| 楔横轧轴类件热变形时奥氏体微观组织演变的预测 |
| 王敏婷 杜凤山 李学通 郑炀曾 |
| 燕山大学亚稳材料重点实验室; 秦皇岛 066004 |
|
引用本文:
王敏婷; 杜凤山; 李学通; 郑炀曾 . 楔横轧轴类件热变形时奥氏体微观组织演变的预测[J]. 金属学报, 2005, 41(2): 118-122 .
[1] Hu Z H, Zhang K S, Wang B Y, Zhang W. Cross-Wedge Rolling Theory and Application. Beijing: Metallurgical Industry Press, 1996: 20(胡正寰,张康生,王宝雨,张巍.楔横轧理论与应用.北京:冶金工业出版社, 1996:20) [2] Fu X P. Int J Mach Tools Manuf, 1993; 33(3): 367 [3] Pater Z. J Mater Process Technol, 1999; (92-93): 468 [4] Li Q, Michael R Lovell. J Tribology, 2003; 125: 200 [5] Li Q, Michael R Lovell, Deng Z. Soc Manuf Eng, 2001: 9 [6] Dong Y M, Kaveh A Tagavi, Michael R Lovell. J MaterProcess Technol, 2000; 97: 44 [7] Zhang K S, Hu Z H. Forging Technol, 1996; 4: 30(张康生,胡正寰.锻压技术, 1996;4:30) [8] Feng J C, Zhang W, Hu Z H. J Plast Eng, 1995; 2(1): 61(冯建春,张巍,胡正寰.塑性工程学报, 1995;2(1):61) [9] Hu Z H. Forging Technol, 1995; 5: 25(胡正寰.锻压技术, 1995;5:25) [10] Fang G, Lei L P, Zeng P. J Mater Process Technol, 2002;129: 245 [11] Dong Y M, Kaveh A Tagavi, Michael R Lovell. Int J MechSci, 2000; 42: 1233 [12] Du F S, Li X T, Wang M T. Chin J Mech Eng, 2002; 38:231(杜凤山,李学通,王敏婷.机械工程学报, 2002;38:231) [13] Poliak E I, Jonas J J. ISIJ Int, 2003; 43(5): 684 [14] Balance J B. The Deformation of Austenite. AIME, 1977: 36 [15] Sellars C M. ISIJ Int, 1999; 39(4): 26 [16] Roberts G. Met Sci, 1979; 13(2): 94I |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|