Please wait a minute...
金属学报  2012, Vol. 48 Issue (11): 1315-1320    DOI: 10.3724/SP.J.1037.2012.00086
  论文 本期目录 | 过刊浏览 |
P92钢中δ铁素体对700和750℃时效析出相成分和体积分数的影响
彭志方1), 蔡黎胜1), 彭芳芳2), 党莹樱1), 陈方玉3)
1) 武汉大学动力与机械学院, 武汉 430072
2) 东方锅炉(集团)股份有限公司材料研究所, 自贡 643001
3) 武汉钢铁(集团)公司研究院检测所, 武汉 430080
 EFFECT OF δ-FERRITE ON THE COMPOSITION AND VOLUME FRACTION OF PRECIPITATES IN P92 STEEL AGED AT 700 AND 750℃
PENG Zhifang1), CAI Lisheng1),  PENG Fangfang2),  DANG Yingying1), CHEN Fangyu3)
1) School of Power and Mechanical Engineering, Wuhan University, Wuhan 430072
2) Materials Research Department, Dong Fang Boiler Group Corp. Ltd., Zigong 643001
3) Research Institute of Wuhan Iron and Steel Company Ltd., Wuhan 430080
引用本文:

彭志方 蔡黎胜 彭芳芳 党莹樱 陈方玉. P92钢中δ铁素体对700和750℃时效析出相成分和体积分数的影响[J]. 金属学报, 2012, 48(11): 1315-1320.
PENG Zhifang CAI Lisheng Fangfang DANG Yingying CHEN Fangyu.  EFFECT OF δ-FERRITE ON THE COMPOSITION AND VOLUME FRACTION OF PRECIPITATES IN P92 STEEL AGED AT 700 AND 750℃[J]. Acta Metall Sin, 2012, 48(11): 1315-1320.

全文: PDF(806 KB)  
摘要: 

将有、无δ铁素体的P92钢管样在700和750℃分别时效1000, 3000和5000 h, 采用电子探针-X射线能谱分析(EPMA--EDS)和复相分离技术(MPST)研究了δ铁素体对时效析出M23C6及Laves相体积分数及相成分的影响. 结果表明, 在时效过程中, δ铁素体的存在促进了M23C6及 Laves沿δ铁素体的界面析出, 发生聚集与粗化, 并为该过程提供Cr, Mo和W; 在无δ铁素体的P92钢管样中, 不同温度下, M23C6体积分数随时效时间的变化速率不同; 在有δ铁素体的P92钢管样中, 温度降低促进了Laves体积分数的增加, 升高温度则有利于M23C6体积分数的增加. 此外, 提高时效温度和延长时效时间可促进2种析出相的粗化.

关键词 : P92钢,  δ铁素体,  M23C6,  Laves    
Abstract:

Using the as-received P92 steel pipe steel samples with/without δ-ferrite as objects and EPMA-EDS+MPST (multiphase separation technique), this work investigated the effects of δ-ferrite on the volume fraction and< composition of M23C6 and Laves phases precipitated in the ageing treatment at 700 and 750℃ for 1000, 3000 and 5000 h, respectively. The results are as follows. The existence of δ-ferrite promoted aggregation and coarsening of M23C6 and Laves particles precipitated along boundaries with its neighboring lath martensite at the expense of consuming Cr, Mo and W in δ-ferrite during the ageing treatments. Varying rate of the volume fraction of M23C6 with the ageing time for the samples without δ-ferrite would chang at different ageing temperatures, and also the volume fraction of Laves phase would increase with decreasing ageing temperature for the samples with δ-ferrite. Owing to a few amount of Laves formed at higher temperature, the volume fraction of M23C6 increased in the samples with δ-ferrite. And increasing ageing temperature and time stimulated the coarsening of particles precipitated in the pipe samples investigated. It is expected that the related information from this study on the effects of existence of δ-ferrite on the microstructural stability and high temperature properties of P92 can be used as a reference when needed.

Key words: P92 steel    δ-ferrite    M23C6    Laves
收稿日期: 2012-02-22     
基金资助:

国家自然科学基金项目50674072和东方锅炉(集团)股份有限公司2009-2011科技项目资助

作者简介: 彭志方, 男, 1954年生, 教授, 博士

[1] Abe F. Sci Technol Adv Mater, 2008; 9: 1

[2] Maruyama F. ISIJ Int, 2001; 6: 612

[3] Yang F. In: Chinese Society for Electrical Engineering, ed., Symposium on Localization of A New Steel For 600 MW/1000 MW Ultra–Supercritical Units, Zibo: EPTCINA.CN, 2009: 1

(杨 富. 见: 中国电机工程学会主编, 600 MW/1000 MW超超临界机组新型钢

国产化研讨会报告文集, 淄博: 中国电力科技网, 2009: 1)

[4] Ryu S H, Yu J. Metall Mater Trans, 1998; 29A: 1573

[5] Faulkner R G, Williams J A, Sanchez E G, Marshall A W. Mater Sci Technol, 2003; 19: 347

[6] Yoshizawa M, Igarashi M. Int J Pres Ves Pip, 2007; 84: 37

[7] Kimura K, Yamaoka S. Mater Sci Eng, 2004; A387–389: 628

[8] Cai G J, Andren H O, Svensson L E. Metall Mater Trans, 1997; 28A: 1417

[9] Maruyama K, Sawada K, Koike J. ISIJ Int, 2001; 41: 641

[10] Tchizhik A A, Tchizhik T A, Tchizhik A A. J Metall Process Technol, 1998; 77: 226

[11] Kishore R, Singh R N, Sinha T K, Kashyap B P. J Nucl Mater, 1992; 195: 198

[12] Mayr P, Palmer T A, Elmer J W, Specht E D, Allen S M. Metall Mater Trans, 2010; 41A: 2010

[13] Anderko K, Schafer L, Materna–Morris E. J Nucl Mater, 1991; 179–181: 492

[14] Onoro J. J Mater Process Technol, 2006; 180: 137

[15] Sawada K, Kushima H, Kimura K. ISIJ Int, 2006; 46: 769

[16] Vijayalakshmi M, Saroja S, Thomas Paul V, Mythili R, Raghunathan V S. Metall Mater Trans, 1999; 30A: 162

[17] Baek J W, Nam S W, Kong B O. Key Eng Mater, 2005; 297–300: 463

[18] Peng Z F, Cai L S, Dang Y Y, Zhao L, Peng F F, Yang Z G, Yan G Z, Chen S G, Zhou J, Zhou Y G. Mater Sci Forum, 2012; 706–709: 2450

[19] Peng Z F, Dang Y Y, Peng F F. Acta Metall Sin, 2012; 48: 450

(彭志方, 党莹樱, 彭芳芳. 金属学报, 2012; 48: 450)

[20] Peng Z F, Cai L S, Peng F F, Hu Y P, Chen F Y. Acta Metall Sin, 2010; 46: 429

(彭志方, 蔡黎胜, 彭芳芳, 胡永平, 陈方玉. 金属学报, 2010; 46: 429)

[21] Peng Z F, Peng F F, Chen F Y. Electr Power Constr, 2009; 30(12): 1

(彭志方, 彭芳芳, 陈方玉. 电力建设, 2009; 30(12): 1)

[22] Peng F F, Peng Z F, Chen F Y. In: Chinese Society for Electrical Engineering ed., Symposium on Localization of A New Steel For 600 MW/1000 MW Ultra–Supercritical Units, Zibo: EPTCINA.CN, 2009: 178

(彭芳芳, 彭志方, 陈方玉. 见: 中国电机工程学会主编, 600 MW/1000 MW超超临界机组新型钢国产化研讨会报告文集, 淄博: 中国电力科技网, 2009: 178)

[1] 温冬辉, 姜贝贝, 王清, 李相伟, 张鹏, 张书彦. MoNb改性FeCrAl不锈钢高温组织演变和力学性能[J]. 金属学报, 2022, 58(7): 883-894.
[2] 陈建军, 丁雨田, 王琨, 闫康, 马元俊, 王兴茂, 周胜名. Laves相对 GH3625合金管材热挤压过程中爆裂行为的影响[J]. 金属学报, 2021, 57(5): 641-650.
[3] 吴贇, 刘雅辉, 康茂东, 高海燕, 王俊, 孙宝德. K4169合金循环加载过程中的微观组织演变[J]. 金属学报, 2020, 56(9): 1185-1194.
[4] 秦高梧, 谢红波, 潘虎成, 任玉平. 一类介于晶体与准晶体之间的有序结构[J]. 金属学报, 2018, 54(11): 1490-1502.
[5] 李振亮,刘飞,袁爱萍,段宝玉,李晓伟,李一鸣. 轧制变形对喷射沉积含Nd镁合金织构及LPSO相的影响*[J]. 金属学报, 2016, 52(8): 938-944.
[6] 李克俭,蔡志鹏,李轶非,潘际銮. FB2马氏体耐热钢中Laves相在焊接过程中演化行为的研究*[J]. 金属学报, 2016, 52(6): 641-648.
[7] 马坪, 吴二冬, 李武会, 孙凯, 陈东风. Ti0.7Zr0.3(Cr1-xVx)2合金的结构和贮氢性能*[J]. 金属学报, 2014, 50(4): 454-462.
[8] 王学, 于淑敏, 任遥遥, 刘洪, 刘洪伟, 胡磊. P92钢时效的Laves相演化行为[J]. 金属学报, 2014, 50(10): 1195-1202.
[9] 王学, 李勇, 任遥遥, 刘洪伟, 刘洪, 王伟. Laves相析出对P92钢合金元素再分布的影响[J]. 金属学报, 2014, 50(10): 1203-1209.
[10] 张芮辉,张弛,夏志新,杨志刚. T91铁素体耐热钢析出相的优化控制[J]. 金属学报, 2013, 49(9): 1075-1080.
[11] 郑雷刚,胡小强,康秀红,李殿中. Cr-Mn-N奥氏体耐热钢中M23C6型碳化物析出特征及其对韧塑性的影响[J]. 金属学报, 2013, 49(9): 1081-1088.
[12] 王永强,韩军,杨滨,武焕春,王西涛. 核电站主管道Z3CN20.09M不锈钢中金属间相的析出行为[J]. 金属学报, 2013, 29(4): 415-420.
[13] 张麦仓,曹国鑫,董建新,郑磊,姚志浩. 基于经典动态模型的GH4169合金钢锭中Laves相的回溶规律分析[J]. 金属学报, 2013, 49(3): 372-378.
[14] 李冬杰, 陆善平, 李殿中, 李依依. 高氮钢焊缝的组织和冲击性能研究[J]. 金属学报, 2013, 49(2): 129-136.
[15] 盛立远,章炜,赖琛,郭建亭,奚廷斐,叶恒强. 快速凝固制备Laves相增强NiAl基复合材料的微观组织及力学性能[J]. 金属学报, 2013, 49(11): 1318-1324.