| 750 ℃热暴露对定向层片组织铸造TiAl合金室温拉伸塑性的影响 |
朱春雷, 李胜, 李海昭, 张继( ) |
| 钢铁研究总院高温合金新材料北京市重点实验室, 北京 100081 |
|
| EFFECT OF THERMAL EXPOSURE AT 750 ℃ ON ROOM TEMPERATURE TENSILE DUCTILITY OF CAST TiAl ALLOY WITH DIRECTIONAL LAMELLAR MICROSTRUCTURE |
ZHU Chunlei, LI Sheng, LI Haizhao, ZHANG Ji( ) |
| Beijing Key Laborary of Advanced High Temperature Materials, Central Iron and Steel Research Institute,Beijing 100081 |
引用本文:
朱春雷, 李胜, 李海昭, 张继. 750 ℃热暴露对定向层片组织铸造TiAl合金室温拉伸塑性的影响[J]. 金属学报, 2014, 50(12): 1478-1484.
Chunlei ZHU,
Sheng LI,
Haizhao LI,
Ji ZHANG.
EFFECT OF THERMAL EXPOSURE AT 750 ℃ ON ROOM TEMPERATURE TENSILE DUCTILITY OF CAST TiAl ALLOY WITH DIRECTIONAL LAMELLAR MICROSTRUCTURE[J]. Acta Metall Sin, 2014, 50(12): 1478-1484.
| [1] |
Lu M, Barrett J R, Kelly T J. In: Hemker K J, Dimiduk D M, Clemens H, Darolia R, Inui H, Larsen J M, Sikka V K, Thomas M, Whittenberger J D eds., Structural Intermetallics 2001, Warrendale PA: TMS, 2001: 225
|
| [2] |
Tetsui T. Mater Sci Eng, 2002; A329-331: 582
|
| [3] |
Kim Y W. Mater Sci Eng, 1995; A192-193: 519
|
| [4] |
Huang S C. In: Darolia R, Lewandowski J J, Liu C T, Martin P L, Miracle D B, Nathal M V eds., Structural Intermetallics 1993, Warrendale PA: TMS, 1993: 299
|
| [5] |
Dowling W E, Donlon W T. Scr Metall Mater, 1992; 27: 1663
|
| [6] |
Kelly T J, Austin C M, Fink P J, Schaeffer J. Scr Metall Mater, 1994; 30: 1105
|
| [7] |
Lee D S, Stucke M A, Dimiduk D M. Mater Sci Eng, 1995; A192-193: 824
|
| [8] |
Draper S L, Lerch B A, Locci I E, Shazly M, Prakash V. Intermetallics, 2005; 13: 1014
|
| [9] |
Pilone D, Felli F, Brotzu A. Intermetallics, 2013; 40: 131
|
| [10] |
Wu X H, Huang A, Hu D, Loretto M H. Intermetallics, 2009; 17: 540
|
| [11] |
Pather R, Mitten W A, Holdway P, Ubhi H S, Wisbey A, Brooks J W. Intermetallics, 2003; 11: 1015
|
| [12] |
Zhang J, Zhong Z Y. Mater China, 2010; 29(2): 9
|
| [12] |
(张 继, 仲增墉. 中国材料进展, 2010; 29(2): 9)
|
| [13] |
Zhu C L, Zhang X W, Li S, Zhang J. Rare Met Mater Eng, 2014; 43(9): 2124
|
| [13] |
(朱春雷, 张熹雯, 李 胜, 张 继. 稀有金属材料与工程, 2014; 43(9): 2124)
|
| [14] |
Planck S K, Rosenberger A H. Mater Sci Eng, 2002; A325: 270
|
| [15] |
Shida Y, Anada H. Corros Sci, 1993; 35(5~8): 945
|
| [16] |
Lu W, Chen C L, Xi Y J, Wang F H, He L L. Intermetallics, 2007; 15: 989
|
| [17] |
Yokoshima S, Yamaguchi M. Acta Mater, 1996; 44: 873
|
| [18] |
Thomas M, Berteaux O, Popoff F, Bacos M P, Morel A, Passilly B, Ji V. Intermetallics, 2006; 14: 1143
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|