| 晶粒细化对K417G高温合金蠕变性能的影响 |
都贝宁, 杨金侠, 崔传勇( ), 孙晓峰 |
| 中国科学院金属研究所, 沈阳 110016 |
|
| EFFECTS OF GRAIN REFINEMENT ON CREEP PROPERTIES OF K417G SUPERALLOY |
DU Beining, YANG Jinxia, CUI Chuanyong( ), SUN Xiaofeng |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
引用本文:
都贝宁, 杨金侠, 崔传勇, 孙晓峰. 晶粒细化对K417G高温合金蠕变性能的影响[J]. 金属学报, 2014, 50(11): 1384-1392.
Beining DU,
Jinxia YANG,
Chuanyong CUI,
Xiaofeng SUN.
EFFECTS OF GRAIN REFINEMENT ON CREEP PROPERTIES OF K417G SUPERALLOY[J]. Acta Metall Sin, 2014, 50(11): 1384-1392.
| [1] |
Yang Y H, Xie Y J, Wang M S, Ye W. Mater Des, 2013; 51: 141
|
| [2] |
Xu Y, Guo S R. Acta Metall Sin, 1999; 35: 1249
|
| [2] |
(徐 岩, 郭守仁. 金属学报, 1999; 35: 1249)
|
| [3] |
Zheng L. J Aeronaut Mater, 2006; 26(3): 7
|
| [3] |
(郑 亮. 航空材料学报, 2006; 26(3): 7)
|
| [4] |
Andersson J. Int J Fatigue, 2005; 27: 847
|
| [5] |
Ho H, Risbet M, Feaugas X, Moulin G. Scr Mater, 2011; 65: 998
|
| [6] |
Kobayashi K, Yamaguchi K, Hayakawa M, Kimura M. Mater Lett, 2005; 59: 383
|
| [7] |
Torster F, Baumeister G, Albrecht J, Lütjering G, Helm D, Daeubler M A. Mater Sci Eng, 1997; A234: 189
|
| [8] |
Wei C N, Bor H Y, Ma C Y, Lee T S. Macromol Chem Phys, 2003; 80: 89
|
| [9] |
Xiong Y H, Liu W, Yang A M, Zhang R, Liu L. Acta Metall Sin, 1999; 35: 689
|
| [9] |
(熊玉华, 柳 伟, 杨爱民, 张 蓉, 刘 林. 金属学报, 1999; 35: 689)
|
| [10] |
Yang A M. PhD Dissertation, Northwestern Polytechnical University, Xi'an, 2002
|
| [10] |
(杨爱民. 西北工业大学博士学位论文, 西安, 2002)
|
| [11] |
Soula A, Renollet Y, Boivin D, Pouchou J L, Locq D, Caron P. Mater Sci Eng, 2009; A510: 301
|
| [12] |
Yuan Y, Gu Y F, Cui C Y, Osada T, Tetsui T, Yokokawa T. Mater Sci Eng, 2011; A528: 5106
|
| [13] |
Thibault K, Locq D, Caron P, Boivin D, Renollet Y, Bréchet Y. Mater Sci Eng, 2013; A588: 14
|
| [14] |
Shingledecker J P, Evans N D, Pharr G M. Mater Sci Eng, 2013; A578: 277
|
| [15] |
Morrison D J, Moosbrugger J C. Int J Fatigue, 1997; 19: 51
|
| [16] |
Qiao Y, Chakravarthula S S. Int J Fatigue, 2005; 27: 1251
|
| [17] |
Larson J M, Floreen S. Metall Trans, 1977; 8A: 51
|
| [18] |
Quested P N, Osgerby S. Mater Sci Technol, 1986; 2: 461
|
| [19] |
Kuhn F, Zeismann F, Brueckner-Foit A. Int J Fatigue, 2014; 65: 86
|
| [20] |
Miao J, Pollock T M, Wayne Jones J. Acta Mater, 2009; 57: 5964
|
| [21] |
Miao J, Pollock T M, Wayne Jones J. Acta Mater, 2012; 60: 2840
|
| [22] |
Brewer L N, Field D P, Merriman C C. Electron Backscatter Diffraction in Materials Science. New York: Springer, 2009: 18
|
| [23] |
Wang D, Zhang J, Lou L H. Mater Charact, 2009; 60: 1517
|
| [24] |
Liu L R, Jin T, Zhao N R, Sun X F, Guan H R, Hu Z Q. Mater Sci Eng, 2003; A361: 191
|
| [25] |
Guo Y, Wang B H, Hou S F. Acta Metall Sin (Eng Lett), 2013; 26: 307
|
| [26] |
Zhang J X, Murakumo T, Harada H, Koizumi Y. Scr Mater, 2003; 48: 287
|
| [27] |
Nategh S, Sajjadi S A. Mater Sci Eng, 2003; A339: 103
|
| [28] |
Zhu Y, Li Z, Huang M. Comput Mater Sci, 2013; 70: 178
|
| [29] |
Tian S G, Zhou H H, Zhang J H,Yang H C, Xu Y B, Hu Z Q. Mater Sci Eng, 2000; A279: 160
|
| [30] |
Hantcherli M, Pettinari-Sturmel F, Viguier B, Douin J, Coujou A. Scr Mater, 2012; 66: 143
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|