| Sm0.99Gd0.01Al2金属间化合物的声学和比热容性质研究 |
| 苏金瑞 王克勤 屈继锋 朱长飞 |
| 中国科学技术大学材料科学与工程系内耗与固体缺陷实验室;合肥230026 |
|
引用本文:
苏金瑞; 王克勤; 屈继锋; 朱长飞 . Sm0.99Gd0.01Al2金属间化合物的声学和比热容性质研究[J]. 金属学报, 2003, 39(11): 1186-1188 .
[1] Adachi H, Ino H. Nature, 1999; 401: 148 [2] Adachi H, Kawata H, Hashimoto H, Sato Y, Matsumoto I, Tanaka Y. Phys Rev Lett, 2001; 87: 127202-1 [3] Wang K Q, Zhuang Z Z. Chin J Low Temp Phys, 1996;18: 339(王克勤,庄志忠.低温物理学报, 1996;18:339) [4] Wang H F, Wu Z Q. Experimental Methods for Solid State Physics. Beijing: Higher Education Press, 1990: 161(王华馥,吴自勤.固体物理实验方法.北京:高等教育出版社,1990:161) [5] Nowick A S, Berry B S. Anelastic Relaxation in Crystalline Solids. London: Academic Press, 1972: 588 [6] Qu J F. Thesis for Bachelor's Degree, University of Science and Technology of China, Hefei, 2001(屈继锋.中国科学技术大学学士学位论文,合肥, 2001) [7] Landau L D, Lifshitz E M. Statistical Physics. New York:Pergamon Press, 1958: 430 [8] Landau L D, Khalatnikov S M. Doklady Akad Nauk SSSR,1954; 96: 469 [9] Rosen M. Phys Rev, 1968; 174: 504 [10] Rosen M. Phys Rev, 1969; 180: 540 [11] Bennett H S, Pytte E. Phys Rev, 1967; 155: 553 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|