| 连铸结晶器内钢液涡流现象的水模型观察和数值模拟 |
| 李宝宽 李东辉 |
| 东北大学材料冶金学院热能工程系;沈阳 110004 |
|
引用本文:
李宝宽; 李东辉 . 连铸结晶器内钢液涡流现象的水模型观察和数值模拟[J]. 金属学报, 2002, 38(3): 315-320 .
[1]Wang Y H. In: Schneider G P ed. 73rd Steelmaking Con-ference Proceedings, Warrendale: Iron and Steel Society, 1990: 473 [2]HE Q L. ISIJ Inter, 1993; 33: 343 [3]Gebhard M, He Q L, Herbertson J. In: Rote F E ed. 76th Steelmaking Conference Proceedings, Warrendale: Iron and Steel Society, 1993: 441 [4]Honeyands T, Herbertson J. Steel Res, 1995; 66: 287 [5]Gupta E, Lahri A K. Metall Mater Trans, 1996; 27B: 757 [6]Huang X, Thomas B G. Canadian Metall Quarterly, 1998;37:197 [7]Lam C K G, Bremhorst K. J Fluid Eng, 1981; 103: 456 [8]Li B K, Okane T, Umeda T. Metall Mater Trans, 2000; 31B: 1491j |
|