| 相场仿真二维晶粒长大过程中的尺寸分布和拓扑演变 |
| 孙 亚 刘国权 王 超 |
| 北京科技大学材料科学与工程学院; 北京 100083 |
|
| Grain Size Distribution And Topological Evolution in 2D Grain Growth Process Based on Phase Field Simulation |
| SUN Ya; LIU Guoquan; WANG Chao |
| School of Materials Science and Enginering; University of Science and Technology Beijing; Beijing 100083 |
引用本文:
孙亚; 刘国权; 王超 . 相场仿真二维晶粒长大过程中的尺寸分布和拓扑演变[J]. 金属学报, 2004, 40(6): 609-.
,
,
.
Grain Size Distribution And Topological Evolution in 2D Grain Growth Process Based on Phase Field Simulation[J]. Acta Metall Sin, 2004, 40(6): 609-.
[1] Fayad W, Thompson C V, Frost H J. Scr Mater, 1999;40(10) : 1199 [2] Wang C, Liu G Q, Qin X G. Acta Metall Sin, 2003; 39:635(王超, 刘国权, 秦湘阁. 金属学报, 2003; 39: 635) [3] Wang C, Liu G Q, Qin X G. ISIJ Int, 2003; 43(5) : 774 [4] Fan D N, Chen L Q. Acta Mater, 1997; 45: 611 [5] Fan D N, G Chengwei, Chen L Q. Acta Mater, 1997; 45:1115 [6] Anderson M P, Fortes M A. Philos Mag, 1989; B59: 293 [7] Wang C. PhD Dissertation, University of Science and Technology Beijing. 2003. 5(王超.北京科技大学博士学位论文, 2003) [8] Nordbakke M W, Ryum N, Hunderi O. Acta Mater, 2002;50: 3661 [9] Beck P A. Philos Mag Suppl, 1954; 3: 245 [10] Tikare V, Holm E A, Fan D, Chen L Q. Acta Mater, 1999;47: 363 [11] Mullins W W. Acta Mater, 1998; 46: 6219 [12] Fradkov V E, Frachenko A S, Shvindlerman L S. Scr Met,1985; 19: 1291 |
|