| 穿孔等离子弧焊接熔池流动和传热过程的数值模拟 |
| 张涛, 武传松, 陈茂爱 |
| 山东大学材料液固结构演变与加工教育部重点实验室, 济南 250061 |
|
| MODELLING FLUID FLOW AND HEAT TRANSFER PHENOMENA IN KEYHOLING STAGE OF PLASMA ARC WELDING |
| ZHANG Tao, WU Chuansong, CHEN Maoai |
| Key Lab for Liquid-Solid Structure Evolution and Materials Processing (Ministry of Education), Shandong University, Jinan 250061 |
引用本文:
张涛 武传松 陈茂爱. 穿孔等离子弧焊接熔池流动和传热过程的数值模拟[J]. 金属学报, 2012, 48(9): 1025-1032.
,
,
.
MODELLING FLUID FLOW AND HEAT TRANSFER PHENOMENA IN KEYHOLING STAGE OF PLASMA ARC WELDING[J]. Acta Metall Sin, 2012, 48(9): 1025-1032.
| [1] Lucas W. In: Hirata Y, Tanaka M eds., Proc 8th Int Symp on Innovations in Welding and Joining for a New Era in Manufacturing, Kyoto: Japan Welding Society, 2008: 189[2] Irving B. Weld J, 1997; 76(1): 31[3] Kaplan A. J Phys, 1994; 27D: 1805[4] Colla T J, Vicanek M, Simon G. J Phys, 1994; 27D: 2035[5] Sudnik W, Radaj D, Breitschwerd S, Erofeew W. J Phys, 2000; 33D: 662[6] Cho J H, Na S J. J Phys, 2006; 39D: 5372[7] Kazemi K, Goldak J A. Comput Mater Sci, 2009; 44: 841[8] Wang R P, Lei Y P, Shi Y W. Opt Laser Technol, 2011; 43: 870[9] Xu G X. PhD Thesis, Shandong University, Jinan, 2009(胥国祥. 山东大学博士学位论文, 济南, 2009)[10] Dong H G, Gao H M, Wu L. Trans China Weld Inst, 2002; 23(4): 24(董红刚, 高洪明, 吴林. 焊接学报, 2002; 23(4): 24)[11] Wu C S, Wang H G, Zhang M X. Acta Metall Sin, 2006; 42: 311(武传松, 王怀刚, 张明贤. 金属学报, 2006; 42: 311)[12] Wu C S, Hu Q X, Gao J Q. Comput Mater Sci, 2009; 46: 167[13] Li L, Hu S S, Yin F L, Ma L. J Tianjin Univ, 2007; 40: 1260(李力, 胡绳荪, 殷凤良, 马立. 天津大学学报, 2007; 40: 1260)[14] Yin F L. PhD Thesis, Tianjin University, 2007(殷凤良. 天津大学博士学位论文, 2007)[15] Lei Y C, Zheng H J, Cheng X N. Trans China Weld Inst, 2003; 24(1): 44(雷玉成, 郑惠锦, 程晓农. 焊接学报, 2003; 24(1): 44)[16] Hsu Y F, Rubinsky B. Int J Heat Mass Transfer, 1988; 31: 1409[17] Nehad A K. Int Commun Heat Mass Transfer, 1995; 22: 779[18] Keanini R G, Rubinsky B. Int J Heat Mass Transfer, 1993; 36: 3283[19] Wang X J, Wu C S, Chen M A. Acta Metall Sin, 2010; 46: 984(王小杰, 武传松, 陈茂爱. 金属学报, 2010; 46: 984)[20] Fan H G, Kovacevic R. J Phys, 1999; 32D: 2902[21] Huo Y S, Wu C S, Chen M A. Acta Metall Sin, 2011; 47: 706(霍玉双, 武传松, 陈茂爱. 金属学报, 2011; 47: 706)[22] Voller V R, Prakash C. Int J Heat Mass Transfer, 1987; 30: 1709[23] Sun J H, Wu C S, Qin G L. Acta Metall Sin, 2011; 47: 1061(孙俊华, 武传松, 秦国梁. 金属学报, 2011; 47: 1061)[24] Wu C S. Welding Thermal Processes and Weld Pool Behaviors. Beijing: China Machine Press, 2008: 123(武传松. 焊接热过程与熔池形态. 北京: 机械工业出版社, 2008: 123)[25] TaoWQ. Numerical Heat Transfer. 2nd Ed., Xi’an: Xi’an Jiaotong University Press, 2001: 218(陶文铨. 数值传热学. 第2版, 西安: 西安交通大学出版社, 2001: 218) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|