| TA18合金铸锭-管坯组织遗传行为及力学性能调控 |
李帅雨1, 刘泽栋1, 杨劼人1( ), 金伟2, 彭博1, 杜新1, 周斯曼1 |
1 四川大学 材料科学与工程学院 成都 610065 2 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016 |
|
| Microstructural Inheritance Behavior and Mechanical Property Control of TA18 Alloy From Ingot to Tube Blank |
LI Shuaiyu1, LIU Zedong1, YANG Jieren1( ), JIN Wei2, PENG Bo1, DU Xin1, ZHOU Siman1 |
1 College of Materials Science and Engineering, Sichuan University, Chengdu 610065, China 2 Shi -changxu Innovation Center for Advanced Materials, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China |
引用本文:
李帅雨, 刘泽栋, 杨劼人, 金伟, 彭博, 杜新, 周斯曼. TA18合金铸锭-管坯组织遗传行为及力学性能调控[J]. 金属学报, 2026, 62(9): 1487-1502.
Shuaiyu LI,
Zedong LIU,
Jieren YANG,
Wei JIN,
Bo PENG,
Xin DU,
Siman ZHOU.
Microstructural Inheritance Behavior and Mechanical Property Control of TA18 Alloy From Ingot to Tube Blank[J]. Acta Metall Sin, 2026, 62(9): 1487-1502.
| [1] |
Najafizadeh M, Yazdi S, Bozorg M, et al. Classification and applications of titanium and its alloys: A review [J]. J. Alloys Compd. Commun., 2024, 3: 100019
|
| [2] |
Alabort E, Tang Y T, Barba D, et al. Alloys-by-design: A low-modulus titanium alloy for additively manufactured biomedical implants [J]. Acta Mater., 2022, 229: 117749
doi: 10.1016/j.actamat.2022.117749
|
| [3] |
Xu W C, Tong X Y, Wang Y Q, et al. Research progress on the influence of the deep-sea environment on the stress corrosion of titanium alloys [J]. Acta Metall. Sin., 2025, 61: 1469
doi: 10.11900/0412.1961.2024.00221
|
| [3] |
徐玮辰, 佟向瑜, 王优强 等. 深海环境对钛合金应力腐蚀影响的研究进展 [J]. 金属学报, 2025, 61: 1469
doi: 10.11900/0412.1961.2024.00221
|
| [4] |
Yang Z K, Wu J J, Wang M Y, et al. Tensile deformation behavior of high-strength TA18 titanium alloy tube under warm forming conditions and constitutive model based on dislocation density [J]. Mater. Today Commun., 2023, 37: 107336
|
| [5] |
Cheng Z H, Abd El-Aty A, Zhang R S X, et al. Finite element modeling and experimental investigation on manufacturing TA18 alloy pipes via hot free bending forming technology: Forming characteristics and process optimization [J]. J. Mater. Res. Technol., 2024, 29: 5225
doi: 10.1016/j.jmrt.2024.02.187
|
| [6] |
He S T, Zeng W D, Xu J W, et al. The texture evolution related to the interactions between α and β phases in dual-phase region annealing of a near α titanium alloy pipe after Pilger cold rolling [J]. J. Alloys Compd., 2022, 890: 161807
doi: 10.1016/j.jallcom.2021.161807
|
| [7] |
Lu S L, Zhang Z J, Liu R, et al. Optimal tensile properties of laser powder bed fusion hereditary basket-weave microstructure in additive manufactured Ti6Al4V [J]. Addit. Manuf., 2022, 59: 103092
|
| [8] |
Sun Z Y, Mo X F, Li Y F, et al. Effects of hot isostatic pressing parameters on microstructure and properties of TA15 titanium alloy [J]. Spec. Cast. Nonferrous Alloys, 2023, 43: 804
|
| [8] |
孙志雨, 莫晓飞, 李亚峰 等. 热等静压工艺参数对TA15钛合金组织及性能的影响 [J]. 特种铸造及有色合金, 2023, 43: 804
|
| [9] |
Wang C Y, Wang Y H, Li Y, et al. Effect of texture inheritance on microstructure of beta C titanium alloy [J]. Rare Met. Mater. Eng., 2023, 52: 3382
|
| [9] |
王春阳, 王玉会, 李 野 等. TB9钛合金棒材组织遗传效应与性能(英文) [J]. 稀有金属材料与工程, 2023, 52: 3382
|
| [10] |
Qin X Y, Liu H, Chen Y Y, et al. Optimization in strength-ductility of Mg-Gd-Y-Zn-Al alloy through microstructural heredity process regulation [J]. Mater. Sci. Eng., 2025, A944: 148930
|
| [11] |
Chen Q Y, Zhang W N, Tang S, et al. Microstructural heredity of Ni-containing cryogenic steel and its effect on the toughness at 77 K [J]. Mater. Sci. Eng., 2022, A832: 142441
|
| [12] |
Cheng X, Gao G H, Fu C, et al. Mechanistic understanding of banded microstructure and its effect on anisotropy of toughness in low carbon-low alloy steel [J]. Mater. Sci. Eng., 2025, A919: 147507
|
| [13] |
Azizi N, Mahmudi R. Microstructure, texture, and mechanical properties of the extruded and multi-directionally forged Mg-xGd alloys [J]. Mater. Sci. Eng., 2021, A817: 141385
|
| [14] |
Semiatin S L. An overview of the thermomechanical processing of α/β titanium alloys: Current status and future research opportunities [J]. Metall. Mater. Trans., 2020, 51A: 2593
|
| [15] |
Chen P, Li J S, Li C C, et al. Research on the hot-temperature rheological behavior and microstructural evolution of TA18 titanium alloy [J]. Mater. Today Commun., 2025, 43: 111810
|
| [16] |
Wang Z L, Wang L, Zhang S Y, et al. Analytical springback modelling for thermal-mechanical bending of TA18 tube under non-isothermal loading [J]. Appl. Math. Model., 2025, 143: 115964
doi: 10.1016/j.apm.2025.115964
|
| [17] |
Zhao Z B, Tan H B, Zhang B H, et al. Review: Microtextures in near α and α + β dual-phase titanium alloys [J]. Acta Metall. Sin., 2026, 62: 275
|
| [17] |
赵子博, 谭海兵, 张博华 等. 综述: 近α型和α + β两相钛合金的微织构 [J]. 金属学报, 2026, 62: 275
doi: 10.11900/0412.1961.2024.00449
|
| [18] |
Liang C Z, Wang J, Xu J F, et al. High-temperature tensile deformation behavior and damage model of TB6 alloy [J]. J. Inn. Mong. Univ. Technol. Nat. Sci. Ed., 2024, 43: 434
|
| [18] |
梁春祖, 王 静, 许江帆 等. TB6钛合金高温拉伸变形过程临界损伤模型 [J]. 内蒙古工业大学学报(自然科学版), 2024, 43: 434
|
| [19] |
Wang B, Li R, Liu J L. Grain refinement of ZALSi7Mg1 alloy by structure heredity [J]. Found. Technol., 2009, 30: 779
|
| [19] |
王 斌, 李 日, 刘军利. 利用组织遗传性细化ZAlSi7Mg1合金晶粒的研究 [J]. 铸造技术, 2009, 30: 779
|
| [20] |
Jing Z Q, Sun Y H, Song S C. Numerical simulation of macrosegregation heredity on TC4 titanium alloy ingot by vacuum arc remelting [J]. Metall. Res. Technol., 2023, 120: 116
doi: 10.1051/metal/2023012
|
| [21] |
Li D, Huang H L, Chen C, et al. Additive manufacturing of high strength near β titanium alloy Ti-55511 by engineering nanoscale secondary α laths via in-situ heat treatment [J]. Mater. Sci. Eng., 2021, A814: 141245
|
| [22] |
He S H, He B B, Zhu K Y, et al. On the correlation among dislocation density, lath thickness and yield stress of bainite [J]. Acta Mater., 2017, 135: 382
doi: 10.1016/j.actamat.2017.06.050
|
| [23] |
Zhang Y, Li D S, Li X Q, et al. Creep deformation and strength evolution mechanisms of a Ti-6Al-4V alloy during stress relaxation at elevated temperatures from elastic to plastic loading [J]. J. Mater. Sci. Technol., 2022, 126: 93
doi: 10.1016/j.jmst.2022.02.042
|
| [24] |
Sun Y G, Zhang C J, Feng H, et al. Dynamic recrystallization mechanism and improved mechanical properties of a near α high temperature titanium alloy processed by severe plastic deformation [J]. Mater. Charact., 2020, 163: 110281
doi: 10.1016/j.matchar.2020.110281
|
| [25] |
Fan X G, Yang H, Gao P F. Prediction of constitutive behavior and microstructure evolution in hot deformation of TA15 titanium alloy [J]. Mater. Des., 2013, 51: 34
doi: 10.1016/j.matdes.2013.03.103
|
| [26] |
Matsumoto H, Velay V. Mesoscale modeling of dynamic recrystallization behavior, grain size evolution, dislocation density, processing map characteristic, and room temperature strength of Ti-6Al-4V alloy forged in the (α + β) region [J]. J. Alloys Compd., 2017, 708: 404
doi: 10.1016/j.jallcom.2017.02.285
|
| [27] |
Yang G J, Park S J. Deformation of single crystals, polycrystalline materials, and thin films: A review [J]. Materials, 2019, 12: 2003
doi: 10.3390/ma12122003
|
| [28] |
Zhou Z C, Jiang B B, Qiu J K, et al. Phase interface-induced dwell fatigue cracks in titanium alloy with lamellar microstructure [J]. Sci. China Mater., 2023, 66: 4267
doi: 10.1007/s40843-023-2641-7
|
| [28] |
周志春, 江彬彬, 邱建科 等. 片层组织钛合金中相界面诱导保载疲劳裂纹形成(英文) [J]. 中国科学: 材料科学(英文版), 2023, 66: 4267
|
| [29] |
Burtscher M, Alfreider M, Schmuck K, et al. In situ fracture observations of distinct interface types within a fully lamellar intermetallic TiAl alloy [J]. J. Mater. Res., 2021, 36: 2465
doi: 10.1557/s43578-020-00088-z
|
| [30] |
Duan C Z, Zhang L C, Li H H, et al. Ductile fracture due to adiabatic shear during the serrated chip formation in high speed cutting: A microscopic investigation [J]. Key Eng. Mater., 2011, 467-469: 181
doi: 10.4028/www.scientific.net/KEM.467-469
|
| [31] |
Zhang M C, Xu Q S, Liu Y, et al. Effect of hot-pressing temperature on the microstructure and properties of the diffusion-bonded region of TC4 alloy [J]. Acta Metall. Sin., 2025, 61: 1183
doi: 10.11900/0412.1961.2023.00414
|
| [31] |
张洺川, 徐勤思, 刘 意 等. 热压温度对TC4合金扩散连接区组织与性能的影响 [J]. 金属学报, 2025, 61: 1183
doi: 10.11900/0412.1961.2023.00414
|
| [32] |
Wang K, Li H H, Zhou Y, et al. Dislocation slip and crack nucleation mechanism in dual-phase microstructure of titanium alloys: A review [J]. Acta Metall. Sin. (Engl. Lett.), 2023, 36: 353
doi: 10.1007/s40195-022-01505-4
|
| [33] |
Fan X G, Zeng X, Yang H, et al. Deformation banding in β working of two-phase TA15 titanium alloy [J]. Trans. Nonferrous Met. Soc. China, 2017, 27: 2390
doi: 10.1016/S1003-6326(17)60265-6
|
| [34] |
Chen G X. Microscopic deformation behavior of Ti-6Ai-4V titanium alloy based on the characteristic of two phase [D]. Qinhuangdao: Yanshan University, 2018
|
| [34] |
陈国兴. 基于双相特征的Ti-6Al-4V钛合金微观变形行为研究 [D]. 秦皇岛: 燕山大学, 2018
|
| [35] |
Chen Y T, Wang K, Ren Z. Interaction between phase transformation and static recrystallization during annealing of rolled TC18 titanium alloy [J]. J. Mater. Sci. Technol., 2024, 202: 1
doi: 10.1016/j.jmst.2024.03.011
|
| [36] |
Li Y L, Fang H Z, Chen R R, et al. A comparative analysis of a unique DRX process in achieving a homogeneous distribution of β grains in the single phase region of as-cast Ti644321 alloy [J]. Mater. Charact., 2024, 207: 113505
doi: 10.1016/j.matchar.2023.113505
|
| [37] |
Li H Z, Wu D P, Jiang H J, et al. Dynamic recrystallization mechanism and model of TC31 titanium alloy sheet during hot deformation [J]. J. Mater. Res., 2025, 40: 1877
doi: 10.1557/s43578-025-01620-9
|
| [38] |
Yang Q Y, Ma M, Tan Y B, et al. Microstructure and texture evolution of TB8 titanium alloys during hot compression [J]. Rare Met., 2021, 40: 2917
doi: 10.1007/s12598-020-01643-7
|
| [39] |
Rios P R, Siciliano Jr F, Sandim H R Z, et al. Nucleation and growth during recrystallization [J]. Mater. Res., 2005, 8: 225
doi: 10.1590/S1516-14392005000300002
|
| [40] |
Hadadzadeh A, Mokdad F, Wells M A, et al. A new grain orientation spread approach to analyze the dynamic recrystallization behavior of a cast-homogenized Mg-Zn-Zr alloy using electron backscattered diffraction [J]. Mater. Sci. Eng., 2018, A709: 285
|
| [41] |
Chen Y L, Jin L, Dong J, et al. Twinning effects on the hot deformation behavior of AZ31 Mg alloy [J]. Mater. Charact., 2016, 118: 363
doi: 10.1016/j.matchar.2016.06.014
|
| [42] |
Huang K, Logé R E. A review of dynamic recrystallization phenomena in metallic materials [J]. Mater. Des., 2016, 111: 548
doi: 10.1016/j.matdes.2016.09.012
|
| [43] |
Wang Y S, Li Z D, Wang H Y, et al. Flow behavior and dynamic recrystallization mechanism of a new near-alpha titanium alloy Ti-0.3Mo-0.8Ni-2Al-1.5Zr [J]. J. Mater. Res. Technol., 2024, 30: 3863
doi: 10.1016/j.jmrt.2024.04.076
|
| [44] |
Xie B C, Zhang B Y, Yu H, et al. Nucleation mechanism of discontinuous dynamic recrystallization with restrained grain boundary sliding [J]. Met. Mater. Int., 2021, 27: 5476
doi: 10.1007/s12540-020-00847-x
|
| [45] |
Qiang F M, Kou H C, Zhang Y D, et al. Crystallographic orientation related dynamic recrystallization behavior and its impact on texture development of high-temperature α phase in TiAl alloy [J]. J. Alloys Compd., 2025, 1010: 178066
doi: 10.1016/j.jallcom.2024.178066
|
| [46] |
Burgers W G. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium [J]. Physica, 1934, 1: 561
doi: 10.1016/S0031-8914(34)80244-3
|
| [47] |
Li J S, Tang B, Fan J K, et al. Deformation mechanism and microstructure control of high strength metastable β titanium alloy [J]. Acta Metall. Sin., 2021, 57: 1438
|
| [47] |
李金山, 唐 斌, 樊江昆 等. 高强亚稳β钛合金变形机制及其组织调控方法 [J]. 金属学报, 2021, 57: 1438
doi: 10.11900/0412.1961.2021.00352
|
| [48] |
Guo B Q, Jonas J J. Dynamic transformation during the high temperature deformation of titanium alloys [J]. J. Alloys Compd., 2021, 884: 161179
doi: 10.1016/j.jallcom.2021.161179
|
| [49] |
Shi R, Dixit V, Viswanathan G B, et al. Experimental assessment of variant selection rules for grain boundary α in titanium alloys [J]. Acta Mater., 2016, 102: 197
doi: 10.1016/j.actamat.2015.09.021
|
| [50] |
Li H, Wei D, Zhang H Q, et al. Texture evolution and controlling of high-strength titanium alloy tube in cold pilgering for properties tailoring [J]. J. Mater. Process. Technol., 2020, 279: 116520
doi: 10.1016/j.jmatprotec.2019.116520
|
| [51] |
Chatterjee R, Narayana Murty S V S, Alankar A. Dynamic recrystallization in titanium alloys: A comprehensive review [J]. Mater. Perform. Charact., 2020, 9: 1
|
| [52] |
Hall E O. The deformation and ageing of mild steel: III Discussion of results [J]. Proc. Phys. Soc., 1951, 64B: 747
|
| [53] |
Petch N J. The cleavage strength of polycrystals [J]. J. Iron Steel Inst., 1953, 174: 25
|
| [54] |
Hémery S, Naït-Ali A, Smerdova O, et al. Deformation mechanisms in the α phase of the Ti-6Al-2Sn-4Zr-2Mo titanium alloy: In situ experiments and simulations [J]. Int. J. Plast., 2024, 175: 103947
doi: 10.1016/j.ijplas.2024.103947
|
| [55] |
Spurr W F, Quist W E. The effects of crystallographic texture on the mechanical and fracture properties of Ti-3Al-2.5V hydraulic tubing [J]. SAE Trans., 1973, 82: 730515
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|