| 快速凝固Fe-6.5%Si合金有序结构及力学性能研究 |
| 李慧1),梁永锋1),贺睿琦2),林均品1), 叶丰1) |
1) 北京科技大学新金属材料国家重点实验室, 北京 100083
2) 邮政科学研究规划院, 北京 100096 |
|
| ORDERED STRUCTURE AND MECHANICAL PROPERTIES OF Fe-6.5%Si ALLOY FABRICATED BY RAPID QUENCHING |
| LI Hui 1), LIANG Yongfeng1), HE Ruiqi2), LIN Junpin1), YE Feng1) |
1) State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing,Beijing 100083
2) Postal Scientific Research & Planning Academy, Beijing 100096 |
引用本文:
李慧,梁永锋,贺睿琦,林均品,叶丰. 快速凝固Fe-6.5%Si合金有序结构及力学性能研究[J]. 金属学报, 2013, 49(11): 1452-1456.
LI Hui,
LIANG Yongfeng,
HE Ruiqi,
LIN Junpin,
YE Feng.
ORDERED STRUCTURE AND MECHANICAL PROPERTIES OF Fe-6.5%Si ALLOY FABRICATED BY RAPID QUENCHING[J]. Acta Metall Sin, 2013, 49(11): 1452-1456.
| [1] Arai K I, Ishiyama K J. J Magn Magn Mater, 1994; 133: 233
[2] Littmann M F. IEEE Trans Magn, 1971; 7: 48
[3] Bozorth R M. Ferromagnetism. New York: D. Van Nostrand Company, 1951: 67
[4] Shin J S, Lee Z H, Lee T D, Lavernia E J. Scr Mater, 2001; 45: 725
[5] Raviprasad K, Chattopadhyay K. Acta Metall Mater, 1993; 41: 609
[6] Gao Z Q, Fultz B. Hyperfine Interact, 1994; 94: 2361
[7] Takada Y, Abe M, Masuda S, Inagaki J. J Appl Phys, 1988; 64: 5367
[8] Ros-Yanez T, Houbaert Y. J Appl Phys, 2002; 91: 7857
[9] Li R, Shen Q, Zhang L, Zhang T. J Magn Magn Mater, 2004; 281: 135
[10] Fish G E, Chang C F, Bye R. J Appl Phys, 1988; 64: 5370
[11] Marcinkowski M J, Brown N. J Appl Phys, 1962; 33: 537
[12] Gemperle A. Czech J Phys, 1968; 18B: 1433
[13] Bakker H, Zhou G F, Yang H. Prog Mater Sci, 1995; 39: 159
[14] Raviprasad K, Chattopadhyay K. Mater Sci Eng, 1988; 98: 281
[15] Brown N. Philos Mag, 1959; 4: 693
[16] Marcinkowski M J, Brown N. Acta Metall Mater, 1961; 9: 764
[17] Marcinkowski M J, Fisher R M. J Appl Phys, 1963; 34: 2135
[18] Raviprasad K, Aoki K, Chattopadhyay K. Mater Sci Eng, 1993; A172: 125 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|