| 金属中间隙原子的有效相互作用势* |
| 张志鹏, 雷明凯 |
| 大连理工大学材料科学与工程学院表面工程实验室, 大连 116024 |
|
| EFFECTIVE PAIR INTERACTION POTENTIAL OF INTERSTITIAL ATOMS IN METAL |
| ZHANG Zhipeng, LEI Mingkai |
| Surface Engineering Laboratory, School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024 |
引用本文:
张志鹏, 雷明凯. 金属中间隙原子的有效相互作用势*[J]. 金属学报, 2014, 50(1): 103-109.
Zhipeng ZHANG,
Mingkai LEI.
EFFECTIVE PAIR INTERACTION POTENTIAL OF INTERSTITIAL ATOMS IN METAL[J]. Acta Metall Sin, 2014, 50(1): 103-109.
| [1] |
Khachaturyan A G. Theory of Structural Transformations in Solids. New York: John Wiley and Sons, 1983: 446
|
| [2] |
Cao B S, Lei M K.Phys Rev, 2007; 76B: 212301
|
| [3] |
Lepri S, Livi R, Politi A.Phys Rev Lett, 1997; 78: 1896
|
| [4] |
Hu B, Li B, Zhao H.Phys Rev, 1998; 57E: 2992
|
| [5] |
Zener C.Phys Rev, 1948; 74: 639
|
| [6] |
Udyansky A, Von Pezold J, Bugaev V N, Friák M, Neugebauer J.Phys Rev, 2009; 79B: 224112
|
| [7] |
Varvenne C, Finel A, Le Bouar Y, Fèvre M.Phys Rev, 2012; 86B: 184203
|
| [8] |
Matsubara T J. J Phys Soc Jpn, 1952; 7: 270
|
| [9] |
Kanzaki H.J Phys Chem Solids, 1957; 2: 24
|
| [10] |
Hillert M, Staffansson L I.Acta Chem Scand, 1970; 24: 3618
|
| [11] |
Cook H E, Fontaine D D.Acta Metall, 1969; 17: 915
|
| [12] |
Dremov V, Sapozhnikov P, Kutepov A, Anisimov V, Korotin M, Shorikov A, Preston D L, Zocher M A.Phys Rev, 2008; 77B: 224306
|
| [13] |
Wheeler D W, Bayer P D.J Alloys Compd, 2007; 444: 212
|
| [14] |
Dremov V V, Karavaev A V, Sapozhnikov F A, Vorobyova M A, Preston D L, Zocher M A.J Nucl Mater, 2011; 414: 471
|
| [15] |
Jeffries J R, Wall M A, Moore K T, Schwartz A J.J Nucl Mater, 2011; 410: 84
|
| [16] |
Wyttenbach T, Bleiholder C, Bowers M T.Anal Chem, 2013; 85: 2191
|
| [17] |
Cerutti D S, Rice J E, Swope W C, Case D A.J Phys Chem, 2013; 117B: 2328
|
| [18] |
Ansari R, Sadeghi F, Motevalli B. Commun Nonlinear Sci Numerical Simul, 2013; 18: 769
|
| [19] |
Ao B Y, Wang X L, Hu W Y, Yang J Y, Xia J X. J Alloys Compd, 2007; 444-445: 300
|
| [20] |
Johnson R A.J Phys, 1973; 3F: 295
|
| [21] |
Schwerdtfeger P, Gaston N, Krawczyk R P, Tonner R, Moyano G E.Phys Rev, 2006; 73B: 064112
|
| [22] |
Fevre M, Varvenne C, Fine A, Bouar Y L.Philos Mag, 2013; 93: 1563
|
| [23] |
Martin G.Phys Rev, 1990; 41B: 2279
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|