| 试样温度对激光重熔Zr55Cu30Al10Ni5块体非晶合金晶化的影响 |
| 杨高林,林鑫,胡桥,宋梦华,汪志太,黄卫东 |
| 西北工业大学凝固技术国家重点实验室, 西安 710072 |
|
| EFFECT OF SPECIMEN TEMPERATURE ON CRYSTALLIZATION DURING LASER REMELTITNG Zr55Cu30Al10Ni5 BULK METALLIC GLASS |
| YANG Gaolin, LIN Xin, HU Qiao, SONG Menghua, WANG Zhitai, HUANG Weidong |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
引用本文:
杨高林,林鑫,胡桥,宋梦华,汪志太,黄卫东. 试样温度对激光重熔Zr55Cu30Al10Ni5块体非晶合金晶化的影响[J]. 金属学报, 2013, 49(8): 925-931.
YANG Gaolin,
LIN Xin,
HU Qiao,
SONG Menghua,
WANG Zhitai,
HUANG Weidong.
EFFECT OF SPECIMEN TEMPERATURE ON CRYSTALLIZATION DURING LASER REMELTITNG Zr55Cu30Al10Ni5 BULK METALLIC GLASS[J]. Acta Metall Sin, 2013, 49(8): 925-931.
| [1] Wang C, Zhang Q S, Jiang F, Zhang H F, Hu Z Q. Acta Metall Sin, 2002; 38: 765
(王成, 张庆生, 江峰, 张海峰, 胡壮麒. 金属学报, 2002; 38: 765)
[2] Inoue A, Takeuchi A. Acta Mater, 2011; 59: 2243
[3] Byrne C, Eldrup M. Science, 2008; 321: 502
[4] Kumagai N, Samata Y, Kawashima A, Asami K, Hashimoto K. J Non-Cryst Solids, 1987; 93: 78
[5] Kim J H, Lee C, Lee D M, Sun J H, Shin S Y, Bae J C. Mater Sci Eng, 2007; A449-451: 872
[6] Chen B, Pang S, Han P, Li Y, Yavari A R, Vaughan G, Zhang T. J Alloys Compd, 2010; 504: S45
[7] Yue T M, Su Y P, Yang H O. Mater Lett, 2007; 61: 209
[8] Yang G L, Lin X, Liu F C, Hu Q, Ma L, Li J F, Wei D H. Intermetallics, 2012; 22: 110
[9] Lin X, Yang H O, Chen J, Huang W D. Acta Metall Sin, 2006; 42: 361
(林鑫, 杨海欧, 陈静, 黄卫东. 金属学报, 2006; 42: 361
[10] Cao J, Liu F C, Lin X, Huang C P, Chen J, Huang W D. Opt Laser Technol, 2013; 45: 228
[11] Liu F C, Lin X, Huang C P, Song M H, Yang G L, Chen J, Huang W D. J Alloys Compd,2011; 509: 4505
[12] Cervo R, Ferro P, Tiziani A, Zucchi F. J Mater Sci, 2010; 45: 4378
[13] Liu F C, Lin X, Yang G L, Song M H, Chen J, Huang W D. Opt Laser Technol, 2011; 43: 208
[14] Jia W P, Chen J, Lin X, Zhong C W, Huang W D. Acta Metall Sin, 2007; 43: 546
(贾文鹏, 陈静, 林鑫, 钟诚文, 黄卫东. 金属学报, 2007; 43: 546)
[15] Liu F C, Lin X, Yang G L, Huang C P, Chen J, Huang W D. Acta Metall Sin, 2010; 46: 1047
(刘奋成, 林鑫, 杨高林, 黄春平, 陈静, 黄卫东. 金属学报, 2010; 46: 1047)
[16] Laeng J, Stewart J G, Liou F W. Int J Prod Res, 2000; 38: 3973
[17] Sun H, Flores K M. Metall Mater Trans, 2010; 41A: 1752
[18] Zheng B, Zhou Y, Smugeresky J E, Lavernia E J. Metall Mater Trans, 2009; 40A: 2009
[19] Wang H S, Chen H G, Jang J S C, Chiou M S. Mater Sci Eng, 2010; A528: 338
[20] Yamasaki M, Kagao S, Kawamura Y. Scr Mater, 2005; 53: 63
[21] Hu Q, Lin X, Yang G L, Huang W D, Li J F. Acta Metall Sin, 2012; 48: 1467
(胡桥, 林鑫, 杨高林, 黄卫东, 李金富. 金属学报, 2012; 48: 1467)
[22] Xing D W, Shen J, Zhang L F, Sun J F, Wang X D, Wang H. J Alloys Compd, 2009; 481: 531
[23] Zheng Q G, Gu J H. Interaction between Laser and Matter. Wuhan: Huazhong
University of Science and Technology Press, 1996: 129
(郑启光, 辜建辉. 激光与物质相互作用. 武汉: 华中理工大学出版社, 1996: 129)
[24] Kuo T Y, Lin Y D. Mater Trans, 2007; 48: 219
[25] Shao D, Hu B, Zheng Q G. Advanced Laser Manufacturing Technology and
Device Integration. Beijing: Science Press, 2009: 44
(邵丹, 胡兵, 郑启光. 激光先进制造技术与设备集成. 北京: 科学出版社, 2009: 44) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|