| 基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究 |
丁宗业, 胡侨丹( ), 卢温泉, 李建国 |
| 上海交通大学 材料科学与工程学院 上海 200240 |
|
| In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology |
DING Zongye, HU Qiaodan( ), LU Wenquan, LI Jianguo |
| School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China |
引用本文:
丁宗业, 胡侨丹, 卢温泉, 李建国. 基于同步辐射X射线成像液/固复层界面氢气泡的形核、生长演变与运动行为的原位研究[J]. 金属学报, 2022, 58(4): 567-580.
Zongye DING,
Qiaodan HU,
Wenquan LU,
Jianguo LI.
In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. Acta Metall Sin, 2022, 58(4): 567-580.
| 1 |
Zhao X, Sun Y, Hou X Y, et al. Effect of orientation deviation on microstructure and mechanical properties of nickel-based single crystal superalloy brazing joints [J]. Acta Metall. Sin., 2020, 56: 171
|
| 1 |
赵 旭, 孙 元, 侯星宇 等. 取向偏差对镍基单晶高温合金钎焊接头组织与力学性能的影响 [J]. 金属学报, 2020, 56: 171
|
| 2 |
Liu L H, Che C S, Kong G, et al. Destabilization mechanism of Fe-Al inhibition layer in Zn-0.2%Al hot-dip galvanizing coating and related thermodynamic evaluation [J]. Acta Metall. Sin., 2016, 52: 614
|
| 2 |
刘力恒, 车淳山, 孔 纲 等. 热镀Zn-0.2%Al镀层中Fe-Al抑制层失稳机理及其热力学评估 [J]. 金属学报, 2016, 52: 614
|
| 3 |
Sadeghian A, Mirsalehi S E, Arhami F, et al. Effect of bonding time on dissimilar transient liquid phase (TLP) bonding of IN939 to IN625 superalloys: Microstructural characterization and mechanical properties [J]. Metall. Mater. Trans., 2021, 52A: 1526
|
| 4 |
Wen F L, Zhao J H, Yuan M W, et al. Influence of Ni interlayer on interfacial microstructure and mechanical properties of Ti-6Al-4V/AZ91D bimetals fabricated by a solid-liquid compound casting process [J]. J. Magnes. Alloy., 2021, 9: 1382
|
| 5 |
Ding Z Y, Zhang N F, Yu L, et al. Recent progress in metallurgical bonding mechanisms at the liquid/solid interface of dissimilar metals investigated via in situ X-ray imaging technologies [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 145
|
| 6 |
Ding Z Y, Hu Q D, Lu W Q, et al. In situ observation on the formation of intermetallics compounds at the interface of liquid Al/solid Ni [J]. Scr. Mater., 2017, 130: 214
|
| 7 |
Ding Z Y, Hu Q D, Lu W Q, et al. In-situ observation on the diversified morphology and growth behavior of Al3Ni phase at the liquid Al/solid Ni interface [J]. Metall. Mater. Trans., 2018, 49A: 1486
|
| 8 |
Ding Z Y, Hu Q D, Lu W Q, et al. A full view of the interfacial behavior between the liquid Al and solid Ni by synchrotron radiation [J]. Metall. Mater. Trans., 2019, 50A: 300
|
| 9 |
Ding Z Y, Hu Q D, Lu W Q, et al. Continuous morphological transition and its mechanism of Al3Ni phase at the liquid-solid interface during solidification [J]. Metall. Mater. Trans., 2019, 50A: 556
|
| 10 |
Kunwar A. Simulations on the growth of bubbles and interfacial intermetallic compounds in liquid Sn-based soders [D]. Dalian: Dalian University of Technology, 2016
|
| 10 |
Kunwar A. Sn基液态钎焊界面气泡及IMC生长数值模拟研究 [D]. 大连: 大连理工大学, 2016
|
| 11 |
Liu Y. Computer simulation of hydrogen in aluminum [D]. Shanghai: Shanghai Jiao Tong University, 2012
|
| 11 |
柳 洋. 铝中氢行为的计算机模拟研究 [D]. 上海: 上海交通大学, 2012
|
| 12 |
Lee P D, Chirazi A, See D. Modeling microporosity in aluminum-silicon alloys: A review [J]. J. Light Met., 2001, 1: 15
|
| 13 |
Poirier D R, Yeum K, Maples A L. A thermodynamic prediction for microporosity formation in aluminum-rich Al-Cu alloys [J]. Metall. Trans., 1987, 18A: 1979
|
| 14 |
Han Q, Viswanathan S. Hydrogen evolution during directional solidification and its effect on porosity formation in aluminum alloys [J]. Metall. Mater. Trans., 2002, 33A: 2067
|
| 15 |
Li K D, Chang E. Mechanism of nucleation and growth of hydrogen porosity in solidifying A356 aluminum alloy: An analytical solution [J]. Acta Mater., 2004, 52: 219
|
| 16 |
Yousefian P, Tiryakioğlu M. Pore formation during solidification of aluminum: Reconciliation of experimental observations, modeling assumptions, and classical nucleation theory [J]. Metall. Mater. Trans., 2018, 49A: 563
|
| 17 |
Atwood R C, Sridhar S, Zhang W, et al. Diffusion-controlled growth of hydrogen pores in aluminium-silicon castings: In situ observation and modelling [J]. Acta Mater., 2000, 48: 405
|
| 18 |
Yin H B, Koster J N. In-situ observed pore formation during solidification of aluminium [J]. ISIJ Int., 2000, 40: 364
|
| 19 |
Zhang Q Y, Sun D K, Pan S Y, et al. Microporosity formation and dendrite growth during solidification of aluminum alloys: Modeling and experiment [J]. Int. J. Heat Mass Transfer, 2020, 146: 118838
|
| 20 |
Sun S Y, Hu Q D, Lu W Q, et al. In situ observation on bubble behavior of solidifying Al-Ni alloy under the interference of intermetallic compounds [J]. Metall. Mater. Trans., 2018, 49A: 4429
|
| 21 |
Lee P D, Hunt J D. Hydrogen porosity in directional solidified aluminium-copper alloys: In situ observation [J]. Acta Mater., 1997, 45: 4155
|
| 22 |
Zhang S G, Zhang L, Lu W Q, et al. Observation of bubble-involving spontaneous gas dissolution in superheated Al alloy melt [J]. Appl. Phys. Lett., 2013, 103: 164103
|
| 23 |
Lu W Q, Zhang N F, Ding Z Y, et al. Bubble growth, intermetallic compounds dissolution and their interactions during heating of an Al-5wt.%Mn alloy by in-situ synchrotron radiography [J]. J. Alloys Compd., 2020, 822: 153554
|
| 24 |
Lu W Q, Hu Q D, Zhang W, et al. Dynamic behaviors of minor droplets and the role of bubbles in phase-separating Al-Bi immiscible alloy [J]. J. Mol. Liq., 2020, 320: 114478
|
| 25 |
Lu W Q, Zhang N F, Ren N, et al. Bubble-induced formation of new intermetallic compounds in an Al-Mn alloy during heating observed by synchrotron radiography [J]. Materialia, 2021, 15: 100991
|
| 26 |
Campbell J. Entrainment defects [J]. Mater. Sci. Technol., 2006, 22: 127
|
| 27 |
Ding Z Y, Hu Q D, Lu W Q, et al. In-situ study on hydrogen bubble evolution in the liquid Al/solid Ni interconnection by synchrotron radiation X-ray radiography [J]. J. Mater. Sci. Technol., 2019, 35: 1388
|
| 28 |
Ding Z Y, Hu Q D, Lu W Q, et al. Microstructural evolution and growth behavior of intermetallic compounds at the liquid Al/solid Fe interface by synchrotron X-ray radiography [J]. Mater. Charact., 2018, 136: 157
|
| 29 |
Kurz W, Fisher D J, translated by Li J G, Hu Q D. Fundamentals of Solidification [M]. Beijing: Higher Education Press, 2010: 108
|
| 29 |
Kurz W, Fisher D J著, 李建国, 胡侨丹译. 凝固原理 [M]. 北京: 高等教育出版社, 2010: 108
|
| 30 |
Lee P D, Hunt J D. Hydrogen porosity in directionally solidified aluminium-copper alloys: A mathematical model [J]. Acta Mater., 2001, 49: 1383
|
| 31 |
Sun Y Z, Li S C, Zhang G Q, et al. Research on absorbing hydrogen special property of liquid state ZL101 Aluminium alloys [J]. Acta Metall. Sin., 1999, 35: 939
|
| 31 |
孙业赞, 厉松春, 张国强 等. 液态ZL101 Al合金吸氢特性的研究 [J]. 金属学报, 1999, 35: 939
|
| 32 |
Markworth A J. The transverse thermal conductivity of a unidirectional fibre composite with fibre-matrix debonding: A calculation based on effective-medium theory [J]. J. Mater. Sci. Lett., 1993, 12: 1487
|
| 33 |
Tiryakioğlu M. On the heterogeneous nucleation pressure for hydrogen pores in liquid aluminium [J]. Int. J. Cast Met. Res., 2020, 33: 153
|
| 34 |
Ding Z Y, Hu Q D, Yang F, et al. A new sight of the growth characteristics of solidified Al3Ni at the liquid-solid interface by synchrotron radiography and 3D tomography [J]. Metall. Mater. Trans., 2020, 51A: 2689
|
| 35 |
Ding Z Y, Hu Q D, Lu W Q, et al. Intergrowth mechanism and morphology prediction of faceted Al3Ni formed during solidification by a spatial geometric model [J]. J. Mater. Sci. Technol., 2020, 54: 40
|
| 36 |
Takemura F, Yabe A. Gas dissolution process of spherical rising gas bubbles [J]. Chem. Eng. Sci,. 1998, 53: 2691
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|