细观力学模拟双峰晶粒分布铜的异质变形诱导效应
李少杰1, 金剑锋1,2(), 田艳中1, 潘虎成1, 王明涛1, 秦高梧1,2,3()
1 东北大学 材料科学与工程学院 沈阳 110819
2 辽宁材料实验室 材料智能技术研究所 沈阳 110167
3 沈阳化工大学 战略材料与关键构件研究院 沈阳 110142
Micromechanics Modeling of the Hetero-Deformation Induced Strengthening and Strain Hardening Effect in Bimodal Structure Copper
LI Shaojie1, JIN Jianfeng1,2(), TIAN Yanzhong1, PAN Hucheng1, WANG Mingtao1, QIN Gaowu1,2,3()
1 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
2 Institute of Materials Intelligent Technology, Liaoning Academy of Materials, Shenyang 110167, China
3 Institute for Strategic Materials and Components, Shenyang University of Chemical Technology, Shenyang 110142, China
引用本文:

李少杰, 金剑锋, 田艳中, 潘虎成, 王明涛, 秦高梧. 细观力学模拟双峰晶粒分布铜的异质变形诱导效应[J]. 金属学报, 2026, 62(10): 1687-1701.
Shaojie LI, Jianfeng JIN, Yanzhong TIAN, Hucheng PAN, Mingtao WANG, Gaowu QIN. Micromechanics Modeling of the Hetero-Deformation Induced Strengthening and Strain Hardening Effect in Bimodal Structure Copper[J]. Acta Metall Sin, 2026, 62(10): 1687-1701.

全文: PDF(2980 KB)   HTML
摘要: 

双峰异质结构金属因其独特的异质变形诱导(HDI)强化和应变硬化效应,可具有强塑兼备的力学性能;然而HDI微观机制如何发挥作用尚不清晰。本工作基于Mori-Tanaka平均场方法,以双峰异构金属Cu为例(细晶230 nm和粗晶3 μm),构建了细观力学模型的框架,其中双峰结构由微米级粗晶作为粒子相、纳米级细晶作为基体相的异构基元构成;结合塑性应变梯度与位错密度演化理论,将塑性变形过程中产生的HDI效应以软域硬化、硬域软化和应力再协调三个阶段引入各相的本构关系中,定量评估HDI效应对双峰结构材料整体力学行为的影响。通过对比计算与实验结果,认为硬域中的前应力效应归因于前应力促使硬域内缠结位错的解缠而导致的软化与促使硬域内剪切带形成而导致的硬化的共同作用。通过与双峰结构铜的实验拉伸应力-应变曲线比较,验证了模型的有效性。结果表明,当硬域完全包裹软域时,前应力效应对双峰结构铜的综合力学性能起主要作用;随着软域体积分数的增加,双峰结构铜整体强度增加而拉伸塑性下降;当软域体积分数为25%~30%时,存在强塑匹配最佳值:双峰结构铜的抗拉强度417~420 MPa、延伸率28.2%~29.8%,相比均质细晶Cu,强度减低7%、拉伸塑性提升了10倍;相比均质粗晶Cu,强度提高约100%、拉伸塑性降低约50%。

关键词 : 双峰结构,  细观力学,  塑性应变梯度理论,  异质变形诱导效应,  力学性能    
Abstract:

Owing to their unique hetero-deformation induced (HDI) strengthening and strain hardening effect, bimodal structure alloys can exhibit excellent strength-ductility synergy. However, the roles of the HDI mechanism remain incompletely understood. This study establishes a micromechanical model of the bimodal structure of pure Cu with 230 nm fine grains and 3 μm coarse grains as an example and estimates the HDI effects on the mechanical properties of Cu. This model is based on the Mori-Tanaka mean field method. The bimodal structure comprises a particulate inclusion phase of coarse grains (soft zone) and a hard matrix phase of fine grains (hard zone). Combining plastic strain gradient and dislocation theories, the HDI effect is proposed as a three-stage process of soft zone hardening, hard zone softening, and stress repartitioning, thereby providing quantitative assessments of the HDI effects on the overall mechanical behaviors of bimodal copper. Based on the experimental observations, the forward stress effect is considered to result from softening via the disentanglement and annihilation of entangled dislocations and from hardening caused by shear band formations. The model predictions favorably agree with the existing experimental data. The role of the forward stress effect in the mechanical response is apparently enhanced when the hard zone (230 nm grains) completely encloses the soft zone (3 μm grains). Moreover, increasing the volume fraction of the soft zone decreases the overall strength and reduces the ductility of Cu. At soft zone fractions of 25%-30%, the strength and ductility were optimally balanced with a tensile strength of 417-420 MPa and an elongation of 28.2%-29.8%. The ultimate tensile strength and elongation were 7% lower and 10-fold higher, respectively, than those of unimodal 230-nm-grained Cu and almost doubled and halved, respectively, from those of unimodal 3-μm-grained Cu.

Key words: bimodal structure    micromechanics    strain gradient theory of plasticity    heterogeneous deformation-induced (HDI) effect    mechanical property
收稿日期: 2024-09-03     
ZTFLH:  TG146.1  
基金资助:国家重点研发计划项目(2023YFB3710900)
通讯作者: 金剑锋,jinjf@atm.neu.edu.cn,主要从事计算材料学、颗粒增强复合材料力学性能方面的研究;
秦高梧,qingw@smm.neu.edu.cn,主要从事计算材料学辅助高性能、新材料设计和制备方面的研究
Corresponding author: JIN Jianfeng, associate professor, Tel: 13194248493, E-mail: jinjf@atm.neu.edu.cn;
QIN Gaowu, professor, Tel: (024)83691565, E-mail: qingw@smm.neu.edu.cn
作者简介: 李少杰,男,1995年生,博士生
图1  双峰结构异构基元的几何建模
图2  软域硬化示意图
图3  硬域软化示意图
图4  应力再协调示意图
图5  双峰结构细观力学模型的框架
Parameter typeSymbolUnitParameter valueNote
Hard zoneSoft zone
Elastic modulusEGPa121.1121.11*
Shear modulusμGPa45.245.2
Poisson's ratiov-0.340.34
Burgers vector magnitudebnm0.2560.256
Taylor factorM-3.063.06
Taylor constantα-0.330.33
Rate sensitivity exponentm-2020
Initial dislocation densityρ0m-26.7 × 10141.89 × 10132*
Geometric factork0-2.200.08
Proportionality factork1-0.1500.013
Dynamic recovery factork2-39.81.31
Size of zoneΓμm-6
Dislocation pileup spacinghnm15423*
Dynamic recovery factor of GNDsk3-7
Stress attenuation factorλ-0.1
Saturation accumulated shear strainγ0SB-0.20-
表1  双峰结构铜的材料和模拟参数
图6  双峰结构铜平均场模型的模拟结果及与实验值[4,74]的比较
No.Stress componentConstitutive equation
T1With HDI effectσf,0=Mαμbρ0S+ρ0I+ρ0G+σ1Bσf,1=Mαμbρ1SR+ρ1G+σ1B
T2Without HDI effectσf,0=Mαμbρ0Sσf,1=Mαμbρ1S
T3Without forward stress (FS) effectσf,0=Mαμbρ0Sσf,1=Mαμbρ1SR+ρ1G+σ1B
T4Without hard zone softeningσf,0=Mαμbρ0S+ρ0G+σ0Bσf,1=Mαμbρ1SR+ρ1G+σ1B
T5Without shear band hardeningσf,0=Mαμbρ0S+ρ0Iσf,1=Mαμbρ1SR+ρ1G+σ1B
T6Without compensating dislocation effectσf,0=Mαμbρ0S+ρ0I+ρ0G+σ1Bσf,1=Mαμbρ1S+ρ1G+σ1B
表2  考虑不同影响因素的本构方程
图7  双峰结构铜中各类强化/软化单一因素对力学性能的影响
图8  当软域体积分数为5%~65%时,双峰结构铜的屈服强度、抗拉强度、均匀延伸率的变化趋势
图9  双峰结构铜的强度-拉伸塑性关系图
[1] Zhu Y T, Wu X L. Heterostructured materials[J]. Prog. Mater. Sci., 2023, 131: 101019
doi: 10.1016/j.pmatsci.2022.101019
[2] Wu X L, Zhu Y T. Heterostructured metallic materials: Plastic deformation and strain hardening[J]. Acta Metall. Sin., 2022, 58: 1349
doi: 10.11900/0412.1961.2022.00327
[2] 武晓雷, 朱运田. 异构金属材料及其塑性变形与应变硬化[J]. 金属学报, 2022, 58: 1349
doi: 10.11900/0412.1961.2022.00327
[3] Tellkamp V L, Lavernia E J, Melmed A. Mechanical behavior and microstructure of a thermally stable bulk nanostructured Al alloy[J]. Metall. Mater. Trans., 2001, 32A: 2335
[4] Wang Y M, Chen M W, Zhou F H, et al. High tensile ductility in a nanostructured metal[J]. Nature, 2002, 419: 912
doi: 10.1038/nature01133
[5] Li Y S, Zhang Y, Tao N R, et al. Effect of thermal annealing on mechanical properties of a nanostructured copper prepared by means of dynamic plastic deformation[J]. Scr. Mater., 2008, 59: 475
doi: 10.1016/j.scriptamat.2008.04.043
[6] Bach J, Stoiber M, Schindler L, et al. Deformation mechanisms and strain rate sensitivity of bimodal and ultrafine-grained copper[J]. Acta Mater., 2020, 186: 363
doi: 10.1016/j.actamat.2019.12.044
[7] Qian T, Karaman I, Marx M. Mechanical properties of nanocrystalline and ultrafine-grained nickel with bimodal microstructure[J]. Adv. Eng. Mater., 2014, 16: 1323
doi: 10.1002/adem.v16.11
[8] Prasad M J N V, Suwas S, Chokshi A H. Microstructural evolution and mechanical characteristics in nanocrystalline nickel with a bimodal grain-size distribution[J]. Mater. Sci. Eng., 2009, A503: 86
[9] Tejedor R, Rodríguez-Baracaldo R, Benito J A, et al. Plastic deformation of a nanostructured and ultra-fine grained Fe-1%Cr with a bimodal grain size distribution[J]. Int. J. Mater. Form., 2008, 1: 487
doi: 10.1007/s12289-008-0109-x
[10] Fan G J, Choo H, Liaw P K, et al. Plastic deformation and fracture of ultrafine-grained Al-Mg alloys with a bimodal grain size distribution[J]. Acta Mater., 2006, 54: 1759
doi: 10.1016/j.actamat.2005.11.044
[11] Lee Z, Radmilovic V, Ahn B, et al. Tensile deformation and fracture mechanism of bulk bimodal ultrafine-grained Al-Mg alloy[J]. Metall. Mater. Trans., 2010, 41A: 795
[12] Shakoori Oskooie M, Asgharzadeh H, Kim H S. Microstructure, plastic deformation and strengthening mechanisms of an Al-Mg-Si alloy with a bimodal grain structure[J]. J. Alloys Compd., 2015, 632: 540
doi: 10.1016/j.jallcom.2015.01.229
[13] He J H, Jin L, Wang F H, et al. Mechanical properties of Mg-8Gd-3Y-0.5Zr alloy with bimodal grain size distributions[J]. J. Magnes. Alloy., 2017, 5: 423
doi: 10.1016/j.jma.2017.09.004
[14] Xu C, Fan G H, Nakata T, et al. Deformation behavior of ultra-strong and ductile Mg-Gd-Y-Zn-Zr alloy with bimodal microstructure[J]. Metall. Mater. Trans., 2018, 49A: 1931
[15] Zhang H, Wang H Y, Wang J G, et al. The synergy effect of fine and coarse grains on enhanced ductility of bimodal-structured Mg alloys[J]. J. Alloys Compd., 2019, 780: 312
doi: 10.1016/j.jallcom.2018.11.229
[16] Jin Z Z, Zha M, Yu Z Y, et al. Exploring the Hall-Petch relation and strengthening mechanism of bimodal-grained Mg-Al-Zn alloys[J]. J. Alloys Compd., 2020, 833: 155004
doi: 10.1016/j.jallcom.2020.155004
[17] Wei X X, Jin L, Wang F H, et al. High strength and ductility Mg-8Gd-3Y-0.5Zr alloy with bimodal structure and nano-precipitates[J]. J. Mater. Sci. Technol., 2020, 44: 19
doi: 10.1016/j.jmst.2019.10.024
[18] Liu S S, Zhang J L, Chen X, et al. Improving mechanical properties of heterogeneous Mg-Gd alloy laminate via accumulated extrusion bonding[J]. Mater. Sci. Eng., 2020, A785: 139324
[19] Wang Y F, Huang C X, He Q, et al. Heterostructure induced dispersive shear bands in heterostructured Cu[J]. Scr. Mater., 2019, 170: 76
doi: 10.1016/j.scriptamat.2019.05.036
[20] Li G D, Morinaka S, Kawabata M, et al. Improvement of strength with maintaining ductility of harmonic structure pure copper by cold rolling and annealing process[J]. Procedia Manuf., 2018, 15: 1641
[21] Park H K, Ameyama K, Yoo J, et al. Additional hardening in harmonic structured materials by strain partitioning and back stress[J]. Mater. Res. Lett., 2018, 6: 261
doi: 10.1080/21663831.2018.1439115
[22] Wu X L, Yang M X, Yuan F P, et al. Heterogeneous lamella structure unites ultrafine-grain strength with coarse-grain ductility[J]. Proc. Natl. Acad. Sci. USA, 2015, 112: 14501
doi: 10.1073/pnas.1517193112 pmid: 26554017
[23] Zhou X, Li X Y, Lu K. Stabilizing nanograins in metals with grain boundary relaxation[J]. Scr. Mater., 2020, 187: 345
doi: 10.1016/j.scriptamat.2020.06.047
[24] Yasnikov I S, Kaneko Y, Uchida M, et al. The grain size effect on strain hardening and necking instability revisited from the dislocation density evolution approach[J]. Mater. Sci. Eng., 2022, A831: 142330
[25] Bouaziz O, Estrin Y, Bréchet Y, et al. Critical grain size for dislocation storage and consequences for strain hardening of nanocrystalline materials[J]. Scr. Mater., 2010, 63: 477
doi: 10.1016/j.scriptamat.2010.05.006
[26] Wu X L, Zhu Y T. Heterogeneous materials: A new class of materials with unprecedented mechanical properties[J]. Mater. Res. Lett., 2017, 5: 527
doi: 10.1080/21663831.2017.1343208
[27] Zhu L L, Lu J. Modelling the plastic deformation of nanostructured metals with bimodal grain size distribution[J]. Int. J. Plast., 2012, 30-31: 166
doi: 10.1016/j.ijplas.2011.10.003
[28] Li J J, Lu W J, Chen S H, et al. Revealing extra strengthening and strain hardening in heterogeneous two-phase nanostructures[J]. Int. J. Plast., 2020, 126: 102626
doi: 10.1016/j.ijplas.2019.11.005
[29] Cheng Z, Bu L F, Zhang Y, et al. Unraveling the origin of extra strengthening in gradient nanotwinned metals[J]. Proc. Natl. Acad. Sci. USA, 2022, 119: e2116808119
doi: 10.1073/pnas.2116808119
[30] Wang Y F, Zhu Y T, Yu Z J, et al. Hetero-zone boundary affected region: A primary microstructural factor controlling extra work hardening in heterostructure[J]. Acta Mater., 2022, 241: 118395
doi: 10.1016/j.actamat.2022.118395
[31] Wu H, Fan G H. An overview of tailoring strain delocalization for strength-ductility synergy[J]. Prog. Mater. Sci., 2020, 113: 100675
doi: 10.1016/j.pmatsci.2020.100675
[32] Li J J, Qin F, Yan D S, et al. Shear instability in heterogeneous nanolayered Cu/Zr composites[J]. J. Mater. Sci. Technol., 2022, 105: 81
doi: 10.1016/j.jmst.2021.06.070
[33] Wu X L, Yang M X, Li R G, et al. Plastic accommodation during tensile deformation of gradient structure[J]. Sci. China Mater., 2021, 64: 1534
doi: 10.1007/s40843-020-1545-2
[34] Fan G H, Miao K S, Li D Y, et al. Unraveling the strength-ductility synergy of heterostructured metallic materials from the perspective of local stress/strain[J]. Acta Metall. Sin., 2022, 58: 1427
doi: 10.11900/0412.1961.2022.00317
[34] 范国华, 缪克松, 李丹阳 等. 从局域应力/应变视角理解异构金属材料的强韧化行为[J]. 金属学报, 2022, 58: 1427
doi: 10.11900/0412.1961.2022.00317
[35] Yuan R, Beyerlein I J, Zhou C Z. Homogenization of plastic deformation in heterogeneous lamella structures[J]. Mater. Res. Lett., 2017, 5: 251
doi: 10.1080/21663831.2016.1255264
[36] Ma H W, Zhao Y C, Lyu Z, et al. What are the “dispersive shear bands” on the surfaces of layered heterostructured materials?[J]. J. Mech. Phys. Solids, 2023, 181: 105467
doi: 10.1016/j.jmps.2023.105467
[37] Wang Y F, Huang C X, Li Y S, et al. Dense dispersed shear bands in gradient-structured Ni[J]. Int. J. Plast., 2020, 124: 186
doi: 10.1016/j.ijplas.2019.08.012
[38] Estrin Y, Vinogradov A. Extreme grain refinement by severe plastic deformation: A wealth of challenging science[J]. Acta Mater., 2013, 61: 782
doi: 10.1016/j.actamat.2012.10.038
[39] Peng P, Tang A T, She J, et al. Significant improvement in yield stress of Mg-Gd-Mn alloy by forming bimodal grain structure[J]. Mater. Sci. Eng., 2021, A803: 140569
[40] Renk O, Hohenwarter A, Pippan R. Cyclic deformation behavior of a 316L austenitic stainless steel processed by high pressure torsion[J]. Adv. Eng. Mater., 2012, 14: 948
doi: 10.1002/adem.v14.11
[41] Huang C X, Wang Y F, Ma X L, et al. Interface affected zone for optimal strength and ductility in heterogeneous laminate[J]. Mater. Today, 2018, 21: 713
doi: 10.1016/j.mattod.2018.03.006
[42] Zhu L L, Shi S Q, Lu K, et al. A statistical model for predicting the mechanical properties of nanostructured metals with bimodal grain size distribution[J]. Acta Mater., 2012, 60: 5762
doi: 10.1016/j.actamat.2012.06.059
[43] Weng G J. The overall elastoplastic stress-strain relations of dual-phase metals[J]. J. Mech. Phys. Solids, 1990, 38: 419
doi: 10.1016/0022-5096(90)90007-Q
[44] Delincé M, Bréchet Y, Embury J D, et al. Structure-property optimization of ultrafine-grained dual-phase steels using a microstructure-based strain hardening model[J]. Acta Mater., 2007, 55: 2337
doi: 10.1016/j.actamat.2006.11.029
[45] Gao H J, Huang Y G. Taylor-based nonlocal theory of plasticity[J]. Int. J. Solids Struct., 2001, 38: 2615
doi: 10.1016/S0020-7683(00)00173-6
[46] Orowan E. Zur kristallplastizität. III: Über den mechanismus des gleitvorganges[J]. Z. Phys., 1934, 89: 634
doi: 10.1007/BF01341480
[47] Taylor G I. The mechanism of plastic deformation of crystals. Part I.—Theoretical[J]. Proc. Roy. Soc., 1934, 145A: 362
[48] Zerilli F J, Armstrong R W. Dislocation-mechanics-based constitutive relations for material dynamics calculations[J]. J. Appl. Phys., 1987, 61: 1816
doi: 10.1063/1.338024
[49] Elmasry A, Azoti W, El-Safty S A, et al. A comparative review of multiscale models for effective properties of nano- and micro-composites[J]. Prog. Mater. Sci., 2023, 132: 101022
doi: 10.1016/j.pmatsci.2022.101022
[50] Mori T, Tanaka K. Average stress in matrix and average elastic energy of materials with misfitting inclusions[J]. Acta Metall., 1973, 21: 571
doi: 10.1016/0001-6160(73)90064-3
[51] Benveniste Y. A new approach to the application of Mori-Tanaka's theory in composite materials[J]. Mech. Mater., 1987, 6: 147
doi: 10.1016/0167-6636(87)90005-6
[52] Li J J, Chen S H, Weng G J, et al. A micromechanical model for heterogeneous nanograined metals with shape effect of inclusions and geometrically necessary dislocation pileups at the domain boundary[J]. Int. J. Plast., 2021, 144: 103024
doi: 10.1016/j.ijplas.2021.103024
[53] Mura T. Micromechanics of Defects in Solids[M]. 2nd Ed., Dordrecht: Springer, 1987: 188
[54] Bishop J F W, XLVI Hill R.. A theory of the plastic distortion of a polycrystalline aggregate under combined stresses[J]. London Edinburgh Dublin Philos. Mag. J. Sci., 1951, 42: 414
[55] Li J J, Lu W J, Gibson J, et al. Eliminating deformation incompatibility in composites by gradient nanolayer architectures[J]. Sci. Rep., 2018, 8: 16216
doi: 10.1038/s41598-018-34369-9 pmid: 30385852
[56] Крутков Ю А. Тензор Функций Напряжений И Общие Решения В Статике Теории Упругости[M]. Москва: Изд-во АН СССР, 1949: 1
[57] Qu J M, Cherkaoui M. Fundamentals of Micromechanics of Solids[M]. Hoboken: Wiley, 2006: 73
[58] Kachanov M, Sevostianov I. Micromechanics of Materials, with Applications[M]. Cham: Springer, 2018: 391
[59] Shen G L, Hu G K. Mechanics of Composite Materials[M]. Beijing: Tsinghua University Press, 2006: 246
[59] 沈观林, 胡更开. 复合材料力学[M]. 北京: 清华大学出版社, 2006: 246
[60] Jiang S, Lin Peng R, Zhao X, et al. Deformation incompatibility enables hetero-deformation induced strengthening in Ti/Nb laminates[J]. Mater. Res. Lett., 2023, 11: 126
doi: 10.1080/21663831.2022.2128916
[61] Nix W D, Gao H J. Indentation size effects in crystalline materials: A law for strain gradient plasticity[J]. J. Mech. Phys. Solids, 1998, 46: 411
doi: 10.1016/S0022-5096(97)00086-0
[62] Feaugas X. On the origin of the tensile flow stress in the stainless steel AISI 316L at 300 K: Back stress and effective stress[J]. Acta Mater., 1999, 47: 3617
doi: 10.1016/S1359-6454(99)00222-0
[63] Yang M X, Pan Y, Yuan F P, et al. Back stress strengthening and strain hardening in gradient structure[J]. Mater. Res. Lett., 2016, 4: 145
doi: 10.1080/21663831.2016.1153004
[64] Zhou H, Huang C X, Sha X C, et al. In-situ observation of dislocation dynamics near heterostructured interfaces[J]. Mater. Res. Lett., 2019, 7: 376
doi: 10.1080/21663831.2019.1616330
[65] Hasegawa T, Yakou T, Kocks U F. Forward and reverse rearrangements of dislocations in tangled walls[J]. Mater. Sci. Eng., 1986, 81: 189
doi: 10.1016/0025-5416(86)90262-4
[66] Zirkle T, Zhu T, McDowell D L. Micromechanical crystal plasticity back stress evolution within FCC dislocation substructure[J]. Int. J. Plast., 2021, 146: 103082
doi: 10.1016/j.ijplas.2021.103082
[67] Marukawa K, Sanpei T. Stability of the work hardened state against stress reversal in copper single crystals[J]. Acta Metall., 1971, 19: 1169
doi: 10.1016/0001-6160(71)90049-6
[68] Rassweiler G M, Grube W L. Internal Stresses and Fatigue in Metals[M]. Amsterdam: Elsevier, 1959: 1
[69] Wu X L, Jiang P, Chen L, et al. Extraordinary strain hardening by gradient structure[J]. Proc. Natl. Acad. Sci. USA, 2014, 111: 7197
doi: 10.1073/pnas.1324069111 pmid: 24799688
[70] Hirsch J, Lücke K, Hatherly M. Overview No.76: Mechanism of deformation and development of rolling textures in polycrystalline f.c.c. Metals—III. The influence of slip inhomogeneities and twinning[J]. Acta Metall., 1988, 36: 2905
doi: 10.1016/0001-6160(88)90174-5
[71] Wang Y F, Huang C X, Li Z K, et al. Shear band stability and uniform elongation of gradient structured material: Role of lateral constraint[J]. Extreme Mech. Lett., 2020, 37: 100686
doi: 10.1016/j.eml.2020.100686
[72] Wang Y F, Wei Y G, Zhao Z F, et al. Mechanical response of the constrained nanostructured layer in heterogeneous laminate[J]. Scr. Mater., 2022, 207: 114310
doi: 10.1016/j.scriptamat.2021.114310
[73] Wang Y F, Wei Y G, Zhao Z F, et al. Activating dispersed strain bands in tensioned nanostructure layer for high ductility: The effects of microstructure inhomogeneity[J]. Int. J. Plast., 2022, 149: 103159
doi: 10.1016/j.ijplas.2021.103159
[74] Li G D, Jiang J X, Ma H C, et al. Superior strength-ductility synergy in three-dimensional heterogeneous-nanostructured metals[J]. Acta Mater., 2023, 256: 119143
doi: 10.1016/j.actamat.2023.119143
[75] Gao H J, Huang Y G. Geometrically necessary dislocation and size-dependent plasticity[J]. Scr. Mater., 2003, 48: 113
doi: 10.1016/S1359-6462(02)00329-9
[76] von Considére M. Memoire sur L'emploi du fer et de L'acier Dans les Constructions[M]. Paris: Ch. Dunod, 1885: 1
[77] Recht R F. Catastrophic thermoplastic shear[J]. J. Appl. Mech., 1964, 31: 189
doi: 10.1115/1.3629585
[78] Meyers M A, Subhash G, Kad B K, et al. Evolution of microstructure and shear-band formation in α-hcp titanium[J]. Mech. Mater., 1994, 17: 175
doi: 10.1016/0167-6636(94)90058-2
[79] Armstrong R W, Zerilli F J. Dislocation mechanics aspects of plastic instability and shear banding[J]. Mech. Mater., 1994, 17: 319
doi: 10.1016/0167-6636(94)90069-8
[80] Xu Y B, Zhang J H, Bai Y L, et al. Shear localization in dynamic deformation: Microstructural evolution[J]. Metall. Mater. Trans., 2008, 39A: 811
[81] Liu X L, Yuan F P, Zhu Y T, et al. Extraordinary Bauschinger effect in gradient structured copper[J]. Scr. Mater., 2018, 150: 57
doi: 10.1016/j.scriptamat.2018.03.007
[82] Yang Y, Gong Y L, Li X F, et al. Effect of bimodal grain size and gradient structure on heterogeneous deformation induced (HDI) stress and mechanical properties of Cu[J]. Mater. Res. Express, 2022, 9: 035004
[83] Shimokawa T, Hasegawa T, Kiyota K, et al. Heterogeneous evolution of lattice defects leading to high strength and high ductility in harmonic structure materials through atomic and dislocation simulations[J]. Acta Mater., 2022, 226: 117679
doi: 10.1016/j.actamat.2022.117679
[84] Wu H, Huang M, Li X W, et al. Temperature-dependent reversed fracture behavior of multilayered TiBw/Ti-Ti(Al) composites[J]. Int. J. Plast., 2021, 141: 102998
doi: 10.1016/j.ijplas.2021.102998
[85] Tian Y Z, Ren Y P, Gao S, et al. Two-stage Hall-Petch relationship in Cu with recrystallized structure[J]. J. Mater. Sci. Technol., 2020, 48: 31
doi: 10.1016/j.jmst.2019.12.023
[1] 郭传平, 石尘尘, 刘鹏, 高冬芳, 赵洋洋, 乔阳. 基于机器学习的生物可降解锌合金力学性能预测[J]. 金属学报, 2026, 62(9): 1615-1626.
[2] 刘泽田, 路伟昭, 徐新宇, 刘旭, 张少游, 王慧远. 均质化温度对3003铝合金微观组织和力学性能的影响规律[J]. 金属学报, 2026, 62(9): 1503-1516.
[3] 李帅雨, 刘泽栋, 杨劼人, 金伟, 彭博, 杜新, 周斯曼. TA18合金铸锭-管坯组织遗传行为及力学性能调控[J]. 金属学报, 2026, 62(9): 1487-1502.
[4] 杨何, 侯自勇, 胡兴益, 程金骏, 王亚茹, 范国华, 黄晓旭. 超高强不锈钢微丝表征技术:进展与展望[J]. 金属学报, 2026, 62(7): 1189-1206.
[5] 许鼎锋, 韩飞扬, 姜琦成, 王欢, 尚利媛, 卢一平. AlCrFeCoNi低膨胀合金的成分设计及组织和性能优化[J]. 金属学报, 2026, 62(6): 1021-1031.
[6] 王彬, 赵鹏, 刘家伟, 张春波, 秦志伟, 董红刚, 李鹏. 热处理对FGH96高温合金惯性摩擦焊接头微观组织演变及力学性能的影响[J]. 金属学报, 2026, 62(6): 1043-1058.
[7] 郑玉峰, 谌雨农. 纯Mo及钼基可降解金属材料的研究现状与发展趋势[J]. 金属学报, 2026, 62(5): 905-922.
[8] 吕昭平, 申耀祖, 王先珍, 陈强, 唐建国, 张晓宾, 于勇, 蒋虽合, 刘雄军, 王辉, 吴渊. 面向极端服役条件的高熵合金结构材料:性能优势、瓶颈与突破路径[J]. 金属学报, 2026, 62(5): 743-755.
[9] 陈光, 陈奉锐, 朱德民, 李贵忠, 李罗, 宋伟东, 王子特, 相恒高, 陈旸, 祁志祥. 聚片孪生功能基元序构的高性能TiAl合金[J]. 金属学报, 2026, 62(4): 541-549.
[10] 王建峰, 许珍木, 刘战, 高转妮, 占小红. 超声振动对TC4钛合金窄间隙激光焊接组织及强化机理的影响[J]. 金属学报, 2026, 62(3): 406-420.
[11] 蒋志达, 胥杨洋, 于佳新, 刘文才, 朱浩文, 吴国华, 尚郑平. 高温无氧轧制Cu/1060Al/Cu三层复合材料的力学和导电性能[J]. 金属学报, 2026, 62(3): 431-444.
[12] 江国龙, 周霞. 超声辅助下Mg/Mg-Zn-Al钎焊界面行为的分子动力学模拟[J]. 金属学报, 2026, 62(2): 372-382.
[13] 黄成聪, 李亚庚, 王鲁宁. 粉末特征对激光粉末床熔融制备可降解Zn-Mn-Mg合金组织与力学性能的影响[J]. 金属学报, 2026, 62(10): 1702-1712.
[14] 王启勇, 李晓博, 刘小超, 王心成, 张泰瑞, 倪中华, 陈彪. 低碳钢预制涡流搅拌摩擦焊工艺研究[J]. 金属学报, 2026, 62(1): 217-234.
[15] 张天宇, 张鹏, 肖娜, 王小海, 刘国强, 杨志刚, 张弛. 奥氏体化温度对2 GPa超高强钢显微组织和力学性能的影响[J]. 金属学报, 2025, 61(9): 1353-1363.