1225 [14] Braint C L. Metall Trans, 1988; 19A: 137 [15] Miller M K, Horton J A, Cao W D, Kennedy R L. J Phys(France), 1996; 6(5) : 241 [16] Song H W. PhD Thesis, Institute of Metal Research, The Chinese Academy of Science, Shenyang, 1999(宋洪伟,博士学位论文,中国科学院金属研究所.1999) [17] Sherby O D. Acta Met, 1962; 10:135 [18] Dorn J E, Mech J. Phys Solids, 1964; 2:85 [19] Weertman J. J Appl Phys, 1957; 28:362 [20] Barrett C R, Nix W D. Acta Met, 1965; 13:1247 [21] Nabarro F R N. Report of Conference on Strength of Solids, The Physical Society, Bristol, England, 1948:75 [22] Song H W, Guo S R, Lu D Z, Xu Y, Wang Y L, Hu Z Q.Chin J Nonferrous Met, 2000; 10(3) : 301(宋洪伟,郭守仁,卢德忠,徐岩,王玉兰,胡壮麒.中国有色金属学报,2000;10(3) :301) [23] Stroup J P, Heacox R A. JOM, 1969:46 [24] Carreno F, Ruano O A. Acta Mater, 1998; 46(1) : 159 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|