| 高温合金氧化膜破坏的界面断裂力学分析 |
| 雷明凯 徐忠成 杨辅军 高 峰 |
| 大连理工大学材料工程系; 大连 116024 |
|
| Interface Fracture Mechanics of Failure For Oxide Scale on Superalloy |
| LEI Mingkai; XU Zhongcheng; YANG Fujun; GAO Feng |
| Department of Materials Engineering; Dalian University of Technology; Dalian 116024 |
引用本文:
雷明凯; 徐忠成; 杨辅军; 高峰 . 高温合金氧化膜破坏的界面断裂力学分析[J]. 金属学报, 2004, 40(10): 1104-1108 .
,
,
,
.
Interface Fracture Mechanics of Failure For Oxide Scale on Superalloy[J]. Acta Metall Sin, 2004, 40(10): 1104-1108 .
[1] Lowell C E, Barrett C A, Palmer R W, Auping J V, PobstH B. Oxid Met, 1991; 36: 81 [2] Smialek J L. JOM, 2000; 1: 22 [3] Chan K S. Metall Mater Trans, 1997; A28: 411 [4] Chan K S, Cheruvu N S, Leverant G R. J Eng Gas TurbPower, 1998; 120: 609 [5] Chan K S, Cheruvu N S, Leverant G R. J Eng Gas TurbPower, 1999; 121: 484 [6] Lei M K, Yang F J, Luo P, Zhu X P. J Chin Soc CorrosProt. 2002; 22: 65(雷明凯,杨辅军,罗鹏,朱小鹏.中国腐蚀与防护学报,2002;22:65) [7] Evans H E, Lobb R C. Corros Sci, 1984; 24: 209 [8] Hutchinson J W, Thouless M D, Liniger E G. Acta MetallMater, 1992; 40: 295 [9] Wang J S, Evans A G. Acta Mater, 1998; 46: 4993 [10] Evans A G, Hutchinson J W. Int J Solids Struct, 1984;20: 455 [11] Suo Z, Hutchinson J W. Int J Fract, 1990; 43: 1 [12] Hutchinson J W, Suo Z. Adv Appl Mech, 1992; 29: 63 [13] Evans A G, Hutchinson J W. Acta Metall Mater, 1995;43: 2507 [14] Qian Y H, Li M S, Zhang Y M. Corros Sci Prot Technol,2003; 15: 90(钱余海,李美栓,张亚明.腐蚀科学与防护技术,2003;15:90) [15] Hutchinson J W, Mear M E, Rice J R. J Appl Mech, 1987;54: 828 [16] Christensen J R, Lipkin D M, Clarke D R. Acta Mater,1996; 44: 3813 [17] Wang J S, Evans A G. Acta Mater, 1999; 47: 699 [18] Tolpygo V K, Clarke D R. Mater Sci Eng, 2000; A278:151& |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|