| 纳米ZrB2 增强CoNiCrAlY复合粉末的机械合金化制备及其涂层的组织与性能 |
杨康, 辛越, 姜自滔, 刘侠, 薛召露, 张世宏( ) |
| 安徽工业大学 先进金属材料绿色制备与表面技术教育部重点实验室 马鞍山 243002 |
|
| Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings |
YANG Kang, XIN Yue, JIANG Zitao, LIU Xia, XUE Zhaolu, ZHANG Shihong( ) |
| Key Laboratory of Green Fabrication and Surface Technology of Advanced Metal Materials, Ministry of Education, Anhui University of Technology, Ma'anshan 243002, China |
引用本文:
杨康, 辛越, 姜自滔, 刘侠, 薛召露, 张世宏. 纳米ZrB2 增强CoNiCrAlY复合粉末的机械合金化制备及其涂层的组织与性能[J]. 金属学报, 2025, 61(4): 619-631.
Kang YANG,
Yue XIN,
Zitao JIANG,
Xia LIU,
Zhaolu XUE,
Shihong ZHANG.
Mechanical Alloying Fabrication of Nano-ZrB2-Reinforced CoNiCrAlY Composite Powders and Microstructure-Property Characterization of the Resultant Coatings[J]. Acta Metall Sin, 2025, 61(4): 619-631.
| 1 |
Matthews S, James B. Review of thermal spray coating applications in the steel industry: Part 1—Hardware in steel making to the continuous annealing process [J]. J. Therm. Spray Technol., 2010, 19: 1267
|
| 2 |
Bolelli G, Candeli A, Lusvarghi L, et al. Tribology of NiCrAlY + Al2O3 composite coatings by plasma spraying with hybrid feeding of dry powder + suspension [J]. Wear, 2015, 344-345: 69
|
| 3 |
Hou G L, An Y L, Zhao X Q, et al. Effect of alumina dispersion on oxidation behavior as well as friction and wear behavior of HVOF-sprayed CoCrAlYTaCSi coating at elevated temperature up to 1000 oC [J]. Acta Mater., 2015, 95: 164
|
| 4 |
Taylor T A, Bettridge D F. Development of alloyed and dispersion-strengthened MCrAlY coatings [J]. Surf. Coat. Technol., 1996, 86-87: 9
|
| 5 |
Zhao L D, Parco M, Lugscheider E. Wear behaviour of Al2O3 dispersion strengthened MCrAlY coating [J]. Surf. Coat. Technol., 2004, 184: 298
|
| 6 |
Taha M A, Youness R A, Zawrah M F. Review on nanocomposites fabricated by mechanical alloying [J]. Int. J. Miner. Metall. Mater., 2019, 26: 1047
|
| 7 |
Suryanarayana C, Al-Joubori A A, Wang Z. Nanostructured materials and nanocomposites by mechanical alloying: An overview [J]. Met. Mater. Int., 2022, 28: 41
doi: 10.1007/s12540-021-00998-5
|
| 8 |
Liu C J, Sun W Y, Chen M H, et al. High-temperature oxidation behavior of spark plasma sintered Ni20Cr-xAl alloys [J]. Acta Metall. Sin., 2024, 60: 485
|
| 8 |
刘丞济, 孙文瑶, 陈明辉 等. 放电等离子烧结Ni20Cr-xAl合金的高温氧化行为 [J]. 金属学报, 2024, 60: 485
doi: 10.11900/0412.1961.2022.00240
|
| 9 |
Bi S, Li Z C, Sun H X, et al. Microstructure and mechanical properties of carbon nanotubes-reinforced 7055Al composites fabricated by high-energy ball milling and powder metallurgy processing [J]. Acta Metall. Sin., 2021, 57: 71
doi: 10.11900/0412.1961.2020.00238
|
| 9 |
毕 胜, 李泽琛, 孙海霞 等. 高能球磨结合粉末冶金法制备碳纳米管增强7055Al复合材料的微观组织和力学性能[J]. 金属学报, 2021, 57: 71
|
| 10 |
Niespodziana K, Jurczyk K, Jakubowicz J, et al. Fabrication and properties of titanium-hydroxyapatite nanocomposites [J]. Mater. Chem. Phys., 2010, 123: 160
|
| 11 |
Cen S B, Chen H, Liu Y, et al. Effect of CeO2 on corrosion behavior of WC-12Co coatings by high velocity oxygen fuel [J]. Acta Metall. Sin., 2016, 52: 1441
|
| 11 |
岑升波, 陈 辉, 刘 艳 等. CeO2对超音速火焰喷涂WC-12Co涂层腐蚀行为的影响 [J]. 金属学报, 2016, 52: 1441
doi: 10.11900/0412.1961.2016.00031
|
| 12 |
Hou G L, Zhou H D, An Y L, et al. Microstructure and high-temperature friction and wear behavior of WC-(W, Cr)2C-Ni coating prepared by high velocity oxy-fuel spraying [J]. Surf. Coat. Technol., 2011, 206: 82
|
| 13 |
Silveira L L, Sucharski G B, Pukasiewicz A G M, et al. Influence of particle size distribution on the morphology and cavitation resistance of high-velocity oxygen fuel coatings [J]. J. Therm. Spray Technol., 2018, 27: 695
|
| 14 |
Liu M T, Zhong X C, Wang J, et al. Microstructure and thermal stability of MoSi2-CoNiCrAlY nanocomposite feedstock prepared by high energy ball milling [J]. Surf. Coat. Technol., 2014, 239: 78
|
| 15 |
Richer P, Zúñiga A, Yandouzi M, et al. CoNiCrAlY microstructural changes induced during cold gas dynamic spraying [J]. Surf. Coat. Technol., 2008, 203: 364
|
| 16 |
Tahari M, Shamanian M, Salehi M. Microstructural and morphological evaluation of MCrAlY/YSZ composite produced by mechanical alloying method [J]. J. Alloys Compd., 2012, 525: 44
|
| 17 |
Hernández G I V, Albarrán M A G, de Anda E R, et al. Microstructural and high-temperature cyclic oxidation response of NiCoCrAlY coatings with and without SiC + ZrB2 reactive-element dispenser [J]. Corros. Sci., 2021, 189: 109617
|
| 18 |
Bobzin K, Schläfer T, Richardt K, et al. Development of oxide dispersion strengthened MCrAlY coatings [J]. J. Therm. Spray Technol., 2008, 17: 853
|
| 19 |
Wang H Y, Zuo D W, Wang M D, et al. High temperature frictional wear behaviors of nano-particle reinforced NiCoCrAlY cladded coatings [J]. Trans. Nonferrous Met. Soc. China, 2011, 21: 1322
|
| 20 |
Houdková Š, Kašparová M. Experimental study of indentation fracture toughness in HVOF sprayed hardmetal coatings [J]. Eng. Fract. Mech., 2013, 110: 468
|
| 21 |
Wood P D, Evans H E, Ponton C B. Investigation into the wear behaviour of Stellite 6 during rotation as an unlubricated bearing at 600 oC [J]. Tribol. Int., 2011, 44: 1589
|
| 22 |
Inman I A, Rose S R, Datta P K. Studies of high temperature sliding wear of metallic dissimilar interfaces Ⅱ: Incoloy MA956 versus Stellite 6 [J]. Tribol. Int., 2006, 39: 1361
|
| 23 |
Wood P D, Evans H E, Ponton C B. Investigation into the wear behaviour of Tribaloy 400 oC during rotation as an unlubricated bearing at 600 oC [J]. Wear, 2010, 269: 763
|
| 24 |
Wei Z, Wu Y P, Hong S, et al. Effects of temperature on wear properties and mechanisms of HVOF sprayed CoCrAlYTa-10%Al2O3 coatings and H13 steel [J]. Metals, 2019, 9: 1224
|
| 25 |
Zhou W T, Kong D J. Influence of Al2O3 mass fractions on microstructure, oxidation resistance and friction-wear behaviors of CoCrAlYTaSi coatings [J]. Surf. Coat. Technol., 2019, 379: 125058
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|