| Fe--Mn--Si--Cr--Ni形状记忆合金约束下相变的电阻原位分析 |
| 文玉华;严密;李宁 |
| 浙江大学硅材料国家重点实验室 |
|
| In Situ Resistance Analysis On Transformation Of Constrained Fe--Mn--Si--Cr--Ni Shape Memory Alloy |
| WEN Yuhua; YAN Mi; LI Ning\ |
| State Key Laboratory of Silicon Materials; Zhejiang University |
引用本文:
文玉华; 严密; 李宁 . Fe--Mn--Si--Cr--Ni形状记忆合金约束下相变的电阻原位分析[J]. 金属学报, 2004, 40(1): 72-76 .
,
,
.
In Situ Resistance Analysis On Transformation Of Constrained Fe--Mn--Si--Cr--Ni Shape Memory Alloy[J]. Acta Metall Sin, 2004, 40(1): 72-76 .
[1] Yang J H, Chen H, Wayman C M. Metall Trans, 1992; 23A: 1431 [2] Hsu T Y. J Mater Sci Technol, 1994; 40:112 [3] Bergeon N, Guenin G, Esnouf C. Mater Sci Eng, 1997; A238:309 [4] Wu X, Hsu T Y. Mater Charact, 2000; 45:137 [5] Kajiwara S, Liu D, Kikuchi T, Shinya N. Scr Mater, 2001; 44:2809 [6] Wen Y H, Li N, Tu M J. Scr Mater, 2001; 44:1113 [7] Tian S. Materials Physical Properties. Beijing: Aeronautics and Astronautics University Press, 2001:79(田莳.材料物理性能.北京:北京航空航天大学出版社,2001:33) [8] Wen Y H, Li N, Tu M J. J Mater Sci Technol, 2000; 16: 537 [9] Sun B N, Hong T, Yang L X. Engineerig Plastoelasticity. Hangzhou: Zhejiang University Press, 1998:20(孙炳南,洪滔,杨骊先.工程弹塑性力学.杭州:浙江大学出版社,1998:20) [10] Li N. PhD Dissertation, Sichuan University, Chengdu, 2000(李宁.四川大学博士学位论文,成都,2000) [11] Miyazaki S, Matsuda S. Trans ISIJ, 1989; 29:353 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|