| 镍基单晶合金枝晶典型区域相成分最优化测算法 |
| 骆宇时 刘攀 彭志方 |
| 武汉大学动力与机械学院;武汉430072 |
|
引用本文:
骆宇时; 刘攀; 彭志方 . 镍基单晶合金枝晶典型区域相成分最优化测算法[J]. 金属学报, 2002, 38(8): 804-808 .
[1] Schulze C, Feller-Kniepmeier M. Mater Sci Eng, 2000;281A: 204 [2] Peng Z F, Ren Y Y, Zhang W, Yan P, Zhao J C, Wang YQ. Acta Metall Sin, 2001; 37: 345(彭志方,任遥遥,张伟,燕平,赵京晨,王延庆.金属学报,2001;37:345) [3] Link T, Epishin A, Br(?)ckner U. Scr Mater, 1998; 39: 1463 [4] Link T, Epishin A, Br(?)ckner U, Portella P. Acta Mater,2000; 48: 1981 [5] V(?)lkl R, Glatzel U, Feller-Kniepmeier M. Scr Mater,1998; 38: 894 [6] Chen B L. Theories and Algorithms of System Optimiza-tion. Beijing: Tsinghua University Press, 1989: 8(陈宝林.系统最优化理论与算法.北京:清华大学出版社,1989:8) [7] Hu S G, Shi B C. Principles of Optimization Algorithms. Wuhan: Huazhong University of Science and Technology, 2000: 5 [8] Du Z, Luo Y. A Scientific Algorithm Program-MATLAB. Tianjin: Nankai University Press, 1998: 12(杜藏,骆源.科学计算语言MATLAB.天津:南开大学出版社,1998:12) [9] Zheng Y R, Zhang D T. Color Metallographic Investigation of Superalloys and Steels. Beijing: National Defense Industry Press, 1997: 10(郑运荣,张德堂.高温合金与钢的彩色金相研究.北京:国防工业出版社,1997:10) [10] Caron P, Khan T. Mater Sci Eng, 1983; 61: 173 [11] Pollock T M, Argon A S. Ada Metall Mater, 1994; 42:1859 [12] Glatzel U. Microstructure and Internal Strains of Unde-formed and Creep Deformed Samples of a Nickel-BaseSuperalloy. Berlin: Verlag Dr. K(?)ster, 1994: 14 [13] Bruckner U, Epishin A, Link T. Acta. Mater, 1997; 45:5228 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|