| 低温熔盐电沉积Al-Ti合金粉 |
| 过家驹 郭乃名 周虹辉 |
| 北京科技大学表面科学与腐蚀工程系;北京 100083 |
|
引用本文:
过家驹; 郭乃名; 周虹辉 . 低温熔盐电沉积Al-Ti合金粉[J]. 金属学报, 1999, 35(11): 1175-1177 .
[1] Guo N M, Guo J J. Nonferrous Met, 1997; 49(2): 64(郭乃名,过家驹.有色金属, 1997; 49(2): 64) [2] Guo N M, Wei Z Q, Guo J J. In: Electrodremistry Committee of Chinese Chemical Society ed, Digests of 9th NationalConference on Electrochemistry, Tai'an: Shandong miningIndestry Colloge Press, 1997; 3: 354(郭乃名,魏振强,过家驹.见:中国化学会电化学委员会编,第九届全国电化学会议论文摘要集,泰安:山东矿业学院出版社,1997;3:354) [3] Guo N M, Xiong S H, Guo J J Eng Chem Metall, 1997;18(4): 38(郭乃名,熊申海,过家驹.化工冶金, 1997; 18(4): 318) [4] Guo N M, Guo J J. Acta Metall Sin, 1996; 32(3): 274(郭乃名,过家驹.金属学报, 1996; 32(3): 274) [5] Uchida J I, Tsuda Y, Yamamoto Y, Seto H, Abe M, ShibuyaA. Iron Steel, 1991; (7): 931 [6] Guo N M, Gao Y P, Wang C F. Rare Met, 1983; (2): 147 [7] Duan S Z, Qiao Z Y. Molten Salt Electrochemistrlly. Beijing:Metallurgical industry Press, 1990: 202(段淑贞,乔芝郁主编.熔盐电化学.北京:冶金工业出版社,1990:202) |
|